JPH07504762A5 - - Google Patents
Info
- Publication number
- JPH07504762A5 JPH07504762A5 JP5-515779A JP51577993A JPH07504762A5 JP H07504762 A5 JPH07504762 A5 JP H07504762A5 JP 51577993 A JP51577993 A JP 51577993A JP H07504762 A5 JPH07504762 A5 JP H07504762A5
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Applications Claiming Priority (5)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US904,229 | 1978-05-09 | ||
| US84745492A | 1992-03-06 | 1992-03-06 | |
| US847,454 | 1992-03-06 | ||
| US90422992A | 1992-06-25 | 1992-06-25 | |
| PCT/US1993/001749 WO1993018437A1 (en) | 1992-03-06 | 1993-02-25 | Photoresists having a low level of metal ions |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH07504762A JPH07504762A (ja) | 1995-05-25 |
| JPH07504762A5 true JPH07504762A5 (enExample) | 2000-07-11 |
| JP3184530B2 JP3184530B2 (ja) | 2001-07-09 |
Family
ID=27126706
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP51577993A Expired - Lifetime JP3184530B2 (ja) | 1992-03-06 | 1993-02-25 | 金属イオンレベルが低いフォトレジスト |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US5543263A (enExample) |
| EP (1) | EP0635145B1 (enExample) |
| JP (1) | JP3184530B2 (enExample) |
| KR (1) | KR100242920B1 (enExample) |
| DE (1) | DE69320468T2 (enExample) |
| SG (1) | SG48944A1 (enExample) |
| WO (1) | WO1993018437A1 (enExample) |
Families Citing this family (29)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP3630422B2 (ja) * | 1991-12-18 | 2005-03-16 | クラリアント・ファイナンス・(ビーブイアイ)・リミテッド | ノボラック樹脂中の金属イオンの低減 |
| US5580949A (en) * | 1991-12-18 | 1996-12-03 | Hoechst Celanese Corporation | Metal ion reduction in novolak resins and photoresists |
| SG52770A1 (en) * | 1992-07-10 | 1998-09-28 | Hoechst Celanese Corp | Metal ion reduction in top anti-reflective coatings for photoresists |
| US5830990A (en) * | 1992-07-10 | 1998-11-03 | Clariant Finance (Bvi) Limited | Low metals perfluorooctanoic acid and top anti-reflective coatings for photoresists |
| EP0671025B1 (en) * | 1992-11-25 | 1997-08-13 | Hoechst Celanese Corporation | Metal ion reduction in bottom anti-reflective coatings for photoresists |
| JP2998095B2 (ja) * | 1992-12-07 | 2000-01-11 | ジェイエスアール株式会社 | レジスト塗布組成物溶液 |
| US5614349A (en) * | 1992-12-29 | 1997-03-25 | Hoechst Celanese Corporation | Using a Lewis base to control molecular weight of novolak resins |
| US5476750A (en) * | 1992-12-29 | 1995-12-19 | Hoechst Celanese Corporation | Metal ion reduction in the raw materials and using a Lewis base to control molecular weight of novolak resin to be used in positive photoresists |
| US5286606A (en) * | 1992-12-29 | 1994-02-15 | Hoechst Celanese Corporation | Process for producing a developer having a low metal ion level |
| US5679766A (en) * | 1993-12-07 | 1997-10-21 | Shipley Company, L.L.C. | Purification process of novolar resins using acid treated chelating cation exchange resin |
| WO1996012214A1 (en) * | 1994-10-12 | 1996-04-25 | Hoechst Celanese Corporation | Low metal ion photoactive compounds and photoresists compositions produced therefrom |
| US5837417A (en) * | 1994-12-30 | 1998-11-17 | Clariant Finance (Bvi) Limited | Quinone diazide compositions containing low metals p-cresol oligomers and process of producing the composition |
| US5614352A (en) * | 1994-12-30 | 1997-03-25 | Hoechst Celanese Corporation | Metal ion reduction in novolak resins solution in PGMEA by chelating ion exchange resin |
