JPH0411614B2 - - Google Patents
Info
- Publication number
- JPH0411614B2 JPH0411614B2 JP58005773A JP577383A JPH0411614B2 JP H0411614 B2 JPH0411614 B2 JP H0411614B2 JP 58005773 A JP58005773 A JP 58005773A JP 577383 A JP577383 A JP 577383A JP H0411614 B2 JPH0411614 B2 JP H0411614B2
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- molybdenum
- tungsten
- less
- ratio
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C19/00—Alloys based on nickel or cobalt
- C22C19/03—Alloys based on nickel or cobalt based on nickel
- C22C19/05—Alloys based on nickel or cobalt based on nickel with chromium
- C22C19/051—Alloys based on nickel or cobalt based on nickel with chromium and Mo or W
- C22C19/055—Alloys based on nickel or cobalt based on nickel with chromium and Mo or W with the maximum Cr content being at least 20% but less than 30%
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Manufacture And Refinement Of Metals (AREA)
- Turbine Rotor Nozzle Sealing (AREA)
- Chemically Coating (AREA)
- Powder Metallurgy (AREA)
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US353459 | 1982-03-01 | ||
US06/353,459 US4476091A (en) | 1982-03-01 | 1982-03-01 | Oxidation-resistant nickel alloy |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS58153751A JPS58153751A (ja) | 1983-09-12 |
JPH0411614B2 true JPH0411614B2 (en, 2012) | 1992-03-02 |
Family
ID=23389195
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP58005773A Granted JPS58153751A (ja) | 1982-03-01 | 1983-01-17 | 耐酸化性ニツケル合金 |
Country Status (7)
Country | Link |
---|---|
US (1) | US4476091A (en, 2012) |
JP (1) | JPS58153751A (en, 2012) |
CA (1) | CA1215255A (en, 2012) |
DE (1) | DE3306824C2 (en, 2012) |
FR (1) | FR2522335B1 (en, 2012) |
GB (1) | GB2116211B (en, 2012) |
IT (1) | IT1160481B (en, 2012) |
Families Citing this family (19)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US5424029A (en) * | 1982-04-05 | 1995-06-13 | Teledyne Industries, Inc. | Corrosion resistant nickel base alloy |
US4692305A (en) * | 1985-11-05 | 1987-09-08 | Perkin-Elmer Corporation | Corrosion and wear resistant alloy |
US4762682A (en) * | 1986-08-21 | 1988-08-09 | Haynes International, Inc. | Nickel-base super alloy |
US4889696A (en) * | 1986-08-21 | 1989-12-26 | Haynes International, Inc. | Chemical reactor for nitric acid |
US5372662A (en) * | 1992-01-16 | 1994-12-13 | Inco Alloys International, Inc. | Nickel-base alloy with superior stress rupture strength and grain size control |
GB2279966A (en) * | 1993-07-17 | 1995-01-18 | Special Melted Products Limite | Improving alloy compositions |
JPH10502129A (ja) * | 1994-06-24 | 1998-02-24 | テレダイン インダストリーズ インコーポレイテッド | ニッケルベース合金及び方法 |
WO1997023659A1 (en) * | 1995-12-21 | 1997-07-03 | Teledyne Industries, Inc. | Stress rupture properties of nickel-chromium-cobalt alloys by adjustment of the levels of phosphorus and boron |
JP4546318B2 (ja) * | 2005-04-15 | 2010-09-15 | 株式会社日立製作所 | Ni基合金部材とその製造法及びタービンエンジン部品並びに溶接材料とその製造法 |
US7803237B2 (en) | 2005-07-20 | 2010-09-28 | Damascus Steel Casting Company | Nickel-base alloy and articles made therefrom |
US9377245B2 (en) | 2013-03-15 | 2016-06-28 | Ut-Battelle, Llc | Heat exchanger life extension via in-situ reconditioning |
US9540714B2 (en) | 2013-03-15 | 2017-01-10 | Ut-Battelle, Llc | High strength alloys for high temperature service in liquid-salt cooled energy systems |
US10017842B2 (en) | 2013-08-05 | 2018-07-10 | Ut-Battelle, Llc | Creep-resistant, cobalt-containing alloys for high temperature, liquid-salt heat exchanger systems |
US9435011B2 (en) | 2013-08-08 | 2016-09-06 | Ut-Battelle, Llc | Creep-resistant, cobalt-free alloys for high temperature, liquid-salt heat exchanger systems |
