JPS5687624A - Heat treatment of ni-containing barlike steel product - Google Patents
Heat treatment of ni-containing barlike steel productInfo
- Publication number
- JPS5687624A JPS5687624A JP16468279A JP16468279A JPS5687624A JP S5687624 A JPS5687624 A JP S5687624A JP 16468279 A JP16468279 A JP 16468279A JP 16468279 A JP16468279 A JP 16468279A JP S5687624 A JPS5687624 A JP S5687624A
- Authority
- JP
- Japan
- Prior art keywords
- steel product
- barlike
- contg
- heat treatment
- temp
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To improve impact toughness while maintaining high productivity by maintaining an Ni-contg. barlike steel product for a specific time in a specific temp. region right after the passage of the steel product through an induction heating coil at the time of continuously tempering said steel material in said specific temp. region through induction heating while conveying the same at specific speed.
CONSTITUTION: While an Ni-contg. barlike steel product contg. 0.5W20% Ni is being conveyed at ≥30mm/sec. conveying speed, it is continuously tempered in (Ac1-50°C)WAc1 temp. region. At this time, the barlike steel product is held for ≥15 seconds at said temp. region right after it has passed the induction heating coil. In this way, the heat treatment furnace is installed just behind tempering coil, and the time when the steel product passes the heat treatment furnace according to its conveying speed is made at least 15 seconds and more, whereby the Ni-contg. barlike steel product having high impact toughness is obtained.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16468279A JPS5687624A (en) | 1979-12-20 | 1979-12-20 | Heat treatment of ni-containing barlike steel product |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP16468279A JPS5687624A (en) | 1979-12-20 | 1979-12-20 | Heat treatment of ni-containing barlike steel product |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5687624A true JPS5687624A (en) | 1981-07-16 |
Family
ID=15797842
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP16468279A Pending JPS5687624A (en) | 1979-12-20 | 1979-12-20 | Heat treatment of ni-containing barlike steel product |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5687624A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03274221A (en) * | 1990-03-23 | 1991-12-05 | Fuji Denshi Kogyo Kk | Method and apparatus for high-frequency shifting quenching and tempering |
-
1979
- 1979-12-20 JP JP16468279A patent/JPS5687624A/en active Pending
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH03274221A (en) * | 1990-03-23 | 1991-12-05 | Fuji Denshi Kogyo Kk | Method and apparatus for high-frequency shifting quenching and tempering |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES344302A1 (en) | Method of bending glass sheets | |
JPS52105520A (en) | Continuous casting and continuous hot rolling of aluminium-killed stee l | |
JPS5687624A (en) | Heat treatment of ni-containing barlike steel product | |
JPS51148611A (en) | Heat-treatment process of steel | |
JPS5582725A (en) | Hardening unit | |
JPS51140817A (en) | Martensite tool steel for hot forming | |
ES8202367A1 (en) | Continuous heat treatment plant for steel sheet | |
GB933244A (en) | Process of hardening alloy steels | |
JPS52138013A (en) | Continuous annealing equipment | |
JPS56150127A (en) | Direct normalizing method | |
JPS51112413A (en) | Method of continuous annealing steel strip | |
JPS56102526A (en) | Heat treating apparatus of metallic strip | |
ES466565A1 (en) | Perfected procedure of laminated wire treatment. (Machine-translation by Google Translate, not legally binding) | |
JPS5485116A (en) | Heat treating method for large-sized steel pipe | |
JPS54112364A (en) | Roll for sendzimir mill and its heat treating method | |
JPS5328506A (en) | Induction heating method | |
GB1263460A (en) | Improvements in or relating to apparatus for hardening metal articles | |
JPS5220912A (en) | Method of operating metal heating furnaces | |
JPS5722895A (en) | Method for forming high strength and high toughness welding metal | |
JPS56166319A (en) | Manufacture of nonrefined steel | |
JPS5518543A (en) | Heat-treating method | |
JPS5337511A (en) | Heat treating equipment for steel sheet | |
JPS5690964A (en) | Production of high tensile aluminum hot dipped sheet steel of low yield ratio | |
JPS5325218A (en) | Spheroidizing heat treating method for wire by strand method | |
ES8206644A1 (en) | Manufacture of rolled steel products having good weldability, a high elastic limit, and toughness at very low temperatures |