| US5521052A (en) * | 1994-12-30 | 1996-05-28 | Hoechst Celanese Corporation | Metal ion reduction in novolak resin using an ion exchange catalyst in a polar solvent and photoresists compositions therefrom |
| TW418215B (en) * | 1995-03-13 | 2001-01-11 | Ciba Sc Holding Ag | A process for the production of three-dimensional articles in a stereolithography bath comprising the step of sequentially irradiating a plurality of layers of a liquid radiation-curable composition |
| US5693749A (en) * | 1995-09-20 | 1997-12-02 | Hoechst Celanese Corporation | Fractionation of phenol formaldehyde condensate and photoresist compositions produced therefrom |
| US5739265A (en) * | 1995-09-20 | 1998-04-14 | Clariant Finance (Bvi) Ltd. | Fractionation of phenol formaldehyde condensate and photoresist compositions produced therefrom |
| US5750031A (en) * | 1995-09-26 | 1998-05-12 | Clariant Finance (Bvi) Limited | Process for producing surfactant having a low metal ion level and developer produced therefrom |
| US5656413A (en) * | 1995-09-28 | 1997-08-12 | Hoechst Celanese Corporation | Low metal ion containing 4,4'-[1-[4-[1-(4-Hydroxyphenyl)-1-methylethyl]phenyl]ethylidene]bisphe nol and photoresist compositions therefrom |
| US5962183A (en) * | 1995-11-27 | 1999-10-05 | Clariant Finance (Bvi) Limited | Metal ion reduction in photoresist compositions by chelating ion exchange resin |
| US5665517A (en) * | 1996-01-11 | 1997-09-09 | Hoechst Celanese Corporation | Acidic ion exchange resin as a catalyst to synthesize a novolak resin and photoresist composition therefrom |
| KR100234532B1 (ko) * | 1996-09-21 | 1999-12-15 | 윤종용 | 반도체 제조공정의 포토레지스트 세정용 시너 조성물 및 그를 이용한 반도체장치의 제조방법 |
| WO1998027461A1 (en) * | 1996-12-17 | 1998-06-25 | Clariant International Ltd. | A method for reducing metal ion contaminants in photoresist compositions containing an organic polar solvent by ion exchange |
| US6106722A (en) * | 1997-08-12 | 2000-08-22 | Kinetico Incorporated | Filtering photoresist-containing liquid |
| US5936071A (en) * | 1998-02-02 | 1999-08-10 | Clariant Finance (Bvi) Limited | Process for making a photoactive compound and photoresist therefrom |
| US6610465B2 (en) * | 2001-04-11 | 2003-08-26 | Clariant Finance (Bvi) Limited | Process for producing film forming resins for photoresist compositions |
| JP3854889B2 (ja) * | 2001-04-19 | 2006-12-06 | キヤノン株式会社 | 金属または金属化合物パターンの製造方法および電子源の製造方法 |
| US20040206702A1 (en) * | 2002-08-08 | 2004-10-21 | Davidson James M. | Use of an oxidizer to improve trace metals removal from photoresist and photoresist components |
| TWI441239B (zh) * | 2006-12-12 | 2014-06-11 | Asml荷蘭公司 | 製造微影元件的方法、微影單元及電腦程式產品 |
Family Cites Families (27)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US2929808A (en) * | 1956-04-04 | 1960-03-22 | Exxon Research Engineering Co | Removal of metal contaminants in polymerization processes |
| US4033909A (en) * | 1974-08-13 | 1977-07-05 | Union Carbide Corporation | Stable phenolic resoles |
| US4033910A (en) * | 1975-09-26 | 1977-07-05 | Union Carbide Corporation | Methyl formate as an adjuvant in phenolic foam formation |
| GB1509354A (en) * | 1976-04-24 | 1978-05-04 | Maruzen Oil Co Ltd | Process for purifying halogenated alkenyl-phenol polymers |
| US4452883A (en) * | 1983-05-17 | 1984-06-05 | Minnesota Mining And Manufacturing Company | Barrier resin for photothermographic color separation |