US9683280B2 (en) | 2014-01-10 | 2017-06-20 | Ut-Battelle, Llc | Intermediate strength alloys for high temperature service in liquid-salt cooled energy systems |
US9683279B2 (en) | 2014-05-15 | 2017-06-20 | Ut-Battelle, Llc | Intermediate strength alloys for high temperature service in liquid-salt cooled energy systems |
US9605565B2 (en) | 2014-06-18 | 2017-03-28 | Ut-Battelle, Llc | Low-cost Fe—Ni—Cr alloys for high temperature valve applications |
EP3269472B1 (en) * | 2016-07-13 | 2022-09-07 | Ansaldo Energia IP UK Limited | Method for manufacturing mechanical components |
CN112553505A (zh) * | 2020-12-25 | 2021-03-26 | 江苏新核合金科技有限公司 | 一种镍基板材及其制备方法 |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5129316A (en, 2012) * | 1974-09-06 | 1976-03-12 | Nippon Steel Corp | |
US4110110A (en) * | 1975-08-27 | 1978-08-29 | Mitsubishi Kinzoku Kabushiki Kaisha | Nickel-base alloy excellent in corrosion resistance at high temperatures |
JPS5274509A (en) * | 1975-12-18 | 1977-06-22 | Mitsubishi Metal Corp | Ni-base sintered alloy |
-
1982
- 1982-03-01 US US06/353,459 patent/US4476091A/en not_active Expired - Lifetime
-
1983
- 1983-01-17 JP JP58005773A patent/JPS58153751A/ja active Granted
- 1983-01-20 FR FR8300817A patent/FR2522335B1/fr not_active Expired
- 1983-02-23 GB GB08305081A patent/GB2116211B/en not_active Expired
- 1983-02-25 CA CA000422383A patent/CA1215255A/en not_active Expired
- 1983-02-25 IT IT19778/83A patent/IT1160481B/it active
- 1983-02-26 DE DE3306824A patent/DE3306824C2/de not_active Expired - Lifetime
Also Published As
Publication number | Publication date |
---|---|
GB8305081D0 (en) | 1983-03-30 |
IT8319778A0 (it) | 1983-02-25 |
GB2116211A (en) | 1983-09-21 |
JPS58153751A (ja) | 1983-09-12 |
DE3306824A1 (de) | 1983-09-15 |
FR2522335A1 (fr) | 1983-09-02 |
CA1215255A (en) | 1986-12-16 |
DE3306824C2 (de) | 1995-12-14 |
US4476091A (en) | 1984-10-09 |
FR2522335B1 (fr) | 1987-05-29 |
GB2116211B (en) | 1985-06-26 |
IT1160481B (it) | 1987-03-11 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN102586652B (zh) | 用于先进燃气涡轮发动机的Ni-Cr-Co合金 | |
JPH0411614B2 (en, 2012) | ||
CA2032351C (en) | Oxidation resistant low expansion superalloys | |
US3165400A (en) | Castable heat resisting iron alloy | |
CA1066922A (en) | Heat-resistant allow for welded structures | |
CA2955320C (en) | Ni-based superalloy for hot forging | |
CA2955322C (en) | Ni-based superalloy for hot forging | |
CN108602163A (zh) | 焊接用Ni基合金实芯焊丝和Ni基合金焊接金属 | |
JPS5929105B2 (ja) | 耐溶融亜鉛侵食性にすぐれFe基合金 | |
CA2088065C (en) | Controlled thermal expansion alloy and article made therefrom | |
US5316721A (en) | Heat-resistant alloy having high creep rupture strength under high-temperature low-stress conditions and excellent resistance to carburization | |
US3432294A (en) | Cobalt-base alloy | |
EP0178785B1 (en) | Nickel-based alloy with high intergranular corrosion resistance, high stress corrosion cracking resistance and good hot workability | |
Barker et al. | Effect of Alloying Additions on the Microstructure, Corrosion Resistance and Mechanical Properties of Nickel–Silicon Alloys | |
US3984239A (en) | Filler metal | |
JPH10121170A (ja) | 耐食性に優れたNi−Cr系合金およびその製造方法 | |
JPH0317243A (ja) | タンタル含有超合金 | |
JP2007009279A (ja) | Ni−Fe基合金およびNi−Fe基合金材の製造方法 | |
US4195987A (en) | Weldable alloys | |
US3902899A (en) | Austenitic castable high temperature alloy | |
JPS5912739B2 (ja) | 改良された耐酸化性鉄基合金 | |
Waters et al. | A High Strength Nickel-Base Alloy with Improved Oxidation Resistance up to 2200 deg F | |
US2955034A (en) | Austenitic alloy steel | |
Waters et al. | Investigation of Columbium-Modified NASA TAZ-8 Superalloy | |
US3719475A (en) | Low carbon ferrous alloy containing chromium |