JPS55136580A - Welding method of angle joint part - Google Patents

Welding method of angle joint part

Info

Publication number
JPS55136580A
JPS55136580A JP4379279A JP4379279A JPS55136580A JP S55136580 A JPS55136580 A JP S55136580A JP 4379279 A JP4379279 A JP 4379279A JP 4379279 A JP4379279 A JP 4379279A JP S55136580 A JPS55136580 A JP S55136580A
Authority
JP
Japan
Prior art keywords
molten metal
pocket part
vertical plate
backing strip
joint part
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP4379279A
Other languages
Japanese (ja)
Inventor
Naoki Okuda
Shigezo Nose
Kaoru Hase
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kobe Steel Ltd
Original Assignee
Kobe Steel Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kobe Steel Ltd filed Critical Kobe Steel Ltd
Priority to JP4379279A priority Critical patent/JPS55136580A/en
Publication of JPS55136580A publication Critical patent/JPS55136580A/en
Pending legal-status Critical Current

Abstract

PURPOSE: To prevent the burn-through of molten metal surface from the root gap surface by forming a cut-step part on the surface opposing to a vertical plate or horizontal plate, of a backing strip.
CONSTITUTION: An oblique cut is formed to the upper left corner of a backing strip 4' to form a pocket part 7a. Hence, the molten metal formed in the bottom of the groove is accumulated in this pocket part 7a and will not drop onto its back side. If the amount is large, the molten metal 9 subsequently flows forward so as to gradually fill the inside of the passage of the pocket part 7a extending in the weld line direction, cools in that portion, and solidifies in the state that it is held closely contacted with the vertical plate, whereby the blowing-through of the arc coming from later is prevented.
COPYRIGHT: (C)1980,JPO&Japio
JP4379279A 1979-04-10 1979-04-10 Welding method of angle joint part Pending JPS55136580A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP4379279A JPS55136580A (en) 1979-04-10 1979-04-10 Welding method of angle joint part

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP4379279A JPS55136580A (en) 1979-04-10 1979-04-10 Welding method of angle joint part

Publications (1)

Publication Number Publication Date
JPS55136580A true JPS55136580A (en) 1980-10-24

Family

ID=12673584

Family Applications (1)

Application Number Title Priority Date Filing Date
JP4379279A Pending JPS55136580A (en) 1979-04-10 1979-04-10 Welding method of angle joint part

Country Status (1)

Country Link
JP (1) JPS55136580A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6172367U (en) * 1984-10-16 1986-05-16
JP2013136065A (en) * 2011-12-28 2013-07-11 Jfe Steel Corp Groove part for corner welding of welded tetrahedral box section member

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS6172367U (en) * 1984-10-16 1986-05-16
JP2013136065A (en) * 2011-12-28 2013-07-11 Jfe Steel Corp Groove part for corner welding of welded tetrahedral box section member

Similar Documents

Publication Publication Date Title
Shimada et al. Study of bead formation by low pressure TIG arc and prevention of under-cut bead
JPS55136580A (en) Welding method of angle joint part
JPS6448678A (en) Method and equipment for narrow gap welding
JPS56136281A (en) Horizontal automatic welding method of aluminum and aluminum alloy
JPS5424240A (en) Non-consumable electrode type arc welding method
JPS564381A (en) Two electrode submerged arc welding method
JPS6222313Y2 (en)
JPS5548479A (en) Arc welding method
JPS54119354A (en) One-side welding method
JPS5586689A (en) Electron beam welding method
JPH05261532A (en) Vertical up-gas shielded arc welding method by nonconsumable nozzle
JPS5516754A (en) Welding box pillar by consumed nozzle
JPS6147635B2 (en)
Korneev et al. Automatic Submerged Arc Welding of Aluminum Plate
JPS54132448A (en) Welding method for copper or copper alloy parts and ferro or nickel alloy parts
JPS53108048A (en) Electron beam welding method
JPS5633192A (en) Welding process for copper and copper alloy
JPS5461046A (en) Butt welded joint of clad steel
JPS5714474A (en) One-side welding method
JPS5453645A (en) Butt welding method
JPS53119249A (en) Resistance welding method
Pirner Suitability of Aluminum for Resistance Welding
JPS5395150A (en) Beam welding by filler material adding system
JPS56158277A (en) Vertical narrow groove welding for aluminum alloy thick plate
Ohara et al. Study on High Speed Submerged Arc Welding. II.--Effect of Arc Heat Source Shape on the Occurrence of Undercutting