JPS59123794U - 防食用シ−ト - Google Patents
防食用シ−トInfo
- Publication number
- JPS59123794U JPS59123794U JP1772483U JP1772483U JPS59123794U JP S59123794 U JPS59123794 U JP S59123794U JP 1772483 U JP1772483 U JP 1772483U JP 1772483 U JP1772483 U JP 1772483U JP S59123794 U JPS59123794 U JP S59123794U
- Authority
- JP
- Japan
- Prior art keywords
- sheet
- rubber
- anticorrosive
- corrosion
- sheet according
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Protection Of Pipes Against Damage, Friction, And Corrosion (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1772483U JPS59123794U (ja) | 1983-02-09 | 1983-02-09 | 防食用シ−ト |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP1772483U JPS59123794U (ja) | 1983-02-09 | 1983-02-09 | 防食用シ−ト |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS59123794U true JPS59123794U (ja) | 1984-08-20 |
JPH0228317Y2 JPH0228317Y2 (enrdf_load_stackoverflow) | 1990-07-30 |
Family
ID=30148956
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1772483U Granted JPS59123794U (ja) | 1983-02-09 | 1983-02-09 | 防食用シ−ト |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS59123794U (enrdf_load_stackoverflow) |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS527021A (en) * | 1975-07-07 | 1977-01-19 | Nippon Kokan Kk <Nkk> | Anticorrosive method of tee joint in piping works |
JPS52141066U (enrdf_load_stackoverflow) * | 1976-04-20 | 1977-10-26 |
-
1983
- 1983-02-09 JP JP1772483U patent/JPS59123794U/ja active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS527021A (en) * | 1975-07-07 | 1977-01-19 | Nippon Kokan Kk <Nkk> | Anticorrosive method of tee joint in piping works |
JPS52141066U (enrdf_load_stackoverflow) * | 1976-04-20 | 1977-10-26 |
Also Published As
Publication number | Publication date |
---|---|
JPH0228317Y2 (enrdf_load_stackoverflow) | 1990-07-30 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS59123794U (ja) | 防食用シ−ト | |
KR910001267A (ko) | 나사, 볼트등에 의해 체결되는 자동차 부품용 부식 방지 부재 | |
JPS59118892U (ja) | 防食用シ−ト | |
JPS58161294U (ja) | 防食用シ−ト | |
JPS5899307U (ja) | ゴム支承 | |
JPS58161295U (ja) | 防食用シ−ト | |
JPS59104722U (ja) | 防食テ−プもしくはシ−ト | |
JPS6255334A (ja) | 海洋鋼構造物の防食施工方法 | |
JPH011830A (ja) | 水中打込部材の防食補修方法 | |
JP4823126B2 (ja) | 継手部防食性に優れる重防食被覆鋼矢板の構造体及びその構造体に使用する鋼矢板 | |
JPS6045750U (ja) | 鋼管矢板の防食構造 | |
CN217629184U (zh) | 一种用于铁路轨道的防腐蚀结构 | |
CN201538371U (zh) | 橡胶履带板 | |
CN219808183U (zh) | 一种轨下垫板及轨距块 | |
CN219128147U (zh) | 一种高效耐腐蚀的双联单杠 | |
CN206206487U (zh) | 一种橡胶衬垫组件 | |
JPH0126946Y2 (enrdf_load_stackoverflow) | ||
CN206053509U (zh) | 一种铁塔变坡包钢 | |
CN204435211U (zh) | 钢质桥面板索道桥的专用板式橡胶支座 | |
JPS5811992Y2 (ja) | 海底長尺体用防護体 | |
JPS5865778A (ja) | 接着工法 | |
JPS60126778U (ja) | 配管固定装置 | |
JPS60113292U (ja) | 船舶のタンク構造 | |
JPS5928279U (ja) | リニアモ−タ用リアクシヨンプレ−ト | |
JPS60186325U (ja) | 救命梯子兼用ゴム製防舷材 |