JPH0310699B2 - - Google Patents
Info
- Publication number
- JPH0310699B2 JPH0310699B2 JP59079101A JP7910184A JPH0310699B2 JP H0310699 B2 JPH0310699 B2 JP H0310699B2 JP 59079101 A JP59079101 A JP 59079101A JP 7910184 A JP7910184 A JP 7910184A JP H0310699 B2 JPH0310699 B2 JP H0310699B2
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- less
- temperature
- flux density
- wear
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Magnetic Heads (AREA)
- Soft Magnetic Materials (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59079101A JPS60224728A (ja) | 1984-04-19 | 1984-04-19 | 耐摩耗性高透磁率合金およびその製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP59079101A JPS60224728A (ja) | 1984-04-19 | 1984-04-19 | 耐摩耗性高透磁率合金およびその製造法 |
Related Child Applications (2)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP1262696A Division JPH0645847B2 (ja) | 1989-10-07 | 1989-10-07 | 耐摩耗性高透磁率合金の製造法 |
JP1262697A Division JPH02186605A (ja) | 1989-10-07 | 1989-10-07 | 耐摩耗性高透磁率磁気記録再生ヘッド |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS60224728A JPS60224728A (ja) | 1985-11-09 |
JPH0310699B2 true JPH0310699B2 (en, 2012) | 1991-02-14 |
Family
ID=13680487
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP59079101A Granted JPS60224728A (ja) | 1984-04-19 | 1984-04-19 | 耐摩耗性高透磁率合金およびその製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS60224728A (en, 2012) |
Families Citing this family (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6191340A (ja) * | 1984-10-11 | 1986-05-09 | Res Inst Electric Magnetic Alloys | 耐摩耗性高透磁率合金およびその製造法 |
JPS61174349A (ja) * | 1985-01-30 | 1986-08-06 | Res Inst Electric Magnetic Alloys | 耐摩耗性高透磁率合金およびその製造法ならびに磁気記録再生ヘツド |
JP3294029B2 (ja) * | 1994-11-16 | 2002-06-17 | 財団法人電気磁気材料研究所 | 耐摩耗性高透磁率合金およびその製造法ならびに磁気記録再生ヘッド |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS50121120A (en, 2012) * | 1974-03-12 | 1975-09-22 | ||
JPS58123848A (ja) * | 1982-01-20 | 1983-07-23 | Res Inst Electric Magnetic Alloys | 磁気記録再生ヘツド用耐摩耗性高透磁率合金およびその製造法ならびに磁気記録再生ヘツド |
JPS6024348A (ja) * | 1983-07-21 | 1985-02-07 | Res Inst Electric Magnetic Alloys | 磁気記録再生ヘツド用耐摩耗性高透磁率合金およびその製造法ならびに磁気記録再生ヘツド |
-
1984
- 1984-04-19 JP JP59079101A patent/JPS60224728A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS60224728A (ja) | 1985-11-09 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US4830685A (en) | Wear-resistant alloy of high permeability and method of producing the same | |
JP2777319B2 (ja) | 耐摩耗性高透磁率合金およびその製造法ならびに磁気記録再生ヘッド | |
JPS62988B2 (en, 2012) | ||
KR100405929B1 (ko) | 내마모성고투과율합금,그의제조방법및자기기록재생헤드 | |
JPS625972B2 (en, 2012) | ||
JPS6212296B2 (en, 2012) | ||
JPH0310699B2 (en, 2012) | ||
JP3251899B2 (ja) | 耐摩耗性高透磁率合金および磁気記録再生ヘッド | |
JPH02194154A (ja) | 耐摩耗性高透磁率合金の製造法 | |
JPH0377644B2 (en, 2012) | ||
JPH0645849B2 (ja) | 耐摩耗性高透磁率合金の製造法 | |
JPH0310700B2 (en, 2012) | ||
JPS5947017B2 (ja) | 磁気録音および再生ヘツド用磁性合金ならびにその製造法 | |
JPH02153036A (ja) | 磁気記録再生ヘッド用耐摩耗性高透磁率合金およびその製造法ならびに磁気記録再生ヘッド | |
JPS6218619B2 (en, 2012) | ||
JPH0645846B2 (ja) | 耐摩耗性高透磁率合金の製造法 | |
JPH0368107B2 (en, 2012) | ||
JPH02146704A (ja) | 耐摩耗性高透磁率磁気記録再生ヘッド | |
JPH0377645B2 (en, 2012) | ||
JPH0645848B2 (ja) | 磁気記録再生ヘッド用耐摩耗性高透磁率合金の製造法ならびに磁気記録再生ヘッド | |
JPH032216B2 (en, 2012) | ||
JPS6155583B2 (en, 2012) | ||
KR920006607B1 (ko) | 고투자율 연자성재료용 철(Fe)계 합금의 제조방법 | |
JPS6130405B2 (en, 2012) | ||
JPS5857499B2 (ja) | Ni−Fe−Nb系耐摩耗性高透磁率合金および磁気記録再生ヘッド |