JPS4610430B1 - - Google Patents
Info
- Publication number
- JPS4610430B1 JPS4610430B1 JP3381168A JP3381168A JPS4610430B1 JP S4610430 B1 JPS4610430 B1 JP S4610430B1 JP 3381168 A JP3381168 A JP 3381168A JP 3381168 A JP3381168 A JP 3381168A JP S4610430 B1 JPS4610430 B1 JP S4610430B1
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C21/00—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
- C03C21/001—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface in liquid phase, e.g. molten salts, solutions
- C03C21/002—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface in liquid phase, e.g. molten salts, solutions to perform ion-exchange between alkali ions
Landscapes
- Chemical & Material Sciences (AREA)
- Life Sciences & Earth Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- General Chemical & Material Sciences (AREA)
- Geochemistry & Mineralogy (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Surface Treatment Of Glass (AREA)
- Glass Compositions (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US642686A US3524737A (en) | 1967-06-01 | 1967-06-01 | Method for thermochemical strengthening of glass articles |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| JPS4610430B1 true JPS4610430B1 (enrdf_load_stackoverflow) | 1971-03-16 |
Family
ID=24577600
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP3381168A Pending JPS4610430B1 (enrdf_load_stackoverflow) | 1967-06-01 | 1968-05-21 |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US3524737A (enrdf_load_stackoverflow) |
| JP (1) | JPS4610430B1 (enrdf_load_stackoverflow) |
| BE (1) | BE716046A (enrdf_load_stackoverflow) |
| DE (1) | DE1771427A1 (enrdf_load_stackoverflow) |
| ES (1) | ES354347A1 (enrdf_load_stackoverflow) |
| FR (1) | FR1570118A (enrdf_load_stackoverflow) |
| GB (1) | GB1212123A (enrdf_load_stackoverflow) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2011505323A (ja) * | 2007-11-29 | 2011-02-24 | コーニング インコーポレイテッド | 改良された強靭性および引っかき抵抗性を有するガラス |
| JP2013502371A (ja) * | 2009-08-21 | 2013-01-24 | コーニング インコーポレイテッド | 亀裂および引っ掻き抵抗性のガラスおよびそれから製造されたエンクロージャ |
| JP2014501214A (ja) * | 2010-12-14 | 2014-01-20 | コーニング インコーポレイテッド | ガラス強化のための熱処理 |
Families Citing this family (29)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| BE755946A (fr) * | 1969-09-10 | 1971-03-09 | Saint Gobain Pont A Mousson | Perfectionnements aux procedes de traitement superficiel d'articles en verre ou en ceramique par echange d'ions |
| US3751238A (en) * | 1970-02-25 | 1973-08-07 | Corning Glass Works | Method of chemically strengthening a silicate article containing soda |
| US3773489A (en) * | 1971-03-16 | 1973-11-20 | Corning Glass Works | Chemically strengthened glass |
| DE2205844C3 (de) * | 1972-02-08 | 1975-08-14 | Jenaer Glaswerk Schott & Gen., 6500 Mainz | Durch Alkaliionenaustausch chemisch gehärtetes Brillen-Fernteilglas |
| US4119760A (en) * | 1975-08-15 | 1978-10-10 | Ppg Industries, Inc. | Chemical strengthening of glass |
| DE3840071A1 (de) * | 1988-11-28 | 1990-05-31 | Schott Glaswerke | Verfahren zum ionenaustausch an glas oder glaskeramik |
| GB2335423A (en) | 1998-03-20 | 1999-09-22 | Pilkington Plc | Chemically toughenable glass |
| AU2001273158A1 (en) | 2000-08-15 | 2002-02-25 | Corning Incorporated | High silver borosilicate glasses |
| RU2269493C1 (ru) * | 2004-07-26 | 2006-02-10 | Федеральное государственное унитарное предприятие "Обнинское научно-производственное предприятие "Технология" | Способ упрочнения изделий из стеклокристаллического материала бета-сподуменового состава путем ионного обмена |
| US7666511B2 (en) * | 2007-05-18 | 2010-02-23 | Corning Incorporated | Down-drawable, chemically strengthened glass for cover plate |
| DE202009018732U1 (de) | 2008-02-26 | 2012-11-27 | Corning Inc. | Läutermittel für Silikatgläser |
| WO2010005578A1 (en) * | 2008-07-11 | 2010-01-14 | Corning Incorporated | Glass with compressive surface for consumer applications |
| EP2334613A1 (en) * | 2008-08-21 | 2011-06-22 | Corning Inc. | Durable glass housings/enclosures for electronic devices |
