JPH0354183B2 - - Google Patents
Info
- Publication number
- JPH0354183B2 JPH0354183B2 JP59082800A JP8280084A JPH0354183B2 JP H0354183 B2 JPH0354183 B2 JP H0354183B2 JP 59082800 A JP59082800 A JP 59082800A JP 8280084 A JP8280084 A JP 8280084A JP H0354183 B2 JPH0354183 B2 JP H0354183B2
- Authority
- JP
- Japan
- Prior art keywords
- hot
- galvanized steel
- dip galvanized
- wiping
- gas
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C2/00—Hot-dipping or immersion processes for applying the coating material in the molten state without affecting the shape; Apparatus therefor
- C23C2/14—Removing excess of molten coatings; Controlling or regulating the coating thickness
- C23C2/16—Removing excess of molten coatings; Controlling or regulating the coating thickness using fluids under pressure, e.g. air knives
- C23C2/18—Removing excess of molten coatings from elongated material
- C23C2/20—Strips; Plates
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Coating With Molten Metal (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8280084A JPS60228661A (ja) | 1984-04-26 | 1984-04-26 | 溶融亜鉛めつき鋼板の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP8280084A JPS60228661A (ja) | 1984-04-26 | 1984-04-26 | 溶融亜鉛めつき鋼板の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS60228661A JPS60228661A (ja) | 1985-11-13 |
| JPH0354183B2 true JPH0354183B2 (enExample) | 1991-08-19 |
Family
ID=13784478
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP8280084A Granted JPS60228661A (ja) | 1984-04-26 | 1984-04-26 | 溶融亜鉛めつき鋼板の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS60228661A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP4834922B2 (ja) * | 2001-06-14 | 2011-12-14 | 住友金属工業株式会社 | 溶融亜鉛めっき鋼板の製造方法 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS51114334A (en) * | 1975-04-01 | 1976-10-08 | Nippon Steel Corp | Method of adjusting quantity of adhesion of plated metal in continuous molten metal plating |
| JPS5243455A (en) * | 1975-10-02 | 1977-04-05 | Sakura Sokki Kk | Electrode type liquid level measuring apparatus |
-
1984
- 1984-04-26 JP JP8280084A patent/JPS60228661A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS60228661A (ja) | 1985-11-13 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4053663A (en) | Method of treating ferrous strand for coating with aluminum-zinc alloys | |
| CN114107866B (zh) | 一种消除厚规格厚镀层涂覆钢板表面黑点缺陷的生产方法、一种厚规格厚镀层涂覆钢板 | |
| AU2002323927B2 (en) | Zinc-base hot dip galvanized steel sheet excellent in retention of gloss | |
| JPS6141754A (ja) | 鉄基金属ストリツプへの溶融亜鉛基メツキ被覆において筒口の亜鉛蒸気を調整する方法 | |
| DE112014006715T5 (de) | Verfahren zum direkten Herstellen eines beizenfreien feuermetallisierten Dünnbandprodukts aus einer Stahlschmelze | |
| JPH0354183B2 (enExample) | ||
| CA1069390A (en) | Method for effecting one side molten metal coating | |
| JPH0463259A (ja) | 加工性に優れた溶融合金化亜鉛めっき鋼板及びその製造方法 | |
| DE2339916B2 (de) | Verfahren zum Beschichten von Eisendraht, -band oder -litze mit Metall | |
| JPH04160142A (ja) | 溶融亜鉛系めっき鋼板とその製造方法 | |
| JPH04362167A (ja) | 密着性に優れた合金化溶融亜鉛めっき鋼板の製造方法 | |
| JPS6014116B2 (ja) | 電気錫メツキ鋼ストリツプの木目模様発生防止方法 | |
| JPH03211263A (ja) | 溶融めっき鋼板の製造装置 | |
| EP0082527A1 (en) | Process for partial hot dipping of steel strips | |
| JP3107961B2 (ja) | 連続溶融亜鉛メッキラインにおける浴中Al濃度制御装置 | |
| KR100448622B1 (ko) | 표면외관이 미려한 용융도금강판 제조방법 | |
| JPH0297654A (ja) | 溶融亜鉛メッキ鋼板の製造方法 | |
| CN205296965U (zh) | 一种杆塔防护镀层结构 | |
| JPH042759A (ja) | 合金化溶融亜鉛めっき鋼板の製造方法及びそのめっき浴 | |
| JP2602755B2 (ja) | 密着性の優れた溶融メッキ鋼板 | |
| JPH0225981B2 (enExample) | ||
| JPH02217453A (ja) | 溶融金属めっきにおけるめっき鋼帯の後処理方法 | |
| JPS624473B2 (enExample) | ||
| JPH0235024B2 (enExample) | ||