JPS5853973A - 感圧性接着テ−プの製造方法 - Google Patents
感圧性接着テ−プの製造方法Info
- Publication number
- JPS5853973A JPS5853973A JP15332381A JP15332381A JPS5853973A JP S5853973 A JPS5853973 A JP S5853973A JP 15332381 A JP15332381 A JP 15332381A JP 15332381 A JP15332381 A JP 15332381A JP S5853973 A JPS5853973 A JP S5853973A
- Authority
- JP
- Japan
- Prior art keywords
- reactor
- sensitive adhesive
- polymerization
- pressure
- bulk
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Adhesive Tapes (AREA)
- Adhesives Or Adhesive Processes (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15332381A JPS5853973A (ja) | 1981-09-28 | 1981-09-28 | 感圧性接着テ−プの製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15332381A JPS5853973A (ja) | 1981-09-28 | 1981-09-28 | 感圧性接着テ−プの製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5853973A true JPS5853973A (ja) | 1983-03-30 |
| JPH0143792B2 JPH0143792B2 (enrdf_load_stackoverflow) | 1989-09-22 |
Family
ID=15559978
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15332381A Granted JPS5853973A (ja) | 1981-09-28 | 1981-09-28 | 感圧性接着テ−プの製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5853973A (enrdf_load_stackoverflow) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4619979A (en) * | 1984-03-28 | 1986-10-28 | Minnesota Mining And Manufacturing Company | Continuous free radial polymerization in a wiped-surface reactor |
| US4695608A (en) * | 1984-03-29 | 1987-09-22 | Minnesota Mining And Manufacturing Company | Continuous process for making polymers having pendant azlactone or macromolecular moieties |
| US4843134A (en) * | 1984-03-28 | 1989-06-27 | Minnesota Mining And Manufacturing Company | Acrylate pressure-sensitive adhesives containing insolubles |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5034071A (enrdf_load_stackoverflow) * | 1973-07-27 | 1975-04-02 |
-
1981
- 1981-09-28 JP JP15332381A patent/JPS5853973A/ja active Granted
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5034071A (enrdf_load_stackoverflow) * | 1973-07-27 | 1975-04-02 |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US4619979A (en) * | 1984-03-28 | 1986-10-28 | Minnesota Mining And Manufacturing Company | Continuous free radial polymerization in a wiped-surface reactor |
| US4843134A (en) * | 1984-03-28 | 1989-06-27 | Minnesota Mining And Manufacturing Company | Acrylate pressure-sensitive adhesives containing insolubles |
| US4695608A (en) * | 1984-03-29 | 1987-09-22 | Minnesota Mining And Manufacturing Company | Continuous process for making polymers having pendant azlactone or macromolecular moieties |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0143792B2 (enrdf_load_stackoverflow) | 1989-09-22 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CA2600928C (en) | Continuous bulk polymerization in a planetary roller extruder | |
| US4619979A (en) | Continuous free radial polymerization in a wiped-surface reactor | |
| US4843134A (en) | Acrylate pressure-sensitive adhesives containing insolubles | |
| TWI359157B (en) | Method to produce uv-curable solventless acrylate- | |
| KR101242237B1 (ko) | 아크릴 필름의 제조 방법 및 아크릴 필름 | |
| JP4509279B2 (ja) | アクリル系感圧性接着剤の製造方法 | |
| JP4803916B2 (ja) | アクリル系感圧性接着剤及びその製造方法 | |
| JPS5853973A (ja) | 感圧性接着テ−プの製造方法 | |
| JPS5853974A (ja) | 感圧性接着テ−プの製造方法 | |
| JPH024632B2 (enrdf_load_stackoverflow) | ||
| JP3611653B2 (ja) | アクリル系感圧性接着剤、その接着シ―ト類およびこれらの製造方法 | |
| JPS6241523B2 (enrdf_load_stackoverflow) | ||
| JPS58168610A (ja) | 感圧性接着剤の製造方法 | |
| TWI374175B (en) | Emulsion based adhesive product | |
| JPH0255448B2 (enrdf_load_stackoverflow) | ||
| JPS5853970A (ja) | 感圧性接着剤組成物の製造方法 | |
| JP3375430B2 (ja) | アクリル系重合体の製造方法 | |
| JPS5853969A (ja) | 感圧性接着剤組成物 | |
| JP2002241730A (ja) | 水分散型粘着剤組成物の乾燥方法および水分散型粘着シート類の製造方法と水分散型粘着シート類 | |
| JPH09141718A (ja) | 反応性樹脂シートの製造方法 | |
| JPH08269411A (ja) | 粘着シ―ト類の製造方法 | |
| JPH11228926A (ja) | 放射線硬化型粘着剤組成物とその粘着シ―ト類およびこれらの製造方法 | |
| JPH03227305A (ja) | 光重合装置及びその装置でアクリル系高分子を製造する方法 | |
| JPH08113603A (ja) | アクリル系粘着剤の製造方法 | |
| JPH07224102A (ja) | アクリル系重合体の製造方法 |