JPH0543061Y2 - - Google Patents
Info
- Publication number
- JPH0543061Y2 JPH0543061Y2 JP1987200880U JP20088087U JPH0543061Y2 JP H0543061 Y2 JPH0543061 Y2 JP H0543061Y2 JP 1987200880 U JP1987200880 U JP 1987200880U JP 20088087 U JP20088087 U JP 20088087U JP H0543061 Y2 JPH0543061 Y2 JP H0543061Y2
- Authority
- JP
- Japan
- Prior art keywords
- foam glass
- glass plate
- bending
- gap
- bent
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Re-Forming, After-Treatment, Cutting And Transporting Of Glass Products (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1987200880U JPH0543061Y2 (enrdf_load_stackoverflow) | 1987-12-28 | 1987-12-28 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP1987200880U JPH0543061Y2 (enrdf_load_stackoverflow) | 1987-12-28 | 1987-12-28 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH01106532U JPH01106532U (enrdf_load_stackoverflow) | 1989-07-18 |
| JPH0543061Y2 true JPH0543061Y2 (enrdf_load_stackoverflow) | 1993-10-29 |
Family
ID=31491268
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP1987200880U Expired - Lifetime JPH0543061Y2 (enrdf_load_stackoverflow) | 1987-12-28 | 1987-12-28 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH0543061Y2 (enrdf_load_stackoverflow) |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS6012289B2 (ja) * | 1977-07-29 | 1985-04-01 | 旭硝子株式会社 | ガラス板を折り曲げる方法 |
-
1987
- 1987-12-28 JP JP1987200880U patent/JPH0543061Y2/ja not_active Expired - Lifetime
Also Published As
| Publication number | Publication date |
|---|---|
| JPH01106532U (enrdf_load_stackoverflow) | 1989-07-18 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP6469903B2 (ja) | 材料シートを曲げて成形物品とする方法および装置 | |
| KR950031951A (ko) | 유리 시트를 벤딩 및 템퍼링하기 위한 방법과 장치 | |
| EP2507181B1 (en) | Method for making a shaped glass article | |
| JPH0543061Y2 (enrdf_load_stackoverflow) | ||
| US2729032A (en) | Glass bending apparatus | |
| JPH01242428A (ja) | ガラス製品の成形方法 | |
| JPH0441148Y2 (enrdf_load_stackoverflow) | ||
| JP3879152B2 (ja) | ガラス板の曲げ成形装置、曲げ成形型およびその製造方法 | |
| JPH05116974A (ja) | ガラス薄板の製造方法および製造装置 | |
| JP4171302B2 (ja) | コンフォーマルに加熱される雄型 | |
| JPS58110224A (ja) | 合成樹脂発泡シ−トの熱成型法 | |
| JPS59152232A (ja) | ガラス板の曲げ加工方法 | |
| JPH01122931A (ja) | 平滑面を有するガラス製品の成形方法 | |
| JPS62212237A (ja) | ガラス製品の成形方法 | |
| CN222834193U (zh) | 小曲率热弯玻璃模具 | |
| JPH04104122A (ja) | 曲面ガラス基板の成形型 | |
| WO2002068347A2 (en) | Heated ceramic female mold | |
| CN218232203U (zh) | 热弯模具和热弯机 | |
| JP2879375B2 (ja) | 発泡樹脂成形体の熱板成形方法 | |
| JPS582169B2 (ja) | 屈曲ガラスの製造方法 | |
| CN211111692U (zh) | 一种免抛光3d玻璃加工模具 | |
| JPS6245175B2 (enrdf_load_stackoverflow) | ||
| JPH0776102B2 (ja) | ガラスの中空体成形方法 | |
| JPH0243617B2 (enrdf_load_stackoverflow) | ||
| JPH046118A (ja) | ガラス板の曲げ型及び曲げ成形方法 |