JPS5792066A - Paste ink composition for screen print - Google Patents

Paste ink composition for screen print

Info

Publication number
JPS5792066A
JPS5792066A JP55168395A JP16839580A JPS5792066A JP S5792066 A JPS5792066 A JP S5792066A JP 55168395 A JP55168395 A JP 55168395A JP 16839580 A JP16839580 A JP 16839580A JP S5792066 A JPS5792066 A JP S5792066A
Authority
JP
Japan
Prior art keywords
screen
organosol
plastisol
diameters
mesh
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP55168395A
Other languages
Japanese (ja)
Other versions
JPH0121193B2 (en
Inventor
Go Sugino
Tokio Niiguni
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Kasei Polytec Co
Original Assignee
Mitsubishi Monsanto Chemical Co
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mitsubishi Monsanto Chemical Co filed Critical Mitsubishi Monsanto Chemical Co
Priority to JP55168395A priority Critical patent/JPS5792066A/en
Publication of JPS5792066A publication Critical patent/JPS5792066A/en
Publication of JPH0121193B2 publication Critical patent/JPH0121193B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE: The titled composition useful for a wall material, etc., having printability of improved performances with respect to screen omissions, entrainment of foams, leveling, obtained by dispersing solid particles having specified particle diameters in a specific ratio into plastisol or organosol.
CONSTITUTION: (B) 20W50vol% solid particles having particle diameters of ≥5μ and smaller than the mesh of screen (preferably 5W100μ, ≤1/2 the mesh) in dispersed into (A) plastisol or organosol (preferably consisting essentially of 0.1W 2μ vinyl chloride resin, to give the desired composition. The component B is preferably vinyl chloride resin (especially a blending resin having a weight-average particle diameter of 20W40μ, and comprising 90W100wt% particles with diameters of 5W100μ), and the solid particle is preferably a filler, e.g., calcium carbonate, coloring agent, etc.
EFFECT: The pattern of the printed surface is sharp, printed layer can be made thick, and a pattern with clear unevenness is given.
COPYRIGHT: (C)1982,JPO&Japio
JP55168395A 1980-11-29 1980-11-29 Paste ink composition for screen print Granted JPS5792066A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP55168395A JPS5792066A (en) 1980-11-29 1980-11-29 Paste ink composition for screen print

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP55168395A JPS5792066A (en) 1980-11-29 1980-11-29 Paste ink composition for screen print

Publications (2)

Publication Number Publication Date
JPS5792066A true JPS5792066A (en) 1982-06-08
JPH0121193B2 JPH0121193B2 (en) 1989-04-20

Family

ID=15867315

Family Applications (1)

Application Number Title Priority Date Filing Date
JP55168395A Granted JPS5792066A (en) 1980-11-29 1980-11-29 Paste ink composition for screen print

Country Status (1)

Country Link
JP (1) JPS5792066A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6356579A (en) * 1986-08-27 1988-03-11 Pentel Kk Ink composition for screen printing

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS4957910A (en) * 1972-08-22 1974-06-05

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS4957910A (en) * 1972-08-22 1974-06-05

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6356579A (en) * 1986-08-27 1988-03-11 Pentel Kk Ink composition for screen printing

Also Published As

Publication number Publication date
JPH0121193B2 (en) 1989-04-20

Similar Documents

Publication Publication Date Title
KR910004304A (en) Abrasive article with conductive coating
DE2530657C2 (en) Process for the production of a flexible foam material
KR960022876A (en) Compound Powder Coating
JPS5699692A (en) Recording medium for ink jet recording
JPS57173194A (en) Recording material for ink jet recording
JPS5792066A (en) Paste ink composition for screen print
GB1569943A (en) Decorative sheet-type material containing chips and process for making same
GB1410202A (en) Method for manufacturing plastisol resins
JPS57135878A (en) Erasable ball point pen ink composition
US5084501A (en) Highly filled resin powder
KR870011394A (en) Anti-shake lining material and process for manufacturing anti-shake lining from this material
JP3228962B2 (en) Coating material with excellent ironing workability
JPS5528857A (en) Coloring sheet for pressure-sensitive copying paper
JPS6073940A (en) Decorative board and its production
JPH0780979A (en) Decorative material
JPS5626942A (en) Vinyl chloride plastisol composition
JPS56129059A (en) Production of three-dimensionally patterned decorative sheet excellent in abrasion resistance
JPS6418631A (en) Polyester film having coated layer and containing fine air bubble
JP2910906B2 (en) Film forming composition and film forming method
JPS578229A (en) Foam having woody texture
JPS57188435A (en) Manufacture of colored fine hollow sphere
JPS5773033A (en) Talc-containing propylene polymer composition
KR900010635A (en) Sangsang keyboard materials and manufacturing method thereof
JPS57177070A (en) Coating material for blackboard
JPS55255A (en) Method of making fire-retarding plastic resin insulation material