JPS5674356A - Production of continuously cast ingot free from any sectional defect and surface defect - Google Patents
Production of continuously cast ingot free from any sectional defect and surface defectInfo
- Publication number
- JPS5674356A JPS5674356A JP14944279A JP14944279A JPS5674356A JP S5674356 A JPS5674356 A JP S5674356A JP 14944279 A JP14944279 A JP 14944279A JP 14944279 A JP14944279 A JP 14944279A JP S5674356 A JPS5674356 A JP S5674356A
- Authority
- JP
- Japan
- Prior art keywords
- ingot
- water
- narrow
- cooling
- face width
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To prevent sectional defects and surface defects from occuring on a steel ingot by water cooling the narrow surfaces of the specific range below meniscus at the time of continuously casting a steel ingot of <=4 in ratio between broad face width and narrow face width. CONSTITUTION:At the time of producing a steel ingot of >= in ratio between broad face width and narrow face width by a continuous casting method, the continuously cast ingot narrow surfaces of a range up to 2/3.t<2>/K<2>.Vc from below the surface (meniscus) of the molten metal in the mold are water cooled within a range exceeding a fixed value in which the cooling water ratio of the broad faces is determined by kinds of steel, the thickness of the ingot, the casting speed, and the shape of an immersion nozzle for casting to the mold. [(t); ingot thickness, K; coefficient of solidification, Vc; casting speed]. The formation of the sectional defects and surface defects occuring in the pore groups at the final solidifying of the ingot may be prevented by regulating the flow of the water for cooling the narrow faces according to the flow of the water for cooling the broad faces in this way.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14944279A JPS5674356A (en) | 1979-11-20 | 1979-11-20 | Production of continuously cast ingot free from any sectional defect and surface defect |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14944279A JPS5674356A (en) | 1979-11-20 | 1979-11-20 | Production of continuously cast ingot free from any sectional defect and surface defect |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5674356A true JPS5674356A (en) | 1981-06-19 |
Family
ID=15475197
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP14944279A Pending JPS5674356A (en) | 1979-11-20 | 1979-11-20 | Production of continuously cast ingot free from any sectional defect and surface defect |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5674356A (en) |
-
1979
- 1979-11-20 JP JP14944279A patent/JPS5674356A/en active Pending
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US5592988A (en) | Method for the continuous casting of peritectic steels | |
US5598885A (en) | Method for the continuous casting of high-carbon steels | |
US3891024A (en) | Method for the continuous casting of metal ingots or strips | |
JPS5674356A (en) | Production of continuously cast ingot free from any sectional defect and surface defect | |
US3940976A (en) | Method of determining the suitability of continuously cast slabs of Al- or Al-Si-killed soft steel for producing cold rolled sheets to be tinned | |
CA2071902A1 (en) | Method of controlling the rate of heat extraction in mould casting | |
JPS5568156A (en) | Production of slab for clad steel plate in continuous casting method | |
JPS5762804A (en) | Continuous casting method for cast steel ingot having excellent sour resisting characteristic | |
JPS5611134A (en) | Solidifying method for metal | |
JPS6466061A (en) | Production of ingot having double layers | |
JPS6483339A (en) | Method for continuously casting steel strip | |
JPS55109549A (en) | Continuous casting method of sheet | |
JPS5684157A (en) | Horizontal continuous casting method of molten metal | |
JPS56139268A (en) | Continuous casting method | |
JPS5741848A (en) | Mold for horizontal continuous casting | |
SU1038064A1 (en) | Motor non-chilled complex-configuration iron castings | |
JPS5794448A (en) | Manufacture of high chrome ferritic stainless steel ingot | |
Mairy et al. | Lubrication Control in Caster Molds With the M. L. Tektor | |
SU831294A1 (en) | Metal continuous casting method | |
FR2333596A1 (en) | Casting flat horizontal ingots with good surfaces - where ingot moulds travel through a casting tunnel fed with a coolant | |
Minkoff et al. | Solidification/liquid state processes | |
JPS5719142A (en) | Manufacture of continuous ingot superior in surface characteristic | |
JPS5623217A (en) | Pouring starting method of continuous casting | |
FR2448952A1 (en) | Steel slab continuously cast in a mould which moves continuously - and has an endless surface moving cooperatively with other surfaces to form the mould | |
Takeuchi et al. | Continuous Casting of Composite Metal Material |