JPS5842781A - 電極の製造法 - Google Patents
電極の製造法Info
- Publication number
- JPS5842781A JPS5842781A JP57145486A JP14548682A JPS5842781A JP S5842781 A JPS5842781 A JP S5842781A JP 57145486 A JP57145486 A JP 57145486A JP 14548682 A JP14548682 A JP 14548682A JP S5842781 A JPS5842781 A JP S5842781A
- Authority
- JP
- Japan
- Prior art keywords
- electrode
- particles
- metal
- layer
- nickel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Electrodes For Compound Or Non-Metal Manufacture (AREA)
- Electrolytic Production Of Non-Metals, Compounds, Apparatuses Therefor (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57145486A JPS5842781A (ja) | 1982-08-24 | 1982-08-24 | 電極の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP57145486A JPS5842781A (ja) | 1982-08-24 | 1982-08-24 | 電極の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5842781A true JPS5842781A (ja) | 1983-03-12 |
| JPS6123278B2 JPS6123278B2 (enrdf_load_stackoverflow) | 1986-06-05 |
Family
ID=15386369
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP57145486A Granted JPS5842781A (ja) | 1982-08-24 | 1982-08-24 | 電極の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5842781A (enrdf_load_stackoverflow) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62241278A (ja) * | 1986-04-11 | 1987-10-21 | 矢崎総業株式会社 | 電線張力除去コネクタ |
| JPH02102665U (enrdf_load_stackoverflow) * | 1989-02-01 | 1990-08-15 | ||
| JPH0651013U (ja) * | 1992-12-17 | 1994-07-12 | 古河電気工業株式会社 | ドア用ワイヤハーネス |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB1148865A (en) * | 1965-05-07 | 1969-04-16 | Ceskosloveska Akademie Ved | A method of producing active electrodes with a low over-voltage for electrolysis |
| US3790454A (en) * | 1971-01-22 | 1974-02-05 | Nat Defence | Electrodeposition of sponge nickel |
-
1982
- 1982-08-24 JP JP57145486A patent/JPS5842781A/ja active Granted
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| GB1148865A (en) * | 1965-05-07 | 1969-04-16 | Ceskosloveska Akademie Ved | A method of producing active electrodes with a low over-voltage for electrolysis |
| US3790454A (en) * | 1971-01-22 | 1974-02-05 | Nat Defence | Electrodeposition of sponge nickel |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6123278B2 (enrdf_load_stackoverflow) | 1986-06-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4302322A (en) | Low hydrogen overvoltage electrode | |
| US11757101B2 (en) | Metal porous body and method for producing metal porous body | |
| JP6960096B2 (ja) | 複合金属多孔体、不溶性陽極、燃料電池用電極、水素の製造装置、形状記憶合金、生体材料、および複合金属多孔体の製造方法 | |
| JPS5948872B2 (ja) | 電解用陰極及びその製造法 | |
| US4498962A (en) | Anode for the electrolysis of water | |
| WO2012077550A1 (ja) | 高耐食性を有する金属多孔体及びその製造方法 | |
| JPH01139785A (ja) | 電極触媒及びその製造方法 | |
| US3732157A (en) | Electrolytic cell including titanium hydride cathodes and noble-metal coated titanium hydride anodes | |
| KR890000179B1 (ko) | 고내구성 및 저수소 과전압을 갖는 음극 및 그의 제조방법 | |
| JP2000256898A (ja) | ウェーハの銅めっき方法 | |
| Nikolić et al. | The control of morphology and structure of galvanostatically produced tin dendrites by analysis of chronopotentiometry response | |
| CN100575562C (zh) | 一种高电阻率金属氧化物材料表面电镀的方法 | |
| JPS5842781A (ja) | 電極の製造法 | |
| GB2056495A (en) | Process for the preparation of low hydrogen overvoltage cathodes | |
| JPS60159184A (ja) | 水電解用陽極 | |
| JP4632966B2 (ja) | 電解金属粉の製造方法 | |
| JP4278406B2 (ja) | 燃料電池用セパレーター | |
| TWI300447B (en) | Method of recycling plating liquid | |
| JPS5925985A (ja) | 水電解用高耐久性低過電圧陰極及びその製造法 | |
| Evans et al. | Studies in the Discontinuities in Electrodeposited Metallic Coatings: Part I. | |
| JPS6125790B2 (enrdf_load_stackoverflow) | ||
| JPS58133387A (ja) | 低水素過電圧陰極及びその製法 | |
| KR820000886B1 (ko) | 전극의 제조법 | |
| JPS5967383A (ja) | 水電解用の陽極及びその製法 | |
| JPS58126994A (ja) | 電解用陰極 |