JPS5666649A - Preventing method for dew condensation - Google Patents
Preventing method for dew condensationInfo
- Publication number
- JPS5666649A JPS5666649A JP14278479A JP14278479A JPS5666649A JP S5666649 A JPS5666649 A JP S5666649A JP 14278479 A JP14278479 A JP 14278479A JP 14278479 A JP14278479 A JP 14278479A JP S5666649 A JPS5666649 A JP S5666649A
- Authority
- JP
- Japan
- Prior art keywords
- film layer
- dew condensation
- transparent thin
- laminate body
- preventing method
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE: To prevent the dew condensation effectively by a method wherein a laminate body is formed by covering a metal thin-film layer with a transparent thin- film layer and this laminate body is provided on the surface of the base body of a formed article.
CONSTITUTION: The laminate body is constituted by covering the surface of the metal thin-film layer whose main constituent is gold, silver, copper or the like with the transparent thin-film layer and is provided on the surface of the base body of the formed article. By this constitution, the dew condensation can be prevented effectively by the action of such property of the transparent thin-film layer as transmitting light selectively.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14278479A JPS5666649A (en) | 1979-11-06 | 1979-11-06 | Preventing method for dew condensation |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14278479A JPS5666649A (en) | 1979-11-06 | 1979-11-06 | Preventing method for dew condensation |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5666649A true JPS5666649A (en) | 1981-06-05 |
Family
ID=15323513
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP14278479A Pending JPS5666649A (en) | 1979-11-06 | 1979-11-06 | Preventing method for dew condensation |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5666649A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60242286A (en) * | 1984-05-14 | 1985-12-02 | 帝人株式会社 | Window |
WO2017135441A1 (en) * | 2016-02-05 | 2017-08-10 | 積水化学工業株式会社 | Interlayer for laminated glass, and laminated glass |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS53119987A (en) * | 1977-03-28 | 1978-10-19 | Teijin Ltd | Laminate |
-
1979
- 1979-11-06 JP JP14278479A patent/JPS5666649A/en active Pending
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS53119987A (en) * | 1977-03-28 | 1978-10-19 | Teijin Ltd | Laminate |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS60242286A (en) * | 1984-05-14 | 1985-12-02 | 帝人株式会社 | Window |
WO2017135441A1 (en) * | 2016-02-05 | 2017-08-10 | 積水化学工業株式会社 | Interlayer for laminated glass, and laminated glass |
CN108473372A (en) * | 2016-02-05 | 2018-08-31 | 积水化学工业株式会社 | Intermediate film for laminated glasses and laminated glass |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB2078612B (en) | Self-adhesive roofing laminates having metal layer therein | |
DE3679280D1 (en) | ITEM WITH WEAR PROTECTIVE LAYER FROM PRECIOUS METAL. | |
EP0098795A3 (en) | Time piece and method of manufacturing the same | |
JPS5438593A (en) | Distribution track | |
DE68911669T2 (en) | Flexible hose with an outer layer containing pieces of metal. | |
JPS56125298A (en) | Growth of metal layer or alloy layer on substrate | |
JPS53121034A (en) | Surface treatment of metal | |
JPS5666649A (en) | Preventing method for dew condensation | |
JPS53141369A (en) | Treatment of article with thermosetting resin | |
JPS5425979A (en) | Preparation of multi-layer film | |
JPS53115627A (en) | Silver surface protective film | |
JPS5466536A (en) | Window | |
JPS5249991A (en) | Sputtering method | |
JPS52121685A (en) | Article coated with fluorine resin | |
JPS5428378A (en) | Laminate with improved wearing resistance | |
JPS5291666A (en) | Photodiode | |
JPS5428238A (en) | Watchcase | |
JPS5441673A (en) | Semiconductor device and its manufacture | |
JPS5421272A (en) | Metal photo mask | |
JPS57130232A (en) | Magnetic recording medium | |
JPS52130662A (en) | Dials for clocks | |
JPS53116068A (en) | Insb polycrystal thin film of low noise | |
JPS5472676A (en) | Lead frame having alloy intermediate layer | |
JPS5421290A (en) | Integrated circuit device and its manufacture | |
JPS55116644A (en) | Mirror plate |