JPS5416319A - Cast alloy for hearth rollers having superior rougth surface resistance - Google Patents

Cast alloy for hearth rollers having superior rougth surface resistance

Info

Publication number
JPS5416319A
JPS5416319A JP8169177A JP8169177A JPS5416319A JP S5416319 A JPS5416319 A JP S5416319A JP 8169177 A JP8169177 A JP 8169177A JP 8169177 A JP8169177 A JP 8169177A JP S5416319 A JPS5416319 A JP S5416319A
Authority
JP
Japan
Prior art keywords
rougth
superior
surface resistance
cast alloy
rollers
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP8169177A
Other languages
Japanese (ja)
Other versions
JPS575868B2 (en
Inventor
Hideo Fujita
Arata Komitsu
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kubota Corp
Original Assignee
Kubota Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kubota Corp filed Critical Kubota Corp
Priority to JP8169177A priority Critical patent/JPS5416319A/en
Publication of JPS5416319A publication Critical patent/JPS5416319A/en
Publication of JPS575868B2 publication Critical patent/JPS575868B2/ja
Granted legal-status Critical Current

Abstract

PURPOSE: To prevent the surface roughening of rollers, over a long term, used in a roller hearth type continuous furnace and considerably elongate the life by making the rollers of alloy steel contg. a specified amt. of Si, Cr, Ni, etc.
COPYRIGHT: (C)1979,JPO&Japio
JP8169177A 1977-07-06 1977-07-06 Cast alloy for hearth rollers having superior rougth surface resistance Granted JPS5416319A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP8169177A JPS5416319A (en) 1977-07-06 1977-07-06 Cast alloy for hearth rollers having superior rougth surface resistance

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP8169177A JPS5416319A (en) 1977-07-06 1977-07-06 Cast alloy for hearth rollers having superior rougth surface resistance

Publications (2)

Publication Number Publication Date
JPS5416319A true JPS5416319A (en) 1979-02-06
JPS575868B2 JPS575868B2 (en) 1982-02-02

Family

ID=13753374

Family Applications (1)

Application Number Title Priority Date Filing Date
JP8169177A Granted JPS5416319A (en) 1977-07-06 1977-07-06 Cast alloy for hearth rollers having superior rougth surface resistance

Country Status (1)

Country Link
JP (1) JPS5416319A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS57138797U (en) * 1981-02-24 1982-08-30
JPS60106898U (en) * 1983-12-27 1985-07-20 株式会社 金指造船所 Boarding equipment for deck stowage ships

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS57138797U (en) * 1981-02-24 1982-08-30
JPS60106898U (en) * 1983-12-27 1985-07-20 株式会社 金指造船所 Boarding equipment for deck stowage ships

Also Published As

Publication number Publication date
JPS575868B2 (en) 1982-02-02

Similar Documents

Publication Publication Date Title
JPS53137016A (en) Oriented electrical steel sheet of ultra low iron loss
ES8401342A1 (en) Cast roll for cold rolling, and method for its production.
JPS5416321A (en) Cast alloy for hearth rollers having superior rougth surface resistance
JPS5416319A (en) Cast alloy for hearth rollers having superior rougth surface resistance
JPS5416320A (en) Cast alloy for hearth rollers having superior rougth surface resistance
JPS56163244A (en) Heat resistant austenite steel with superior hot workability and oxidation resistance
JPS5528348A (en) Steel for roll of continuous casting facilities
JPS53140219A (en) Manufacture of hot rolled steel material
JPS54134016A (en) Cast steel of thermal shock resistance
JPS5342114A (en) Backup roll for rolling
JPS53129117A (en) Manufacture of high toughness thick steel plate
JPS544230A (en) Age hardening, wear resistant ni alloy
JPS5288526A (en) Roll for rolling
JPS5453615A (en) Martensitic stainless cast steel for paper-making suction roll
JPS54118323A (en) Heat crack resistant steel for use as metal mold
JPS544229A (en) Age hardening, wear resistant ni alloy
JPS5413414A (en) Medium cr low ni stainless cast steel of high corrosion resistance and high strength
JPS52103312A (en) Wear-resisting and impact-resisting composite material
JPS5268019A (en) Roller conveying steel plate
JPS52128822A (en) Preparation of steel sheet for porcelain enameling by continuous annealing
JPS5392323A (en) Stainless steel product with excellent high temperature corrosion resistance
JPS53117620A (en) Roller hardly causing pickup phenomena for heat treatment furnace
JPS5432126A (en) High permeability amorphous alloy with superior resistance to heat and corrosion
JPS5325212A (en) Wear resistant cast steel alloy for crusher
JPS53149110A (en) Manufacture of nodular graphite cast iron pipe