JPS5528554A - Magnetic recording medium - Google Patents

Magnetic recording medium

Info

Publication number
JPS5528554A
JPS5528554A JP10124778A JP10124778A JPS5528554A JP S5528554 A JPS5528554 A JP S5528554A JP 10124778 A JP10124778 A JP 10124778A JP 10124778 A JP10124778 A JP 10124778A JP S5528554 A JPS5528554 A JP S5528554A
Authority
JP
Japan
Prior art keywords
magnetic
powder
lubricant
magnetic layer
perphloro
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP10124778A
Other languages
Japanese (ja)
Inventor
Kunio Mizushima
Taku Yamase
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Maxell Holdings Ltd
Original Assignee
Hitachi Maxell Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hitachi Maxell Ltd filed Critical Hitachi Maxell Ltd
Priority to JP10124778A priority Critical patent/JPS5528554A/en
Publication of JPS5528554A publication Critical patent/JPS5528554A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To increase the wearing properties by mixing the perphloro alkyl polyether and the prescribed aliphatic alcohol as the lubricant into the magnetic layer.
CONSTITUTION: The magnetic coating material composed of the magnetic powder and the binding agent is coated on the substrate such as the polyester film or the like to form the magnetic layer and then to obtain the magnetic tape and the like. Then the double-component system lubricant featuring, for example, 70:30W99.5:0.5 weight ratio between the perphloro polyether and the aliphatic alcohol of the carbon number 12W20 is mixed into the magnetic layer of the above mentioned magnetic tape. The wearing properties can be enhanced more by using the nonmagnetic powder featuring the Mohs' hardness of over 6 together. The quantity of the lubricant to be used is set preferably to 1W25 part by weight to 100 of the magnetic powder, and the nonmagnetic powder is set to 0.5W5wt% to the magnetic powder respectively.
COPYRIGHT: (C)1980,JPO&Japio
JP10124778A 1978-08-19 1978-08-19 Magnetic recording medium Pending JPS5528554A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP10124778A JPS5528554A (en) 1978-08-19 1978-08-19 Magnetic recording medium

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP10124778A JPS5528554A (en) 1978-08-19 1978-08-19 Magnetic recording medium

Publications (1)

Publication Number Publication Date
JPS5528554A true JPS5528554A (en) 1980-02-29

Family

ID=14295567

Family Applications (1)

Application Number Title Priority Date Filing Date
JP10124778A Pending JPS5528554A (en) 1978-08-19 1978-08-19 Magnetic recording medium

Country Status (1)

Country Link
JP (1) JPS5528554A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS59107428A (en) * 1982-12-10 1984-06-21 Seiko Epson Corp Formation of lubricating layer for magnetic recording medium
US7624496B2 (en) * 2003-08-29 2009-12-01 Hitachi Global Storage Technologies Netherlands B.V. Method for efficient slider burnishing during drive build

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS59107428A (en) * 1982-12-10 1984-06-21 Seiko Epson Corp Formation of lubricating layer for magnetic recording medium
JPH0430084B2 (en) * 1982-12-10 1992-05-20
US7624496B2 (en) * 2003-08-29 2009-12-01 Hitachi Global Storage Technologies Netherlands B.V. Method for efficient slider burnishing during drive build

Similar Documents

Publication Publication Date Title
JPS576439A (en) Magnetic recording medium
JPS57133521A (en) Magnetic recording medium
JPS5414711A (en) Magnetic recording medium
JPS5550251A (en) Magnetic toner for electrostatic image development
JPS5668928A (en) Magnetic recording medium
JPS5528554A (en) Magnetic recording medium
JPS5654637A (en) Magnetic recording medium
JPS5528553A (en) Magnetic recording medium
JPS54119904A (en) Magnetic recording medium
JPS5528562A (en) Magnetic recording medium
JPS5650337A (en) Resin coated carrier
JPS5528560A (en) Magnetic recording medium
JPS5528561A (en) Magnetic recording medium
JPS5528557A (en) Magnetic recording medium
JPS5528558A (en) Magnetic recording medium
JPS5528555A (en) Magnetic recording medium
JPS5528556A (en) Magnetic recording medium
JPS5528559A (en) Magnetic recording medium
JPS5597026A (en) Magnetic recording medium
JPS5671822A (en) Magnetic recording medium
JPS51131303A (en) Magnetic recording medium
JPS5528507A (en) Magnetic recording tape
JPS5517816A (en) Magnetic recording media
JPS5517834A (en) Magnetic recording media
JPS5517811A (en) Magnetic recording media