JPS55110755A - Method for continuous cast production of steel for seamless pipe - Google Patents

Method for continuous cast production of steel for seamless pipe

Info

Publication number
JPS55110755A
JPS55110755A JP1887179A JP1887179A JPS55110755A JP S55110755 A JPS55110755 A JP S55110755A JP 1887179 A JP1887179 A JP 1887179A JP 1887179 A JP1887179 A JP 1887179A JP S55110755 A JPS55110755 A JP S55110755A
Authority
JP
Japan
Prior art keywords
steel
seamless pipe
continuous cast
porocity
tensile strength
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP1887179A
Other languages
Japanese (ja)
Other versions
JPS5943964B2 (en
Inventor
Shinobu Okano
Yutaka Shinjo
Junichi Matsuno
Tokumi Funakoshi
Keiichiro Takitani
Akio Ejima
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
Kawasaki Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kawasaki Steel Corp filed Critical Kawasaki Steel Corp
Priority to JP1887179A priority Critical patent/JPS5943964B2/en
Publication of JPS55110755A publication Critical patent/JPS55110755A/en
Publication of JPS5943964B2 publication Critical patent/JPS5943964B2/en
Expired legal-status Critical Current

Abstract

PURPOSE: To provide the title steel, high in tensile strength and little in porocity and segregation at the center of cast product in operation range of usual molten steel temperature not causing casting trouble by adjusting each content of C, Si and Mn in seamless pipe steel to meet three specific equations.
CONSTITUTION: Each content of C, Si and Mn in seamless pipe steel is adjusted to simultaneously satisfy the following three equations: (%C)+(%Mn)/12.5≤0.53, (%C)+(%Mn)/6≥0.55 and 0.01≤(%Si)≤0.5. This method makes it possible to provide, by continuous cast process, material completely free from center porocity and having tensile strength of 65kg/mm2 or more.
COPYRIGHT: (C)1980,JPO&Japio
JP1887179A 1979-02-20 1979-02-20 Manufacturing method of steel for seamless pipes by continuous casting Expired JPS5943964B2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP1887179A JPS5943964B2 (en) 1979-02-20 1979-02-20 Manufacturing method of steel for seamless pipes by continuous casting

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP1887179A JPS5943964B2 (en) 1979-02-20 1979-02-20 Manufacturing method of steel for seamless pipes by continuous casting

Publications (2)

Publication Number Publication Date
JPS55110755A true JPS55110755A (en) 1980-08-26
JPS5943964B2 JPS5943964B2 (en) 1984-10-25

Family

ID=11983595

Family Applications (1)

Application Number Title Priority Date Filing Date
JP1887179A Expired JPS5943964B2 (en) 1979-02-20 1979-02-20 Manufacturing method of steel for seamless pipes by continuous casting

Country Status (1)

Country Link
JP (1) JPS5943964B2 (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS59120348A (en) * 1982-12-28 1984-07-11 Kawasaki Steel Corp Continuous casting method of bloom for seamless pipe
CN104550790A (en) * 2013-10-09 2015-04-29 宝钢特钢有限公司 Slab continuous casting manufacturing method for medium-manganese wear-resistant steel

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS59120348A (en) * 1982-12-28 1984-07-11 Kawasaki Steel Corp Continuous casting method of bloom for seamless pipe
CN104550790A (en) * 2013-10-09 2015-04-29 宝钢特钢有限公司 Slab continuous casting manufacturing method for medium-manganese wear-resistant steel

Also Published As

Publication number Publication date
JPS5943964B2 (en) 1984-10-25

Similar Documents

Publication Publication Date Title
JPS5314609A (en) Production of nondirectional electromagnetic steel sheet free from ridging
JPS55110755A (en) Method for continuous cast production of steel for seamless pipe
JPS5633156A (en) Preventing method of surface crack formation in continuously cast slab
JPS5568156A (en) Production of slab for clad steel plate in continuous casting method
JPS561253A (en) Continuous casting method of al and al alloy
JPS5782452A (en) Manufacture of nonmagnetic high-manganese steel
JPS5684157A (en) Horizontal continuous casting method of molten metal
JPS5325210A (en) Steel refining method
JPS566758A (en) Steel for mold and its production
JPS5531148A (en) Manufacture of clean cast steel product
JPS5775275A (en) Continuous casting method for steel
JPS57134541A (en) Manufacture of low-carbon sulfur free cutting steel
JPS5641050A (en) Production of roll for rolling
JPS5570458A (en) Production of spheroidal graphite cast iron pipe
JPS57202948A (en) High speed continuous casting method for steel
JPS57130748A (en) Method for preventing surface cracking flaw of continuously cast ingot
Nakata et al. Productivity Improvement of the Bloom CC in Chita Plant
Bornatskii et al. Improving Semi-Killed Steel Ingot Quality When Casting Under Slag
JPS53106618A (en) Manufacture of molten a1-si killed steel for continuous casting
JPS53106617A (en) Manufacture of molten killed steel for continuous casting
JPS579823A (en) Production of mild steel ingot for bar and wire by continuous casting
JPS5723047A (en) Steel material for pipe
Houck Steelmaking to Produce Clean Steel
Wilhelm et al. Ladle Steelmaking
Parshin et al. Development of a Practice for the Continuous Casting of Semi-Killed Steel for the Production of Tinplate