JPH0515005B2 - - Google Patents

Info

Publication number
JPH0515005B2
JPH0515005B2 JP63131454A JP13145488A JPH0515005B2 JP H0515005 B2 JPH0515005 B2 JP H0515005B2 JP 63131454 A JP63131454 A JP 63131454A JP 13145488 A JP13145488 A JP 13145488A JP H0515005 B2 JPH0515005 B2 JP H0515005B2
Authority
JP
Japan
Prior art keywords
yps
conductivity
ysi
component concentration
sintered body
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
JP63131454A
Other languages
English (en)
Japanese (ja)
Other versions
JPH01302606A (ja
Inventor
Takafumi Kanazawa
Takashi Umegaki
Kimihiro Yamashita
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Central Glass Co Ltd
Original Assignee
Central Glass Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Central Glass Co Ltd filed Critical Central Glass Co Ltd
Priority to JP63131454A priority Critical patent/JPH01302606A/ja
Publication of JPH01302606A publication Critical patent/JPH01302606A/ja
Publication of JPH0515005B2 publication Critical patent/JPH0515005B2/ja
Granted legal-status Critical Current

Links

Classifications

    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02EREDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
    • Y02E60/00Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
    • Y02E60/10Energy storage using batteries

Landscapes

  • Compositions Of Oxide Ceramics (AREA)
  • Conductive Materials (AREA)
  • Secondary Cells (AREA)
JP63131454A 1988-05-31 1988-05-31 イオン伝導性リン珪酸塩組成物 Granted JPH01302606A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP63131454A JPH01302606A (ja) 1988-05-31 1988-05-31 イオン伝導性リン珪酸塩組成物

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP63131454A JPH01302606A (ja) 1988-05-31 1988-05-31 イオン伝導性リン珪酸塩組成物

Publications (2)

Publication Number Publication Date
JPH01302606A JPH01302606A (ja) 1989-12-06
JPH0515005B2 true JPH0515005B2 (enrdf_load_stackoverflow) 1993-02-26

Family

ID=15058336

Family Applications (1)

Application Number Title Priority Date Filing Date
JP63131454A Granted JPH01302606A (ja) 1988-05-31 1988-05-31 イオン伝導性リン珪酸塩組成物

Country Status (1)

Country Link
JP (1) JPH01302606A (enrdf_load_stackoverflow)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP5049565B2 (ja) * 2006-11-21 2012-10-17 パナソニック株式会社 全固体型電気二重層コンデンサー
JP6460316B2 (ja) * 2013-12-09 2019-01-30 日本電気硝子株式会社 ナトリウムイオン電池用電極合材、及びその製造方法並びにナトリウム全固体電池
JP7230772B2 (ja) * 2019-10-18 2023-03-01 トヨタ自動車株式会社 ナトリウムイオン伝導体の製造方法

Also Published As

Publication number Publication date
JPH01302606A (ja) 1989-12-06

Similar Documents

Publication Publication Date Title
US4049891A (en) Compositions for fast alkali-metal-ion transport
Khorassani et al. New Li+ ion conductors in the system Li4SiO4− Li3AsO4
US4013477A (en) Method for preparing dense, β-alumina ceramic bodies
US4097345A (en) Na5 GdSi4 O 12 and related rare earth sodium ion conductors and electrolytic cells therefrom
WO2014136650A1 (ja) リチウムイオン伝導性ガラスセラミックスの製造方法、リチウムイオン伝導性ガラスセラミックスおよびリチウムイオン二次電池
Hooper et al. Ionic conductivity of pure and doped Na3PO4
Martin Glass and glass-ceramic sulfide and oxy-sulfide solid electrolytes
Leo et al. Effect of MgO addition on the ionic conductivity of LiGe2 (PO4) 3 ceramics
JP2019046559A (ja) 固体電解質の製造方法、全固体電池用電極材料の製造方法、および全固体電池の製造方法
JPH08208333A (ja) 酸素イオン導電体及びその製造方法
JPH11130595A (ja) 酸化物イオン導電性単結晶及びその製造方法
Glaister Solid solution dielectrics based on sodium niobate
Kawada et al. Effects of boron and phosphorus substitution on sodium-ion conduction properties of glass-ceramic Na5FeSi4O12
US10804563B2 (en) Oxy-thio-nitride mixed network former solid electrolytes
JPH0515005B2 (enrdf_load_stackoverflow)
JP3740504B2 (ja) 固体電解質及びその製造方法
CA1081914A (en) METHOD OF PREPARING .beta."-A1.SUB.2O.SUB.3
Abid et al. Glass-forming region and electrical properties of Li2O-PbO-P2O5 glasses
JPS59141459A (ja) ナトリウムβアルミナ電解質要素及びそれらの製造方法
JPH04240155A (ja) ベータアルミナ質焼結体およびその製造方法
JPH0680462A (ja) 固体電解質
Okura et al. Fast potassium ion conducting glass-ceramics of Na5YSi4O12-type Na4-xKxY0. 6P0. 2Si2. 8O9
Sacks et al. New Solid Electrolytes Based on Cubic ZrP2 O 7
Makyta et al. The lithium ion conductivity of materials formed by pressed vitreous borosulfide slices
JP3202492B2 (ja) ベータアルミナ電解質