JPS55163526A - Production of screen for projection - Google Patents
Production of screen for projectionInfo
- Publication number
- JPS55163526A JPS55163526A JP14918579A JP14918579A JPS55163526A JP S55163526 A JPS55163526 A JP S55163526A JP 14918579 A JP14918579 A JP 14918579A JP 14918579 A JP14918579 A JP 14918579A JP S55163526 A JPS55163526 A JP S55163526A
- Authority
- JP
- Japan
- Prior art keywords
- foil
- coating liquid
- uneven surface
- screen
- unevenness
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To widen the reflection directivity to the transverse direction of the screen for projection and prevent the damaging and staining of its surface by forming a finely uneven surface on an Al foil, and coating the protecting film thinner of thickness than the height of the unevenness thereof by the specific method.
CONSTITUTION: An aluminum foil 1' and an other guiding film 1" are superposed and are fed in the arrow direction between guide rolls 5A, 5B and rolling oil 6 is flowed to make the foil 1 having an uneven surface 1a orthogonal to the feed direction of the foil 1" of the fine waveforms of the height about 3μ on the surface making opposing contact with the guide film 1". The foil 1 is bonded onto the surface of a screen substrate 2 and the coating liquid 9 comprising dissolving the copolymer of vinyl chloride and vinyl acetate in a solvent having a boiling point sufficiently higher than room temperature (n-butyl acetate or the like) is flowed on the foil 1 placed on a rotary table 8. After the coating liquid 9 is spread over the entire surface by 10rpm first, the speed is increased up to 40rpm to shake off the excess coating liquid. After this, it is dried by an infrared ray heater, whereby the protecting film 3 of 0.9W1μ thick is formed. In this way, the uneven surface 3a corresponding to the unevenness 1a of the aluminum foil 1 is formed.
COPYRIGHT: (C)1980,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP54149185A JPS586933B2 (en) | 1979-11-16 | 1979-11-16 | Method of manufacturing a projection screen |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP54149185A JPS586933B2 (en) | 1979-11-16 | 1979-11-16 | Method of manufacturing a projection screen |
Related Parent Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP48127462A Division JPS5079332A (en) | 1973-11-13 | 1973-11-13 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS55163526A true JPS55163526A (en) | 1980-12-19 |
JPS586933B2 JPS586933B2 (en) | 1983-02-07 |
Family
ID=15469648
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP54149185A Expired JPS586933B2 (en) | 1979-11-16 | 1979-11-16 | Method of manufacturing a projection screen |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS586933B2 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0550799A (en) * | 1991-08-23 | 1993-03-02 | Shinzo Takada | Decorated furniture and its decoration forming method |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5144780U (en) * | 1974-09-27 | 1976-04-02 | ||
JPS51151738A (en) * | 1975-06-23 | 1976-12-27 | Hitachi Ltd | Apparatus for spin coating |
-
1979
- 1979-11-16 JP JP54149185A patent/JPS586933B2/en not_active Expired
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5144780U (en) * | 1974-09-27 | 1976-04-02 | ||
JPS51151738A (en) * | 1975-06-23 | 1976-12-27 | Hitachi Ltd | Apparatus for spin coating |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0550799A (en) * | 1991-08-23 | 1993-03-02 | Shinzo Takada | Decorated furniture and its decoration forming method |
Also Published As
Publication number | Publication date |
---|---|
JPS586933B2 (en) | 1983-02-07 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5459926A (en) | Photographic material having antistatic layer | |
JPS55165172A (en) | Applying method for substrate | |
JPS55163526A (en) | Production of screen for projection | |
JPS5325113A (en) | Method for prevention of falsification | |
GB1015892A (en) | Flexible materials having a plurality of superposed layers | |
JPS52834A (en) | Coating process | |
JPS5376748A (en) | Forming method of insulation fulm | |
JPS5532314A (en) | Method and apparatus for manufacturing color picture tube fluorescent screen | |
JPS51130442A (en) | A method for double-side coating | |
JPS5317648A (en) | Process of coating inorganic paint | |
JPS52126431A (en) | Coating composition and method of coating the same | |
JPS5222038A (en) | Trowel apparatus for coating | |
JPS5678657A (en) | Facing method for building board with groove | |
JPS52152944A (en) | Method for application of high-viscosity coating in thin layer | |
JPS5427357A (en) | Formation method of fluorescent screen for color picture tube | |
JPS5626565A (en) | Treating method for double layer painting of travelling paper | |
JPS5376747A (en) | Forming method of insulation film | |
JPS5732994A (en) | Transfer base material for masking | |
JPS5375283A (en) | Coating of fluororesins | |
JPS5667294A (en) | Negative plate for flat plate printing | |
JPS5496547A (en) | Coating device of coating material | |
JPS5359427A (en) | Electrostatic recording material | |
JPS52117550A (en) | Electrode formation method | |
JPS51151737A (en) | Method for applying liquid and a roller for effecting the same | |
JPS5676270A (en) | Method and apparatus for coating and drying |