JPS5743921A - Operating method for bottom-blown oxygen converter - Google Patents
Operating method for bottom-blown oxygen converterInfo
- Publication number
- JPS5743921A JPS5743921A JP11952080A JP11952080A JPS5743921A JP S5743921 A JPS5743921 A JP S5743921A JP 11952080 A JP11952080 A JP 11952080A JP 11952080 A JP11952080 A JP 11952080A JP S5743921 A JPS5743921 A JP S5743921A
- Authority
- JP
- Japan
- Prior art keywords
- refining
- steel
- final period
- tuyere
- flow rate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To contrive to enhance the efficiency of decarburization particularly in the final period of blow refining by increasing the flow rate of a hydrocarbon gas blown- in in the final period of blow refining in which the C content of the molten steel is decreases to 0.1% or below, when refining a steel by blowing-in O2 and the hydrocarbon gas through a double-walled cylindrical tuyere provided at the bottom of a converter. CONSTITUTION:The steel is refined by simultaneously blowing-in a refining O2 gas through an inner pipe of the double-walled cylindrical tuyere provided at the bottom of the converter and blowing-in a tuyere-cooling gas based on a hydrocarbon such as propane through an outer pipe of the tuyere. In the final period of the blow refining in which the C content of the molten steel is reduced to 0.1% or below, the steel in the low carbon region is refined by increasing the flow rate of the blown-in hydrocarbon gas relative to the flow rate of O2 within the range of not more than 10%. As a result, the efficiency of decarburization in the final period of blow refining is enhanced and the iron content of the slag is lowered.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11952080A JPS5743921A (en) | 1980-08-29 | 1980-08-29 | Operating method for bottom-blown oxygen converter |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11952080A JPS5743921A (en) | 1980-08-29 | 1980-08-29 | Operating method for bottom-blown oxygen converter |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5743921A true JPS5743921A (en) | 1982-03-12 |
JPS629644B2 JPS629644B2 (en) | 1987-03-02 |
Family
ID=14763301
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11952080A Granted JPS5743921A (en) | 1980-08-29 | 1980-08-29 | Operating method for bottom-blown oxygen converter |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5743921A (en) |
-
1980
- 1980-08-29 JP JP11952080A patent/JPS5743921A/en active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS629644B2 (en) | 1987-03-02 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS57145917A (en) | Refining method for high chromium steel | |
DE3567031D1 (en) | Process for refining pig iron | |
JPS5743921A (en) | Operating method for bottom-blown oxygen converter | |
TW346505B (en) | Process for producing low-carbon chromium-containing steel | |
ES409323A1 (en) | Method of obtaining low-phosphorus contents in medium-and high-carbon steels in a bottom-blown oxygen steelmaking furnace | |
JPS5432119A (en) | Refining method for high chromium steel | |
EP0087328B1 (en) | Process to produce low hydrogen steel by argon-oxygen decarburization | |
JPS55164017A (en) | Gas blow-in tuyere for refining | |
JPS5594425A (en) | Converter steel making method which reduces phosphorus content | |
JPS6442511A (en) | Secondary combustion method in converter | |
JPS55107715A (en) | Blowing method of dephosphorizer to bottom blowing converter | |
Abel | Physical modeling of bottom-blown continuous steelmaking. I. The decarburization reaction model and water modeling results | |
JPS552759A (en) | Manufacture of ultra-low-carbon stainless steel | |
KR970043125A (en) | Slag deoxidation method of ultra low carbon molten steel | |
SU908831A2 (en) | Process for melting steel | |
Becvar et al. | Comparison of Production Methods of Killed Steel With Sulfur Content Below 0. 005% in Oxygen Converters or Double-Hearth Furnaces by Desulfurizing the Iron or the Steel in the Ladle | |
Messing | Ladle Degassing in Secondary Metallurgy | |
JPS56127711A (en) | Blast furnace operation process | |
Kumar et al. | Effect of Slag Composition and Vacuum on the Deoxidation Behavior of High Carbon Steel | |
JPS5798618A (en) | Decarbulizing refining method for molten pig iron that enlarges reserve heat | |
JPS5665914A (en) | Production of low carbon stainless steel | |
GB1188680A (en) | Improvements in or relating to the Removal of Oxygen from Metals | |
JPH0254725A (en) | Method for preventing foaming of molten slag | |
Gray et al. | Ladle Refining: Application to Desulphurisation and Degassing | |
Riha et al. | Oxygen Converter Alloy Steel Process in Iron and Steel Plant at Trinec |