JPS59123716A - 耐硫化物割れ性に優れた油井用鋼管の製造法 - Google Patents
耐硫化物割れ性に優れた油井用鋼管の製造法Info
- Publication number
- JPS59123716A JPS59123716A JP23304582A JP23304582A JPS59123716A JP S59123716 A JPS59123716 A JP S59123716A JP 23304582 A JP23304582 A JP 23304582A JP 23304582 A JP23304582 A JP 23304582A JP S59123716 A JPS59123716 A JP S59123716A
- Authority
- JP
- Japan
- Prior art keywords
- steel
- hardness
- strength
- steel pipe
- rolling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D8/00—Modifying the physical properties by deformation combined with, or followed by, heat treatment
- C21D8/10—Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of tubular bodies
Landscapes
- Engineering & Computer Science (AREA)
- Chemical & Material Sciences (AREA)
- Manufacturing & Machinery (AREA)
- Physics & Mathematics (AREA)
- Thermal Sciences (AREA)
- Crystallography & Structural Chemistry (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Heat Treatment Of Steel (AREA)
- Heat Treatment Of Articles (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP23304582A JPS59123716A (ja) | 1982-12-28 | 1982-12-28 | 耐硫化物割れ性に優れた油井用鋼管の製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP23304582A JPS59123716A (ja) | 1982-12-28 | 1982-12-28 | 耐硫化物割れ性に優れた油井用鋼管の製造法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS59123716A true JPS59123716A (ja) | 1984-07-17 |
JPS6256929B2 JPS6256929B2 (enrdf_load_stackoverflow) | 1987-11-27 |
Family
ID=16948933
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP23304582A Granted JPS59123716A (ja) | 1982-12-28 | 1982-12-28 | 耐硫化物割れ性に優れた油井用鋼管の製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS59123716A (enrdf_load_stackoverflow) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS634047A (ja) * | 1986-06-20 | 1988-01-09 | Sumitomo Metal Ind Ltd | 耐硫化物割れ性に優れた高張力油井用鋼 |
US5186768A (en) * | 1990-06-14 | 1993-02-16 | Sumitomo Metal Industries, Ltd. | Flat spring hose clamp and manufacture of same |
EP2361996A3 (en) * | 2007-03-30 | 2011-10-19 | Sumitomo Metal Industries, Ltd. | Low alloy pipe steel for oil well use and seamless steel pipe |
-
1982
- 1982-12-28 JP JP23304582A patent/JPS59123716A/ja active Granted
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS634047A (ja) * | 1986-06-20 | 1988-01-09 | Sumitomo Metal Ind Ltd | 耐硫化物割れ性に優れた高張力油井用鋼 |
US5186768A (en) * | 1990-06-14 | 1993-02-16 | Sumitomo Metal Industries, Ltd. | Flat spring hose clamp and manufacture of same |
EP2361996A3 (en) * | 2007-03-30 | 2011-10-19 | Sumitomo Metal Industries, Ltd. | Low alloy pipe steel for oil well use and seamless steel pipe |
Also Published As
Publication number | Publication date |
---|---|
JPS6256929B2 (enrdf_load_stackoverflow) | 1987-11-27 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4814141A (en) | High toughness, ultra-high strength steel having an excellent stress corrosion cracking resistance with a yield stress of not less than 110 kgf/mm2 | |
JP5167616B2 (ja) | 耐遅れ破壊特性に優れた金属ボルト | |
JPS6354765B2 (enrdf_load_stackoverflow) | ||
US7678207B2 (en) | Steel product for induction hardening, induction-hardened member using the same, and methods producing them | |
JPH10121202A (ja) | 耐硫化物応力割れ性を必要とする環境で使用される高強度鋼材およびその製造方法 | |
JP4867638B2 (ja) | 耐遅れ破壊特性および耐腐食性に優れた高強度ボルト | |
EP0738784B1 (en) | High chromium martensitic steel pipe having excellent pitting resistance and method of manufacturing | |
JPH06271975A (ja) | 耐水素脆化特性に優れた高強度鋼およびその製法 | |
JP2541070B2 (ja) | 母材の脆性破壊伝播停止特性に優れた高ニッケル合金クラッド鋼板の製造方法 | |
JPS6164815A (ja) | 耐遅れ破壊性の優れた高強度鋼の製造法 | |
JPH09137253A (ja) | 耐応力腐食割れ性および低温靱性に優れた超高張力鋼およびその製造方法 | |
JPS59123716A (ja) | 耐硫化物割れ性に優れた油井用鋼管の製造法 | |
JPH0413406B2 (enrdf_load_stackoverflow) | ||
JP3201081B2 (ja) | 油井用ステンレス鋼およびその製造方法 | |
JPH05156409A (ja) | 耐海水性に優れた高強度マルテンサイトステンレス鋼とその製造方法 | |
JP2527512B2 (ja) | 耐ssc性の優れた低硬度高靭性シ―ムレス鋼管の製造法 | |
JPS609824A (ja) | 強靭鋼の製造方法 | |
JPS63206449A (ja) | 冷間圧造用低炭素鋼 | |
JPH0569884B2 (enrdf_load_stackoverflow) | ||
JPS61272316A (ja) | 耐応力腐蝕割れ性のすぐれた超高張力鋼の製造法 | |
JP2752505B2 (ja) | 低温靭性および耐硫化物応力腐食割れ性に優れた高強度低合金油井用鋼 | |
JPS6210240A (ja) | 耐食性と圧潰強度の優れた継目無油井管用鋼 | |
JP3099155B2 (ja) | 溶接性に優れた高強度マルテンサイトステンレス鋼とその製造方法 | |
JPS59232221A (ja) | 耐硫化物腐食割れ性に優れた高強度鋼の製法 | |
JPS6117885B2 (enrdf_load_stackoverflow) |