| US4567130A (en) * | 1984-07-27 | 1986-01-28 | E. I. Du Pont De Nemours And Company | Process for etching single photopolymer layer utilizing chemically soluble pigments |
| US4584261A (en) * | 1984-07-27 | 1986-04-22 | E. I. Du Pont De Nemours And Company | Process for etching nonphotosensitive layer under washoff photopolymer layer |
| JPH063549B2 (ja) * | 1984-12-25 | 1994-01-12 | 株式会社東芝 | ポジ型フォトレジスト現像液組成物 |
| US4636540A (en) * | 1985-07-08 | 1987-01-13 | Atlantic Richfield Company | Purification of polymer solutions |
| JPS6232453A (ja) * | 1985-08-06 | 1987-02-12 | Tokyo Ohka Kogyo Co Ltd | ポジ型ホトレジスト用現像液 |
| US4784937A (en) * | 1985-08-06 | 1988-11-15 | Tokyo Ohka Kogyo Co., Ltd. | Developing solution for positive-working photoresist comprising a metal ion free organic base and an anionic surfactant |
| US4747954A (en) * | 1985-09-16 | 1988-05-31 | The Dow Chemical Company | Removal of metals from solutions |
| JPS6472155A (ja) * | 1987-09-12 | 1989-03-17 | 多摩化学工業株式会社 | ポジ型フォトレジスト用現像液 |
| GB8729510D0 (en) * | 1987-12-18 | 1988-02-03 | Ucb Sa | Photosensitive compositions containing phenolic resins & diazoquinone compounds |
| JPH01228560A (ja) * | 1988-03-08 | 1989-09-12 | Hitachi Chem Co Ltd | 不純金属成分の低減された溶液の製造法 |
| US5175078A (en) * | 1988-10-20 | 1992-12-29 | Mitsubishi Gas Chemical Company, Inc. | Positive type photoresist developer |
| JPH03128903A (ja) * | 1989-07-13 | 1991-05-31 | Fine Kurei:Kk | 合成樹脂の改質方法および改質合成樹脂 |
| DE3923426A1 (de) * | 1989-07-15 | 1991-01-17 | Hoechst Ag | Verfahren zur herstellung von novolak-harzen mit geringem metallionengehalt |
| JPH0465415A (ja) * | 1990-07-04 | 1992-03-02 | Hitachi Chem Co Ltd | 不純金属成分の低減されたノボラツク樹脂の製造法 |
| JPH0768297B2 (ja) * | 1991-11-28 | 1995-07-26 | 丸善石油化学株式会社 | フォトレジスト用ビニルフェノール系重合体の精製方法 |
| JPH0768296B2 (ja) * | 1991-11-28 | 1995-07-26 | 丸善石油化学株式会社 | ビニルフェノール系重合体の金属除去方法 |
| JP3630422B2 (ja) * | 1991-12-18 | 2005-03-16 | クラリアント・ファイナンス・(ビーブイアイ)・リミテッド | ノボラック樹脂中の金属イオンの低減 |
| SG52770A1 (en) * | 1992-07-10 | 1998-09-28 | Hoechst Celanese Corp | Metal ion reduction in top anti-reflective coatings for photoresists |
| EP0671025B1 (en) * | 1992-11-25 | 1997-08-13 | Hoechst Celanese Corporation | Metal ion reduction in bottom anti-reflective coatings for photoresists |
| US5476750A (en) * | 1992-12-29 | 1995-12-19 | Hoechst Celanese Corporation | Metal ion reduction in the raw materials and using a Lewis base to control molecular weight of novolak resin to be used in positive photoresists |
| WO1994014858A1 (en) * | 1992-12-29 | 1994-07-07 | Hoechst Celanese Corporation | Metal ion reduction in polyhydroxystyrene and photoresists |
| US5286606A (en) * | 1992-12-29 | 1994-02-15 | Hoechst Celanese Corporation | Process for producing a developer having a low metal ion level |
-
1993
- 1993-02-25 WO PCT/US1993/001749 patent/WO1993018437A1/en not_active Ceased
- 1993-02-25 KR KR1019940703112A patent/KR100242920B1/ko not_active Expired - Lifetime
- 1993-02-25 EP EP93906248A patent/EP0635145B1/en not_active Expired - Lifetime
- 1993-02-25 SG SG1996003934A patent/SG48944A1/en unknown
- 1993-02-25 DE DE69320468T patent/DE69320468T2/de not_active Expired - Lifetime
- 1993-02-25 JP JP51577993A patent/JP3184530B2/ja not_active Expired - Lifetime
-
1994
- 1994-06-17 US US08/261,646 patent/US5543263A/en not_active Expired - Lifetime