JPS555829A - Surface protective agent for flat printing plate - Google Patents

Surface protective agent for flat printing plate

Info

Publication number
JPS555829A
JPS555829A JP7831278A JP7831278A JPS555829A JP S555829 A JPS555829 A JP S555829A JP 7831278 A JP7831278 A JP 7831278A JP 7831278 A JP7831278 A JP 7831278A JP S555829 A JPS555829 A JP S555829A
Authority
JP
Japan
Prior art keywords
water soluble
surface protective
protective agent
high molecular
image portion
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP7831278A
Other languages
Japanese (ja)
Other versions
JPS6145554B2 (en
Inventor
Nobuyuki Kita
Fumihiro Tokunaga
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Fujifilm Holdings Corp
Original Assignee
Fuji Photo Film Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fuji Photo Film Co Ltd filed Critical Fuji Photo Film Co Ltd
Priority to JP7831278A priority Critical patent/JPS555829A/en
Publication of JPS555829A publication Critical patent/JPS555829A/en
Publication of JPS6145554B2 publication Critical patent/JPS6145554B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE: To obtain a surface protective agent for eliminating stains at non-image portion by diffusing alkali soluble resin into the aqueous solution of water soluble high molecular compound, thereby increasing the fat unsensitivity at the non-image portion without decreasing the fat sensitivity at the image portion.
CONSTITUTION: Preferably 0.1W20 wt% of an alkali soluble resin such as phenol formaldehyde resin and polyhydroxystyrene is diffused into the aqueous solution of a water soluble high molecular compound such as a water soluble cellulose ether. If desired, for example, 0.1W0.5 wt% of moistening agent such as polyhydric alcohol may be further added. It is preferable that the above-stated water soluble high molecular compound should be of 10W20 wt%.
COPYRIGHT: (C)1980,JPO&Japio
JP7831278A 1978-06-28 1978-06-28 Surface protective agent for flat printing plate Granted JPS555829A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP7831278A JPS555829A (en) 1978-06-28 1978-06-28 Surface protective agent for flat printing plate

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP7831278A JPS555829A (en) 1978-06-28 1978-06-28 Surface protective agent for flat printing plate

Publications (2)

Publication Number Publication Date
JPS555829A true JPS555829A (en) 1980-01-17
JPS6145554B2 JPS6145554B2 (en) 1986-10-08

Family

ID=13658410

Family Applications (1)

Application Number Title Priority Date Filing Date
JP7831278A Granted JPS555829A (en) 1978-06-28 1978-06-28 Surface protective agent for flat printing plate

Country Status (1)

Country Link
JP (1) JPS555829A (en)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61189996A (en) * 1985-02-18 1986-08-23 Fuji Photo Film Co Ltd Surface protective agent for planographic printing plate
JPS6211693A (en) * 1985-07-10 1987-01-20 Fuji Photo Film Co Ltd Surface protective agent for planographic printing plate
JPS6219494A (en) * 1985-07-18 1987-01-28 Fuji Photo Film Co Ltd Base material for lithographic printing
JPH0261130A (en) * 1988-08-25 1990-03-01 Teijin Seiki Co Ltd Thermal regulator for heating rotator

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61189996A (en) * 1985-02-18 1986-08-23 Fuji Photo Film Co Ltd Surface protective agent for planographic printing plate
JPH0527557B2 (en) * 1985-02-18 1993-04-21 Fuji Photo Film Co Ltd
JPS6211693A (en) * 1985-07-10 1987-01-20 Fuji Photo Film Co Ltd Surface protective agent for planographic printing plate
JPH0517875B2 (en) * 1985-07-10 1993-03-10 Fuji Photo Film Co Ltd
JPS6219494A (en) * 1985-07-18 1987-01-28 Fuji Photo Film Co Ltd Base material for lithographic printing
JPH0528196B2 (en) * 1985-07-18 1993-04-23 Fuji Photo Film Co Ltd
JPH0261130A (en) * 1988-08-25 1990-03-01 Teijin Seiki Co Ltd Thermal regulator for heating rotator

Also Published As

Publication number Publication date
JPS6145554B2 (en) 1986-10-08

Similar Documents

Publication Publication Date Title
JPS55115045A (en) Printing plate preparation
KR880014419A (en) Radiation-sensitive recording materials
JPS555829A (en) Surface protective agent for flat printing plate
JPS53123456A (en) Aqueous diamine dispersion
JPS5635129A (en) Positive type photosensitive composition
JPS57185432A (en) Support for use in photographic paper
JPS5430220A (en) Preparation of dye composition
JPS5545626A (en) Poultice
JPS5380493A (en) Preparation of hydrophilic crosslinked polymer
JPS53134785A (en) Deforming agent
JPS53143693A (en) Preparation of resol-type phenolic resin
JPS5428392A (en) Preparation of resol-type phenolic resin
JPS54136153A (en) Multiple processor
JPS5678837A (en) Hardening method of resist film
JPS56140905A (en) Termite-killing agent composition
JPS53101061A (en) Resin composition for mechanical foam coating
JPS5392892A (en) Preparation of water-soluble melamine-phenol condensation resin having improved storage stability
JPS53143631A (en) Fire-resistant composition
JPS5329356A (en) Resol resin compositions
JPS55129410A (en) Preparation of plasticized modified phenolic resin
JPS5321250A (en) Dissolution of polyvinyl alcohol resin powder
JPS5432598A (en) Preparation of polyoxyalkylene glycol diether
JPS52111508A (en) Preparation of magnesium alkoxides
JPS53136008A (en) Emulsion fuel
JPS5612638A (en) Photosensitive composition