| US20100055395A1 (en) * | 2008-08-28 | 2010-03-04 | Ljerka Ukrainczyk | Method of Making Shaped Glass Articles |
| FR2939787A1 (fr) | 2008-12-15 | 2010-06-18 | Saint Gobain | Composition de verre adaptee a la realisation d'elements optiques plans |
| US10941071B2 (en) | 2013-08-02 | 2021-03-09 | Corning Incorporated | Hybrid soda-lime silicate and aluminosilicate glass articles |
| DE102013019003A1 (de) * | 2013-11-13 | 2015-05-13 | Taiwan Glass Ind. Corp. | Alkali-Alumino-Silikatglas |
| EP3074357B1 (en) | 2013-11-26 | 2022-11-09 | Corning Inc. | Fast ion exchangeable glasses with high indentation threshold |
| US9670088B2 (en) | 2014-05-20 | 2017-06-06 | Corning Incorporated | Scratch resistant glass and method of making |
| JP6716569B2 (ja) | 2014-12-31 | 2020-07-01 | コーニング インコーポレイテッド | ガラス物品の処理方法 |
| AU2015374004B2 (en) | 2014-12-31 | 2020-04-09 | Corning Incorporated | Methods for thermally treating glass articles |
| WO2019070788A1 (en) * | 2017-10-06 | 2019-04-11 | Corning Incorporated | GLASS LAMINATE HAVING LOW COMPRESSION STRENGTH, LARGE LAYER DEPTH, CHEMICALLY REINFORCED INTERNAL GLASS LAYER, AND METHOD THEREOF |
| EP4230593A3 (en) | 2021-06-18 | 2023-11-22 | Corning Incorporated | Colored glass articles having improved mechanical durability |
| WO2022266273A1 (en) | 2021-06-18 | 2022-12-22 | Corning Incorporated | Colored glass articles having improved mechanical durability |
| US11802072B2 (en) | 2021-06-18 | 2023-10-31 | Corning Incorporated | Gold containing silicate glass |
| US12378152B2 (en) | 2021-06-18 | 2025-08-05 | Corning Incorporated | Colored glass articles having improved mechanical durability |
| US12054422B2 (en) | 2021-06-18 | 2024-08-06 | Corning Incorporated | Colored glass articles having improved mechanical durability |
| US11634354B2 (en) | 2021-06-18 | 2023-04-25 | Corning Incorporated | Colored glass articles having improved mechanical durability |
| US12240782B2 (en) | 2022-05-31 | 2025-03-04 | Corning Incorporated | Ion exchangeable yellow glass articles |
Family Cites Families (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3396075A (en) * | 1962-09-17 | 1968-08-06 | Pittsburgh Plate Glass Co | Glass articles |
| NL298724A (enrdf_load_stackoverflow) * | 1962-10-04 | |||
| US3445316A (en) * | 1966-04-14 | 1969-05-20 | Corning Glass Works | Method of differential chemical tempering glass and article |
-
1967
- 1967-06-01 US US642686A patent/US3524737A/en not_active Expired - Lifetime
-
1968
- 1968-05-21 JP JP3381168A patent/JPS4610430B1/ja active Pending
- 1968-05-22 DE DE19681771427 patent/DE1771427A1/de active Pending
- 1968-05-23 GB GB24590/68A patent/GB1212123A/en not_active Expired
- 1968-05-25 ES ES354347A patent/ES354347A1/es not_active Expired
- 1968-05-31 FR FR1570118D patent/FR1570118A/fr not_active Expired
- 1968-05-31 BE BE716046D patent/BE716046A/xx unknown
Cited By (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2011505323A (ja) * | 2007-11-29 | 2011-02-24 | コーニング インコーポレイテッド | 改良された強靭性および引っかき抵抗性を有するガラス |
| CN105776849A (zh) * | 2007-11-29 | 2016-07-20 | 康宁股份有限公司 | 具有改进的韧性和抗刮性的玻璃 |
| US11370695B2 (en) | 2007-11-29 | 2022-06-28 | Corning Incorporated | Glasses having improved toughness and scratch resistance |
| JP2013502371A (ja) * | 2009-08-21 | 2013-01-24 | コーニング インコーポレイテッド | 亀裂および引っ掻き抵抗性のガラスおよびそれから製造されたエンクロージャ |
| US9290407B2 (en) | 2009-08-21 | 2016-03-22 | Corning Incorporated | Crack and scratch resistant glass and enclosures made therefrom |
| USRE47837E1 (en) | 2009-08-21 | 2020-02-04 | Corning Incorporated | Crack and scratch resistant glass and enclosures made therefrom |
| USRE49530E1 (en) | 2009-08-21 | 2023-05-16 | Corning Incorporated | Crack and scratch resistant glass and enclosures made therefrom |
| JP2014501214A (ja) * | 2010-12-14 | 2014-01-20 | コーニング インコーポレイテッド | ガラス強化のための熱処理 |
Also Published As
| Publication number | Publication date |
|---|---|
| ES354347A1 (es) | 1969-11-01 |
| GB1212123A (en) | 1970-11-11 |
| US3524737A (en) | 1970-08-18 |
| FR1570118A (enrdf_load_stackoverflow) | 1969-06-06 |
| DE1771427A1 (de) | 1971-12-16 |
| BE716046A (enrdf_load_stackoverflow) | 1968-12-02 |