JPH0424434B2 - - Google Patents
Info
- Publication number
- JPH0424434B2 JPH0424434B2 JP57197573A JP19757382A JPH0424434B2 JP H0424434 B2 JPH0424434 B2 JP H0424434B2 JP 57197573 A JP57197573 A JP 57197573A JP 19757382 A JP19757382 A JP 19757382A JP H0424434 B2 JPH0424434 B2 JP H0424434B2
- Authority
- JP
- Japan
- Prior art keywords
- cobalt
- water
- elution
- temperature
- metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E30/00—Energy generation of nuclear origin
Landscapes
- Chemical Treatment Of Metals (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP57197573A JPS5989775A (ja) | 1982-11-12 | 1982-11-12 | コバルト含有金属のコバルト溶出抑制方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP57197573A JPS5989775A (ja) | 1982-11-12 | 1982-11-12 | コバルト含有金属のコバルト溶出抑制方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5989775A JPS5989775A (ja) | 1984-05-24 |
JPH0424434B2 true JPH0424434B2 (enrdf_load_stackoverflow) | 1992-04-27 |
Family
ID=16376743
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP57197573A Granted JPS5989775A (ja) | 1982-11-12 | 1982-11-12 | コバルト含有金属のコバルト溶出抑制方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5989775A (enrdf_load_stackoverflow) |
Families Citing this family (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2684648B2 (ja) * | 1986-07-08 | 1997-12-03 | 石川島播磨重工業株式会社 | ニッケル溶出抑制用ステンレス鋼 |
JP2523514B2 (ja) * | 1986-07-16 | 1996-08-14 | 株式会社東芝 | 燃料集合体 |
JP4500741B2 (ja) * | 2005-07-07 | 2010-07-14 | 日立Geニュークリア・エナジー株式会社 | 原子力プラント構造材料の応力腐食割れを緩和する方法 |
KR20080089418A (ko) * | 2005-12-21 | 2008-10-06 | 엑손모빌 리서치 앤드 엔지니어링 컴퍼니 | 파울링 감소를 위한 내식성 물질, 내식성 및 내파울링성이개선된 열 전달 부품, 및 파울링 감소 방법 |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5565368A (en) * | 1978-11-07 | 1980-05-16 | Toshiba Corp | Strengthening method for making passive state of stainless steel |
-
1982
- 1982-11-12 JP JP57197573A patent/JPS5989775A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS5989775A (ja) | 1984-05-24 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4722823A (en) | Nuclear power plant providing a function of suppressing the deposition of radioactive substance | |
JPS61111500A (ja) | 原子力プラントの放射能低減方法 | |
US5171515A (en) | Process for inhibiting corrosion in a pressurized water nuclear reactor | |
JPH0424434B2 (enrdf_load_stackoverflow) | ||
JPS5879196A (ja) | 放射性イオン付着抑制方法 | |
Lister et al. | Effects of magnesium and zinc additives on corrosion and cobalt contamination of stainless steels in simulated BWR coolant | |
JP3620128B2 (ja) | 原子力プラント用炭素鋼部材の表面処理方法 | |
JP2011089942A (ja) | 沸騰水型原子力プラントの水質制御方法 | |
JPS59126996A (ja) | 原子力プラントの製造法 | |
JPS6295498A (ja) | 原子力発電プラントの製造法 | |
JPS62120463A (ja) | 耐粒界腐食性ステンレス鋼 | |
EP0338769B1 (en) | Process for inhibiting corrosion in a pressurized water nuclear reactor | |
JPS63149598A (ja) | 原子力プラントの化学除染後の酸化処理方法 | |
JPH055077B2 (enrdf_load_stackoverflow) | ||
JPH03246496A (ja) | 原子力プラント用配管又は機器の放射性物質の付着抑制方法 | |
JPS6184597A (ja) | 原子力発電プラント構成部材の放射性物質の付着抑制方法 | |
JPS6312551B2 (enrdf_load_stackoverflow) | ||
JPS6053897A (ja) | 給水ヒ−タチユ−ブのコバルト溶出抑制方法 | |
JPS6224195A (ja) | 原子力プラントの放射能低減方法 | |
Mishima | Study on the influence of water chemistry on fuel cladding behaviour of LWR in Japan | |
Pearl et al. | Bibliography on Corrosion Products in High-Temperature Water Systems | |
JPS5912390A (ja) | 酸化皮膜形成方法 | |
JPH0479439B2 (enrdf_load_stackoverflow) | ||
Lister | The behaviour of dissolved cobalt in the cores of water-cooled reactors | |
JPH0249479B2 (enrdf_load_stackoverflow) |