Japan
Prior art keywords
emery cloth
grain
cloth paper
life
sticked
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP12231978A
Other languages
Japanese (ja)
Inventor
Masatoshi Ando
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to JP12231978A priority Critical patent/JPS5548578A/en
Publication of JPS5548578A publication Critical patent/JPS5548578A/en
Pending legal-status Critical Current

Links

Abstract

PURPOSE: To obtain sharp and long-life emery cloth paper sticked with compound grain to meet the life of base of emery cloth paper in which strong base is used.
CONSTITUTION: Emery cloth paper is obtained to stick spherical compound grain uneven in a single layer on the surface of the base by bonding agent. The grain is obtained through that abrasives of #320 grain is put in the hot water at approx. 50°C or brine, mixed up to disperse, resin is added as binder, floating one is taken out, dehydrated, bried and sifted in a ranges of 210W297μ in diameter of grain. Grain is sticked without damage of pliability of emery cloth paper prolonged with the life, thus long-life emery cloth paper is obtained.
COPYRIGHT: (C)1980,JPO&Japio
JP12231978A 1978-10-04 1978-10-04 Manufacturing method and product of emery cloth paper sticked with compound grain Pending JPS5548578A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP12231978A JPS5548578A (en) 1978-10-04 1978-10-04 Manufacturing method and product of emery cloth paper sticked with compound grain

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP12231978A JPS5548578A (en) 1978-10-04 1978-10-04 Manufacturing method and product of emery cloth paper sticked with compound grain

Publications (1)

Publication Number Publication Date
JPS5548578A true JPS5548578A (en) 1980-04-07

Family

ID=14833007

Family Applications (1)

Application Number Title Priority Date Filing Date
JP12231978A Pending JPS5548578A (en) 1978-10-04 1978-10-04 Manufacturing method and product of emery cloth paper sticked with compound grain

Country Status (1)

Country Link
JP (1) JPS5548578A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN115319648A (en) * 2022-03-02 2022-11-11 淄博理研泰山涂附磨具有限公司 Long-life abrasive cloth and preparation method thereof
CN115319648B (en) * 2022-03-02 2024-05-10 淄博三共泰山涂附磨具有限公司 Long-service-life abrasive cloth and preparation method thereof

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS52109689A (en) * 1976-02-28 1977-09-14 Carborundum Co Coating grinding material having layer of spherical grinding body

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS52109689A (en) * 1976-02-28 1977-09-14 Carborundum Co Coating grinding material having layer of spherical grinding body

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN115319648A (en) * 2022-03-02 2022-11-11 淄博理研泰山涂附磨具有限公司 Long-life abrasive cloth and preparation method thereof
CN115319648B (en) * 2022-03-02 2024-05-10 淄博三共泰山涂附磨具有限公司 Long-service-life abrasive cloth and preparation method thereof

Similar Documents

Publication Publication Date Title
Will et al. The ecological zones of northern New York.
JPS5548578A (en) Manufacturing method and product of emery cloth paper sticked with compound grain
JPS5548579A (en) Manufacturing method of composite grain and its product
JPS5315691A (en) Method of making resinoid grinding stone
JPS5214295A (en) Grinding finishing apparatus
JPS55120980A (en) Grinder for vertical-axis plane grinding
JPS52138718A (en) Pipe joint
JPS5537239A (en) Manufacturing method of resin-bonded diamond wheel
JPS52103094A (en) Grinding stone
JPS5380889A (en) Cutting and grinding tool
JPS5536576A (en) Artificial soil spraying process jointly using mud layer
JPS5695991A (en) Grinding with polyethylene glycol
JPS52107033A (en) Method of manufacturing slurry-type water dispersed paint
JPS55131472A (en) Grinding and polishing tool
JPS5477390A (en) Resinoid grindstone ingredients
JPS55102370A (en) Preparation of dry solid seasoning
JPS5741171A (en) Grindstone for grinding and cutting
JPS5248889A (en) Electrolytic grinding grindstone
JPS5321284A (en) Synthetic resin impregnated decorative material and preparation thereof
JPS5621777A (en) Manufacturing method for emery cloth and paper
JPS56106931A (en) Preparation of spongy material by wet method
JPS5276792A (en) Method of manufacturing electrodepositing grindstone
Schulz et al. Influence of binder content on the formation and properties of spray granulate
KALMAN DRESSING OF PERLITE- COMMINUTION, CLASSIFICATION, PRE-DRYING AND THE PORE STRUCTURE OF THE EXPANDED PRODUCT
JPS5237294A (en) Grinder for grinding a whole spherical surface