JPH041059B2 - - Google Patents
Info
- Publication number
- JPH041059B2 JPH041059B2 JP58088991A JP8899183A JPH041059B2 JP H041059 B2 JPH041059 B2 JP H041059B2 JP 58088991 A JP58088991 A JP 58088991A JP 8899183 A JP8899183 A JP 8899183A JP H041059 B2 JPH041059 B2 JP H041059B2
- Authority
- JP
- Japan
- Prior art keywords
- annealing
- secondary recrystallization
- temperature gradient
- grains
- coil
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
- C21D8/00—Modifying the physical properties by deformation combined with, or followed by, heat treatment
- C21D8/12—Modifying the physical properties by deformation combined with, or followed by, heat treatment during manufacturing of articles with special electromagnetic properties
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Physics & Mathematics (AREA)
- Crystallography & Structural Chemistry (AREA)
- Thermal Sciences (AREA)
- Manufacturing & Machinery (AREA)
- Electromagnetism (AREA)
- Mechanical Engineering (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Chemical Treatment Of Metals (AREA)
- Manufacturing Of Steel Electrode Plates (AREA)
- Soft Magnetic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58088991A JPS59215419A (ja) | 1983-05-20 | 1983-05-20 | 磁束密度の高い一方向性珪素鋼板の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP58088991A JPS59215419A (ja) | 1983-05-20 | 1983-05-20 | 磁束密度の高い一方向性珪素鋼板の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS59215419A JPS59215419A (ja) | 1984-12-05 |
| JPH041059B2 true JPH041059B2 (cs) | 1992-01-09 |
Family
ID=13958270
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP58088991A Granted JPS59215419A (ja) | 1983-05-20 | 1983-05-20 | 磁束密度の高い一方向性珪素鋼板の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS59215419A (cs) |
Families Citing this family (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS62156226A (ja) * | 1985-12-27 | 1987-07-11 | Nippon Steel Corp | 均一なグラス皮膜を有し磁気特性が優れた方向性電磁鋼板の製造方法 |
| CA2006292C (en) * | 1988-12-22 | 1997-09-09 | Yoshiyuki Ushigami | Very thin electrical steel strip having low core loss and high magnetic flux density and a process for producing the same |
| JPH0823047B2 (ja) * | 1990-11-19 | 1996-03-06 | 新日本製鐵株式会社 | 磁気特性、被膜特性ともに優れた方向性電磁鋼板の製造方法 |
| KR20250122492A (ko) | 2023-01-18 | 2025-08-13 | 닛폰세이테츠 가부시키가이샤 | 방향성 전자 강판의 제조 방법 |
| WO2024154774A1 (ja) | 2023-01-18 | 2024-07-25 | 日本製鉄株式会社 | 方向性電磁鋼板の製造方法 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS5850295B2 (ja) * | 1980-06-04 | 1983-11-09 | 新日本製鐵株式会社 | 磁束密度の高い一方向性珪素鋼板の製造法 |
| JPS57207114A (en) * | 1981-06-16 | 1982-12-18 | Nippon Steel Corp | Manufacture of anisotropic electric steel plate |
-
1983
- 1983-05-20 JP JP58088991A patent/JPS59215419A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS59215419A (ja) | 1984-12-05 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP5273944B2 (ja) | 鏡面方向性電磁鋼板の製造方法 | |
| EP2743358B1 (en) | Method for producing oriented magnetic steel sheet | |
| KR20180113556A (ko) | 방향성 전자 강판의 제조 방법 | |
| JPS6250529B2 (cs) | ||
| JPH0211728A (ja) | 無配向性電気鉄板の超高速焼なまし | |
| CN111417737A (zh) | 低铁损取向性电磁钢板及其制造方法 | |
| JPS5850295B2 (ja) | 磁束密度の高い一方向性珪素鋼板の製造法 | |
| JP2003171718A (ja) | 圧延面内での平均磁気特性に優れた電磁鋼板の製造方法 | |
| JPH04173923A (ja) | 磁気特性、皮膜特性ともに優れた一方向性電磁鋼板の製造方法 | |
| JPH041059B2 (cs) | ||
| JPS6056403B2 (ja) | 磁気特性の極めてすぐれたセミプロセス無方向性電磁鋼板の製造方法 | |
| CN114829657B (zh) | 取向电工钢板及其制造方法 | |
| JP4241226B2 (ja) | 方向性電磁鋼板の製造方法 | |
| KR950002895B1 (ko) | 초고규소 방향성 전자강판 및 그 제조방법 | |
| JP2011208196A (ja) | 著しく鉄損が低い方向性電磁鋼板の製造方法 | |
| JPS6242968B2 (cs) | ||
| JPH08295937A (ja) | 極めて低い鉄損をもつ一方向性電磁鋼板の製造方法 | |
| JP7623636B2 (ja) | 方向性電磁鋼板の製造方法 | |
| JP7338511B2 (ja) | 方向性電磁鋼板の製造方法 | |
| JPS6253572B2 (cs) | ||
| JPS61190017A (ja) | 鉄損の低い一方向性珪素鋼板の製造方法 | |
| JPS6256924B2 (cs) | ||
| KR970007333B1 (ko) | 저온 스라브가열 방식의 고자속밀도를 갖는 방향성 전기강판의 제조방법 | |
| JPH02259017A (ja) | 磁気特性、皮膜特性とも優れた一方向性電磁鋼板の製造方法 | |
| JPH04350124A (ja) | 薄板厚の一方向性珪素鋼板の製造方法 |