JPH0748665Y2 - 溶融金属めっき浴用ロール - Google Patents
溶融金属めっき浴用ロールInfo
- Publication number
- JPH0748665Y2 JPH0748665Y2 JP1989124010U JP12401089U JPH0748665Y2 JP H0748665 Y2 JPH0748665 Y2 JP H0748665Y2 JP 1989124010 U JP1989124010 U JP 1989124010U JP 12401089 U JP12401089 U JP 12401089U JP H0748665 Y2 JPH0748665 Y2 JP H0748665Y2
- Authority
- JP
- Japan
- Prior art keywords
- roll
- coating
- molten metal
- cermet
- film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Coating With Molten Metal (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1989124010U JPH0748665Y2 (ja) | 1989-10-25 | 1989-10-25 | 溶融金属めっき浴用ロール |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1989124010U JPH0748665Y2 (ja) | 1989-10-25 | 1989-10-25 | 溶融金属めっき浴用ロール |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH0363565U JPH0363565U (enExample) | 1991-06-20 |
| JPH0748665Y2 true JPH0748665Y2 (ja) | 1995-11-08 |
Family
ID=31671956
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1989124010U Expired - Lifetime JPH0748665Y2 (ja) | 1989-10-25 | 1989-10-25 | 溶融金属めっき浴用ロール |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0748665Y2 (enExample) |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0516212Y2 (enExample) * | 1987-08-21 | 1993-04-28 |
-
1989
- 1989-10-25 JP JP1989124010U patent/JPH0748665Y2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0363565U (enExample) | 1991-06-20 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US6132890A (en) | High-temperature spray coated member and method of production thereof | |
| WO1997032053A1 (fr) | Procede de formation d'un depot par pulverisation | |
| JPH0255502B2 (enExample) | ||
| JP2758707B2 (ja) | 溶融亜鉛めっき浴用の溶射被覆部材 | |
| JP2000233986A (ja) | めっき浴用部材およびその製造方法 | |
| JPH10306362A (ja) | 溶融金属に対する耐食性および耐剥離性が優れた複合溶射皮膜を形成した溶融金属浴用部材 | |
| JP2567137B2 (ja) | 耐摩耗性ならびに耐溶融金属性に優れる複合皮膜被覆部材とその製造方法 | |
| Sharma et al. | Cyclic high temperature oxidation behaviour of bare and NiCr coated mild steel and low alloyed steel | |
| JP5596334B2 (ja) | 溶融金属めっき浴用ロール | |
| JP2955625B2 (ja) | 溶融金属浴用部材 | |
| JP2000144366A (ja) | アルミニウム・亜鉛めっき浴用部材およびその製造方法 | |
| JP3502332B2 (ja) | 溶融金属めっき浴用部材およびその製造方法 | |
| JP3580541B2 (ja) | 加工性と加工部耐食性に優れた表面処理鋼板及びその製造方法 | |
| JPH0853749A (ja) | 溶融金属浴用浸漬部材 | |
| JP3930652B2 (ja) | 溶融亜鉛−アルミニウム合金めっき浴用ロール部材およびその製造方法 | |
| JP2953346B2 (ja) | 溶融金属めっき設備の鋼板支持用ロール | |
| JP2739409B2 (ja) | 耐食・耐摩耗多層金属被膜の製造方法 | |
| JP4224150B2 (ja) | 溶融金属めっき浴用ロール部材およびその製造方法 | |
| JPH0696783B2 (ja) | プレス成形性、化成処理性、溶接性に優れた亜鉛系めっき鋼板 | |
| JP4523142B2 (ja) | 溶融塩浴用ローラー | |
| JP2999129B2 (ja) | 溶融金属めっき用部材 | |
| JP3930653B2 (ja) | アルミニウム含有溶融亜鉛合金めっき浴用ロール部材およびその製造方法 | |
| JPH06212379A (ja) | 溶融亜鉛浴浸漬部材およびその製造方法 | |
| JP2002180224A (ja) | 合金化溶融亜鉛めっき鋼板およびその製造法 | |
| JPH10245695A (ja) | 浸漬用耐食性コンダクタロール |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| EXPY | Cancellation because of completion of term |