JPS56161868A - Formation of composite paint film - Google Patents
Formation of composite paint filmInfo
- Publication number
- JPS56161868A JPS56161868A JP6425680A JP6425680A JPS56161868A JP S56161868 A JPS56161868 A JP S56161868A JP 6425680 A JP6425680 A JP 6425680A JP 6425680 A JP6425680 A JP 6425680A JP S56161868 A JPS56161868 A JP S56161868A
- Authority
- JP
- Japan
- Prior art keywords
- paint
- paint film
- preheating
- temperature
- thickness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To easily obtain a paint film applicable to line coating, in recoating an alkyl silicate-bonded zinc powder paint film on a thick metal article with a variety of paints, by preheating the metal article to be coated at a proper temperature.
CONSTITUTION: A metal plate or rod having a thickness or diameter of about 4mm or more is preheated at 40W90°C. When a zinc powder paint containing ethyl silicate or the like as a binder is applied onto the surface of the metal article, a solvent is rapidly dispersed by the preheat and the applied paint layer becomes recoatable within a very short period. Just thereafter, the uncured paint film P is coated with an aqueous dispersion paint T drying at an ordinary temperature, e.g. an acrylic- modified alkyd resin or the like, so that a dry paint film will have a thickness of 30W300μ. The said preheating enables the apply of a paint film having an objective thickness, raises a temperature of moisture in the paint film T penetrating into or being in contact with the paint film P, and accelerates the curing of the paint film P and the drying of the paint T. If the preheating temperature is below the lower limit, these effects are not attained. If the preheating temperature exceeds the upper limit, both of the paint films are not obtained in a uniform and normal state, and the dispersion of moisture from the paint T is too rapid to expect a sufficient curing effect of the paint film P.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6425680A JPS5822269B2 (en) | 1980-05-15 | 1980-05-15 | Method of forming composite coating film |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP6425680A JPS5822269B2 (en) | 1980-05-15 | 1980-05-15 | Method of forming composite coating film |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS56161868A true JPS56161868A (en) | 1981-12-12 |
JPS5822269B2 JPS5822269B2 (en) | 1983-05-07 |
Family
ID=13252908
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP6425680A Expired JPS5822269B2 (en) | 1980-05-15 | 1980-05-15 | Method of forming composite coating film |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5822269B2 (en) |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2002083799A1 (en) * | 2001-04-10 | 2002-10-24 | N.V. Bekaert S.A. | Coated metal wire |
JP2013500154A (en) * | 2009-07-27 | 2013-01-07 | エーヴァルト デルケン アーゲー | Method and apparatus for applying at least one anticorrosive liquid coating comprising metal particles to a workpiece. |
WO2013066141A1 (en) * | 2011-11-04 | 2013-05-10 | Saenz Chapa Armando | Continuous method for applying coatings to a metal element |
JP2017186480A (en) * | 2016-04-08 | 2017-10-12 | 中国塗料株式会社 | Method for manufacturing steel plate with anticorrosive coating film |
JP2019034289A (en) * | 2017-08-21 | 2019-03-07 | 株式会社Ihi | Method for forming ground coat, and ground coat |
-
1980
- 1980-05-15 JP JP6425680A patent/JPS5822269B2/en not_active Expired
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2002083799A1 (en) * | 2001-04-10 | 2002-10-24 | N.V. Bekaert S.A. | Coated metal wire |
JP2013500154A (en) * | 2009-07-27 | 2013-01-07 | エーヴァルト デルケン アーゲー | Method and apparatus for applying at least one anticorrosive liquid coating comprising metal particles to a workpiece. |
WO2013066141A1 (en) * | 2011-11-04 | 2013-05-10 | Saenz Chapa Armando | Continuous method for applying coatings to a metal element |
JP2015501219A (en) * | 2011-11-04 | 2015-01-15 | チャパ アルマンド サエンス | A continuous method for applying paint to metal elements |
EP2774691A4 (en) * | 2011-11-04 | 2016-06-29 | Chapa Armando Saenz | Continuous method for applying coatings to a metal element |
JP2017186480A (en) * | 2016-04-08 | 2017-10-12 | 中国塗料株式会社 | Method for manufacturing steel plate with anticorrosive coating film |
JP2019034289A (en) * | 2017-08-21 | 2019-03-07 | 株式会社Ihi | Method for forming ground coat, and ground coat |
Also Published As
Publication number | Publication date |
---|---|
JPS5822269B2 (en) | 1983-05-07 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DE69322618D1 (en) | COATED FILM AND ITS PRODUCTION PROCESS | |
CA2349233A1 (en) | In-press process for coating composite substrates | |
GR76013B (en) | ||
JPS56161868A (en) | Formation of composite paint film | |
JPS5735971A (en) | Formation of slipery thin film | |
JPS54131640A (en) | Roller coating of multicolor paint | |
JPS56150465A (en) | Decorative board | |
JPS5453153A (en) | Method of finishing anticorrosion lining | |
DE3112658C1 (en) | Metal registration papers and processes for their manufacture | |
JPS57135190A (en) | Manufacture of recording sheet | |
JPS54138039A (en) | Coating of welded seam papt of metallic container | |
JPS5531809A (en) | Composition for can | |
JPS5551463A (en) | Manufacture of precoat metal | |
JPS5531418A (en) | Corrosion resistant coating layer on metal container | |
JPS5670877A (en) | Formation of three dimensional pattern to surface of substrate | |
JPS5511038A (en) | Coating method of metal can, metal can member, or sheet material for metal can with slurry paint | |
JPS56130277A (en) | Formation of composite inorganic-organic coating film by impregnating organic resin to inorganic zinc rich primer coating film | |
JPS58205567A (en) | Pattern forming method | |
JPS5520650A (en) | Pattern forming method | |
US3074813A (en) | Method for the coating of sheets and strips with thermoplastic synthetic high polymers | |
JPS5778979A (en) | Method for coating conductive resin | |
JPS5547372A (en) | Damping method for steel plate | |
JPS57140677A (en) | Production of decorative sheet | |
JPS5765354A (en) | Formation of hardened paint film | |
JPS56130270A (en) | Coating method of improved stucco |