JPS57179011A - Steam cured calcium silicate compound with superior carbonation resistance - Google Patents

Steam cured calcium silicate compound with superior carbonation resistance

Info

Publication number
JPS57179011A
JPS57179011A JP6469881A JP6469881A JPS57179011A JP S57179011 A JPS57179011 A JP S57179011A JP 6469881 A JP6469881 A JP 6469881A JP 6469881 A JP6469881 A JP 6469881A JP S57179011 A JPS57179011 A JP S57179011A
Authority
JP
Japan
Prior art keywords
compound
mixture
calcium silicate
silicate compound
starting materials
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP6469881A
Other languages
Japanese (ja)
Inventor
Hiromasa Yoshikawa
Yoichi Oya
Yosuke Tagawa
Sadahiro Iida
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sumitomo Metal Mining Co Ltd
Original Assignee
Sumitomo Metal Mining Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Mining Co Ltd filed Critical Sumitomo Metal Mining Co Ltd
Priority to JP6469881A priority Critical patent/JPS57179011A/en
Publication of JPS57179011A publication Critical patent/JPS57179011A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To obtain the titled compound causing no efflorescent phenomenon even if exposed to air over a long term by adding a prescribed percentage of an Sr compound to a slurrified mixture contg. powdered siliceous and calcareous starting materials as principal starting materials.
CONSTITUTION: Water is added to a powdered siliceous starting material such as Portland cement + silica powder and a powdered calcareous starting material such as CaO powder to prepare a slurrified mixture of the starting materials. An Sr compound is added to the mixture by 0.2W5wt% as Sr of the total solid content of the mixture, and they are mixed and subjected to steam curing by an ordinary method to manufacture the desired steam cured calcium silicate compound. SrO or the like is used as said Sr compound. The life of tobermorite in the calcium silicate compound is elongated by about 2 times that of conventional tobermorite under severe conditions, so the carbonation resistance is enhanced correspondingly.
COPYRIGHT: (C)1982,JPO&Japio
JP6469881A 1981-04-28 1981-04-28 Steam cured calcium silicate compound with superior carbonation resistance Pending JPS57179011A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP6469881A JPS57179011A (en) 1981-04-28 1981-04-28 Steam cured calcium silicate compound with superior carbonation resistance

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP6469881A JPS57179011A (en) 1981-04-28 1981-04-28 Steam cured calcium silicate compound with superior carbonation resistance

Publications (1)

Publication Number Publication Date
JPS57179011A true JPS57179011A (en) 1982-11-04

Family

ID=13265623

Family Applications (1)

Application Number Title Priority Date Filing Date
JP6469881A Pending JPS57179011A (en) 1981-04-28 1981-04-28 Steam cured calcium silicate compound with superior carbonation resistance

Country Status (1)

Country Link
JP (1) JPS57179011A (en)

Similar Documents

Publication Publication Date Title
DK336185A (en) HYDRAULIC CEMENT
IN168130B (en)
DE3269107D1 (en) Masonry cement composition, masonry construction and method
JPS57179011A (en) Steam cured calcium silicate compound with superior carbonation resistance
EP0384898B1 (en) Cementitious material for masonry constructions
JPS57179010A (en) Steam cured calcium silicate compound with superior carbonation resistance
JPS57179009A (en) Steam cured calcium silicate compound with superior carbonation resistance
JPS57179012A (en) Steam cured calcium silicate compound with superior carbonation resistance
WO1997017307A3 (en) Method for preparing hardened granules from a particulate material
JPS57179013A (en) Steam cured calcium silicate compound with superior carbonation resistance
JPS5578083A (en) Stabilization of soil
FR2228734A1 (en) Lightweight plaster-mortar composition - containing expanded granules, filler, lime, cellulose ether, surfactant cement
JPS5712024A (en) Resin composition having good adhesiveness to moistured surface
SU1291575A1 (en) Mortar
JP2899066B2 (en) Waterproofing admixture and waterproofing composition
GB1550003A (en) Lightweight aggregates
SU1250543A1 (en) Gypsum binder
SU1203067A1 (en) Heat-resistant concrete mix
DE3472945D1 (en) Process for the quick and controlled setting of a hydraulic binder containing both portland cement and alumina cement, hydraulic binder, as well as a process for the manufacture of building elements
JPS577815A (en) Calcium silicate hydrate-base aggregate
JPS51126986A (en) Adhesive water repellents
SU1608158A1 (en) Initial composition for producing unfired aggregate
JPS53106400A (en) Preparation of calcium silicate
JPS56104710A (en) Preparation of calcium silicate fiber
RU2023696C1 (en) Binder