JPS5581002A - Method and apparatus for broadside reduction rolling - Google Patents
Method and apparatus for broadside reduction rollingInfo
- Publication number
- JPS5581002A JPS5581002A JP15551178A JP15551178A JPS5581002A JP S5581002 A JPS5581002 A JP S5581002A JP 15551178 A JP15551178 A JP 15551178A JP 15551178 A JP15551178 A JP 15551178A JP S5581002 A JPS5581002 A JP S5581002A
- Authority
- JP
- Japan
- Prior art keywords
- broadside
- rolling
- reduction rolling
- rolls
- biting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To reduce the fishtail part length produced at the trailing end of material and suppress the build-up of dog-bone part by coating the lubricating material for lowering the coefficient of rolling friction on vertical roll surfaces at the time of performing broadside reduction rolling through the use of the vertical rolls.
CONSTITUTION: When material 1 is bitten to vertical rolls 4, it is accomplished in the absence of lubrication but after the biting of the material 1, the confirmation of the bite by the signal of a load cell 8 causes the valve 9 of a nozzle 5 for lubricant coating is opened and the lubricating material is coated from the nozzle 5 on the roll 4 surface. As a result of this, the rolling through the use of the lubricating material is done after the biting of the material and since this becomes the broadside reduction rolling of a smaller coefficient of friction between the material 1 and the rolls 4, the rolled material of the small fishtail length at the trailing end and dog- bone end part length of the material 1 is obtainable.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15551178A JPS5581002A (en) | 1978-12-13 | 1978-12-13 | Method and apparatus for broadside reduction rolling |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP15551178A JPS5581002A (en) | 1978-12-13 | 1978-12-13 | Method and apparatus for broadside reduction rolling |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5581002A true JPS5581002A (en) | 1980-06-18 |
JPS6247081B2 JPS6247081B2 (en) | 1987-10-06 |
Family
ID=15607640
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP15551178A Granted JPS5581002A (en) | 1978-12-13 | 1978-12-13 | Method and apparatus for broadside reduction rolling |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5581002A (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS62248531A (en) * | 1986-04-18 | 1987-10-29 | Ishikawajima Harima Heavy Ind Co Ltd | Method and apparatus for width reduction |
-
1978
- 1978-12-13 JP JP15551178A patent/JPS5581002A/en active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS62248531A (en) * | 1986-04-18 | 1987-10-29 | Ishikawajima Harima Heavy Ind Co Ltd | Method and apparatus for width reduction |
Also Published As
Publication number | Publication date |
---|---|
JPS6247081B2 (en) | 1987-10-06 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5581002A (en) | Method and apparatus for broadside reduction rolling | |
JPS53112253A (en) | Controlling method for interstand tension in continuous rolling mill | |
JPS579662A (en) | Recording paper curl eliminating equipment | |
JPS57199501A (en) | Hot oil-lubricated rolling method | |
JPS54102270A (en) | Controlling method for rolling reduction in pipe forming mill | |
JPS56165502A (en) | Manufacture of cold rolled titanium sheet | |
JPS55106611A (en) | Determining method for piercing condition of skew roll piercer | |
JPS5736009A (en) | Controlling method for thickness of sheet rolled by rolling mill | |
JPS5772720A (en) | Manufacture of cold rolled steel strip | |
JPS56158204A (en) | Asymmetrical rolling method for strip | |
JPS54133455A (en) | Method and apparatus for rolling | |
JPS5668523A (en) | Pointed part forming method of blank material for drawing | |
JPS57112918A (en) | Hot rolling method | |
JPS57106407A (en) | Bright rolling method | |
JPS57112905A (en) | Cold rolling method by high screw down | |
JPS5641052A (en) | Twin roll type rolling device | |
JPS53118257A (en) | Method of preventing occurrence of surface flaw in continuous steel-plate treating line | |
JPS5689302A (en) | Preventing method for steel strip from heat scratch due to cold rolling work | |
JPS5788915A (en) | Method for coiling steel sheet with less surface flaw | |
JPS57109501A (en) | Rolling method for tri-star rolling mill | |
JPS54103768A (en) | Continuous pipe rolling and apparatus therefor | |
JPS55151093A (en) | Lubrication of sheet material in cold rolling | |
JPH0416518B2 (en) | ||
Mazur et al. | The Effects of Roughness of the Rolls and Strip During Rolling with Lubricant | |
JPS57106415A (en) | Continuous manufacture of seamless steel pipe having outer diameter of different dimension |