JPH0353366B2 - - Google Patents
Info
- Publication number
- JPH0353366B2 JPH0353366B2 JP15638381A JP15638381A JPH0353366B2 JP H0353366 B2 JPH0353366 B2 JP H0353366B2 JP 15638381 A JP15638381 A JP 15638381A JP 15638381 A JP15638381 A JP 15638381A JP H0353366 B2 JPH0353366 B2 JP H0353366B2
- Authority
- JP
- Japan
- Prior art keywords
- molten steel
- gas
- blown
- inclusions
- amount
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21C—PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- C21C7/00—Treating molten ferrous alloys, e.g. steel, not covered by groups C21C1/00 - C21C5/00
- C21C7/04—Removing impurities by adding a treating agent
- C21C7/072—Treatment with gases
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Treatment Of Steel In Its Molten State (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15638381A JPS5858220A (ja) | 1981-10-01 | 1981-10-01 | 取鍋内溶鋼の清浄化方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP15638381A JPS5858220A (ja) | 1981-10-01 | 1981-10-01 | 取鍋内溶鋼の清浄化方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5858220A JPS5858220A (ja) | 1983-04-06 |
| JPH0353366B2 true JPH0353366B2 (enExample) | 1991-08-14 |
Family
ID=15626547
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP15638381A Granted JPS5858220A (ja) | 1981-10-01 | 1981-10-01 | 取鍋内溶鋼の清浄化方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5858220A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH01170555A (ja) * | 1987-12-25 | 1989-07-05 | Nkk Corp | 溶融金属の清浄化方法 |
-
1981
- 1981-10-01 JP JP15638381A patent/JPS5858220A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5858220A (ja) | 1983-04-06 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2018066030A (ja) | 高清浄鋼の製造方法 | |
| CN101294233A (zh) | 一种铁水预处理同时脱硅脱锰的方法 | |
| JP2018066031A (ja) | 高清浄鋼の製造方法 | |
| US4695318A (en) | Method of making steel | |
| KR100985308B1 (ko) | 극저황 고청정 강의 제조 방법 | |
| JPH0353366B2 (enExample) | ||
| KR100368239B1 (ko) | 고청정강의 정련방법 | |
| JP6547638B2 (ja) | 高清浄鋼の製造方法 | |
| JPS5816006A (ja) | 溶銑脱燐方法 | |
| KR20000042054A (ko) | 알루미늄 탈산 고청정강의 정련방법 | |
| RU2201458C1 (ru) | Способ модифицирования стали | |
| KR100336855B1 (ko) | 고청정알루미늄탈산강제조용후럭스와이어 | |
| KR910006640B1 (ko) | 고청정강 제조방법 | |
| JPH07188731A (ja) | 極低酸素鋼溶製方法 | |
| KR940008456B1 (ko) | 투피스캔용 저탄소강의 알루미나계 개재물 저감방법 | |
| KR100910471B1 (ko) | 용강의 청정도 및 탈류효율 향상 방법 | |
| JPS61223120A (ja) | 溶鋼の介在物低減方法 | |
| SU1167212A1 (ru) | Рафинировочна смесь | |
| JP3465801B2 (ja) | Fe−Ni系合金溶湯の精錬方法 | |
| JPH08143943A (ja) | 溶湯の精錬方法 | |
| JPH07224317A (ja) | 高清浄度鋼の製造方法 | |
| JPH0361722B2 (enExample) | ||
| JP3282530B2 (ja) | 高清浄度の低Si鋼の製造方法 | |
| JP2001172715A (ja) | 極低炭素ステンレス溶鋼の製造方法 | |
| KR20050037076A (ko) | 저류강의 제조방법 |