JPS59196580A - 酸素濃淡電池の製造方法 - Google Patents
酸素濃淡電池の製造方法Info
- Publication number
- JPS59196580A JPS59196580A JP58069761A JP6976183A JPS59196580A JP S59196580 A JPS59196580 A JP S59196580A JP 58069761 A JP58069761 A JP 58069761A JP 6976183 A JP6976183 A JP 6976183A JP S59196580 A JPS59196580 A JP S59196580A
- Authority
- JP
- Japan
- Prior art keywords
- particles
- granulated
- granulated particles
- fine particles
- electrode
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- G—PHYSICS
- G01—MEASURING; TESTING
- G01N—INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES
- G01N27/00—Investigating or analysing materials by the use of electric, electrochemical, or magnetic means
- G01N27/26—Investigating or analysing materials by the use of electric, electrochemical, or magnetic means by investigating electrochemical variables; by using electrolysis or electrophoresis
- G01N27/403—Cells and electrode assemblies
- G01N27/406—Cells and probes with solid electrolytes
- G01N27/407—Cells and probes with solid electrolytes for investigating or analysing gases
- G01N27/4071—Cells and probes with solid electrolytes for investigating or analysing gases using sensor elements of laminated structure
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M8/00—Fuel cells; Manufacture thereof
- H01M8/10—Fuel cells with solid electrolytes
- H01M8/12—Fuel cells with solid electrolytes operating at high temperature, e.g. with stabilised ZrO2 electrolyte
- H01M8/1231—Fuel cells with solid electrolytes operating at high temperature, e.g. with stabilised ZrO2 electrolyte with both reactants being gaseous or vaporised
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/30—Hydrogen technology
- Y02E60/50—Fuel cells
Landscapes
- Life Sciences & Earth Sciences (AREA)
- Chemical & Material Sciences (AREA)
- Electrochemistry (AREA)
- Health & Medical Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- General Physics & Mathematics (AREA)
- Pathology (AREA)
- Analytical Chemistry (AREA)
- Biochemistry (AREA)
- General Health & Medical Sciences (AREA)
- Molecular Biology (AREA)
- Immunology (AREA)
- Physics & Mathematics (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Sustainable Development (AREA)
- Sustainable Energy (AREA)
- General Chemical & Material Sciences (AREA)
- Measuring Oxygen Concentration In Cells (AREA)
- Fuel Cell (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58069761A JPS59196580A (ja) | 1983-04-20 | 1983-04-20 | 酸素濃淡電池の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58069761A JPS59196580A (ja) | 1983-04-20 | 1983-04-20 | 酸素濃淡電池の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS59196580A true JPS59196580A (ja) | 1984-11-07 |
| JPH0244391B2 JPH0244391B2 (enExample) | 1990-10-03 |
Family
ID=13412102
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58069761A Granted JPS59196580A (ja) | 1983-04-20 | 1983-04-20 | 酸素濃淡電池の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS59196580A (enExample) |
Cited By (4)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6443752A (en) * | 1987-08-12 | 1989-02-16 | Ngk Spark Plug Co | Element for oxygen sensor |
| JPH01203963A (ja) * | 1988-02-10 | 1989-08-16 | Ngk Spark Plug Co Ltd | 酸素センサ素子及びその製造方法 |
| JP2010204088A (ja) * | 2009-02-06 | 2010-09-16 | Nippon Soken Inc | ガスセンサ用固体電解質、その製造方法、及びそれを用いたガスセンサ |
| JP2018146470A (ja) * | 2017-03-08 | 2018-09-20 | 日本特殊陶業株式会社 | ガスセンサ素子の製造方法 |
-
1983
- 1983-04-20 JP JP58069761A patent/JPS59196580A/ja active Granted
Cited By (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6443752A (en) * | 1987-08-12 | 1989-02-16 | Ngk Spark Plug Co | Element for oxygen sensor |
| JPH01203963A (ja) * | 1988-02-10 | 1989-08-16 | Ngk Spark Plug Co Ltd | 酸素センサ素子及びその製造方法 |
| JP2010204088A (ja) * | 2009-02-06 | 2010-09-16 | Nippon Soken Inc | ガスセンサ用固体電解質、その製造方法、及びそれを用いたガスセンサ |
| JP2018146470A (ja) * | 2017-03-08 | 2018-09-20 | 日本特殊陶業株式会社 | ガスセンサ素子の製造方法 |
| CN108572210A (zh) * | 2017-03-08 | 2018-09-25 | 日本特殊陶业株式会社 | 气体传感器元件的制造方法 |
| CN108572210B (zh) * | 2017-03-08 | 2021-09-21 | 日本特殊陶业株式会社 | 气体传感器元件的制造方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0244391B2 (enExample) | 1990-10-03 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4477487A (en) | Method of producing oxygen concentration cells | |
| JPH01184457A (ja) | 酸素センサ素子 | |
| JPH04100505A (ja) | セラミックフィルタの製造方法 | |
| GB1574007A (en) | Cermets | |
| JPS6249582B2 (enExample) | ||
| JPS59196580A (ja) | 酸素濃淡電池の製造方法 | |
| JPH02276956A (ja) | 酸素センサおよびその製造方法ならびに被毒防止方法 | |
| JP3634956B2 (ja) | ガスセンサ素子の製法 | |
| JPH01203963A (ja) | 酸素センサ素子及びその製造方法 | |
| JP2589130B2 (ja) | 酸素センサ素子 | |
| JP2869487B2 (ja) | ダイアフラムの製造方法及び製造装置 | |
| JPH065219B2 (ja) | 電極形成方法 | |
| JPS63167261A (ja) | 酸素センサ素子の製造方法 | |
| JPS60107560A (ja) | 酸素濃度センサの製造方法 | |
| JP2001124724A (ja) | 酸素センサ素子及びその製法 | |
| CN111505082A (zh) | 一种新型管式传感元件及其制备方法 | |
| CN1031098A (zh) | 氧化锆管电极涂层 | |
| JP2560930B2 (ja) | セラミックス基材の表面処理方法 | |
| JP2868920B2 (ja) | 溶融金属中の酸素濃度測定用素子 | |
| JPS63105469A (ja) | アルカリ電池用ニツケル基板の製法 | |
| JPH0810209B2 (ja) | 酸素センサ素子 | |
| JPH0891840A (ja) | ジルコニア厚膜の製造方法 | |
| JPH0253925B2 (enExample) | ||
| JPH04204046A (ja) | ガラスセラミックスからなる多孔質焼結体の製造方法および酸素濃度検出器 | |
| JPH0272558A (ja) | 燃料電池の電極の製造方法 |