JPS58210200A - 鉄酸化物皮膜の溶解法 - Google Patents
鉄酸化物皮膜の溶解法Info
- Publication number
- JPS58210200A JPS58210200A JP9440782A JP9440782A JPS58210200A JP S58210200 A JPS58210200 A JP S58210200A JP 9440782 A JP9440782 A JP 9440782A JP 9440782 A JP9440782 A JP 9440782A JP S58210200 A JPS58210200 A JP S58210200A
- Authority
- JP
- Japan
- Prior art keywords
- iron oxide
- oxide film
- piping
- dissolving
- electrolytic cell
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Cleaning And De-Greasing Of Metallic Materials By Chemical Methods (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9440782A JPS58210200A (ja) | 1982-06-02 | 1982-06-02 | 鉄酸化物皮膜の溶解法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP9440782A JPS58210200A (ja) | 1982-06-02 | 1982-06-02 | 鉄酸化物皮膜の溶解法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS58210200A true JPS58210200A (ja) | 1983-12-07 |
JPH0255520B2 JPH0255520B2 (enrdf_load_stackoverflow) | 1990-11-27 |
Family
ID=14109380
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP9440782A Granted JPS58210200A (ja) | 1982-06-02 | 1982-06-02 | 鉄酸化物皮膜の溶解法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS58210200A (enrdf_load_stackoverflow) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6225300A (ja) * | 1985-07-26 | 1987-02-03 | 株式会社日立製作所 | 酸化物の溶解法 |
EP1619271A3 (en) * | 1997-09-30 | 2006-02-01 | Larry L. Russell | Method and apparatus for lead contamination control |
JP5721888B1 (ja) * | 2014-07-04 | 2015-05-20 | 三菱日立パワーシステムズ株式会社 | 化学洗浄方法及び化学洗浄装置 |
WO2016002516A1 (ja) * | 2014-07-04 | 2016-01-07 | 三菱日立パワーシステムズ株式会社 | 化学洗浄方法及び化学洗浄装置 |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5221456A (en) * | 1975-08-11 | 1977-02-18 | Hiroko Miyoshi | Knitting machine |
JPS5785980A (en) * | 1980-11-17 | 1982-05-28 | Hitachi Ltd | Method for removal of oxide on metallic surface |
-
1982
- 1982-06-02 JP JP9440782A patent/JPS58210200A/ja active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5221456A (en) * | 1975-08-11 | 1977-02-18 | Hiroko Miyoshi | Knitting machine |
JPS5785980A (en) * | 1980-11-17 | 1982-05-28 | Hitachi Ltd | Method for removal of oxide on metallic surface |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6225300A (ja) * | 1985-07-26 | 1987-02-03 | 株式会社日立製作所 | 酸化物の溶解法 |
EP1619271A3 (en) * | 1997-09-30 | 2006-02-01 | Larry L. Russell | Method and apparatus for lead contamination control |
JP5721888B1 (ja) * | 2014-07-04 | 2015-05-20 | 三菱日立パワーシステムズ株式会社 | 化学洗浄方法及び化学洗浄装置 |
WO2016002516A1 (ja) * | 2014-07-04 | 2016-01-07 | 三菱日立パワーシステムズ株式会社 | 化学洗浄方法及び化学洗浄装置 |
Also Published As
Publication number | Publication date |
---|---|
JPH0255520B2 (enrdf_load_stackoverflow) | 1990-11-27 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPH0445594B2 (enrdf_load_stackoverflow) | ||
US20160247589A1 (en) | TREATMENT METHOD AND TREATMENT APPARATUS OF IRON-GROUP METAL ION-CONTAINING LIQUID, METHOD AND APPARATUS FOR ELECTRODEPOSITING Co AND Fe, AND DECONTAMINATION METHOD AND DECONTAMINATION APPARATUS OF RADIOACTIVE WASTE ION EXCHANGE RESIN | |
JPS58210200A (ja) | 鉄酸化物皮膜の溶解法 | |
Sherar et al. | Nominally anaerobic corrosion of carbon steel in near-neutral pH saline environments | |
Seo et al. | A quartz crystal microbalance study of the corrosion of iron thin films in neutral aqueous solutions | |
Ghabashy et al. | Effect of a magnetic field on the rate of diffusion-controlled corrosion of metals | |
Wang et al. | Anodic dissolution of iron in a magnetic field with holographic microphotography | |
JPS5983800A (ja) | 表面付着鉄酸化物の溶解法 | |
Shoesmith et al. | Characterization and Dissolution of Deposited Magnetite Films on AISI 304 Stainless Steel Surfaces in EDTA and EDTA/Oxalate Solutions | |
JP4257747B2 (ja) | 被処理流体補給水又は被処理流体の帯電性判定方法と装置及び被処理流体処理方法と装置 | |
JPS59162496A (ja) | 酸化鉄皮膜の除去方法 | |
JPS603598A (ja) | 酸化鉄皮膜の除染システム | |
JPS6295498A (ja) | 原子力発電プラントの製造法 | |
CN105393309A (zh) | 用于减少核反应堆所用的部件的表面的放射性污染的方法 | |
JPH06214092A (ja) | 原子力発電プラントの水質制御方法及び燃料棒並びに燃料集合体並びに原子力発電プラント | |
Tewari et al. | The surface charge of oxides and its role in deposition and transport of radioactivity in water-cooled nuclear reactors | |
JPS5965297A (ja) | 原子力プラントの放射性物質の付着抑制方法 | |
Chin | Metal recovery from wastewater with an electrochemical method | |
JPS62207898A (ja) | 配管内面に耐食性酸化皮膜を形成する方法及びその装置 | |
Semmler et al. | Treatment of liquid waste and regeneration of spent ion exchange resin using electrochemical techniques | |
Tolouei Asbforoushani | Corrosion of Carbon Steel Under Disbonded Coatings in Acidified Leaching Processes | |
WO2025024566A2 (en) | Extraction of fission products from molten salt via redox reaction with reducting agents | |
JPH024880B2 (enrdf_load_stackoverflow) | ||
JPS6286200A (ja) | 還元除染における溶解速度調整法 | |
JPS61118700A (ja) | 酸化被膜の除却方法およびその装置 |