JPH0229384U - - Google Patents
Info
- Publication number
- JPH0229384U JPH0229384U JP10758888U JP10758888U JPH0229384U JP H0229384 U JPH0229384 U JP H0229384U JP 10758888 U JP10758888 U JP 10758888U JP 10758888 U JP10758888 U JP 10758888U JP H0229384 U JPH0229384 U JP H0229384U
- Authority
- JP
- Japan
- Prior art keywords
- welding
- joint
- inner lining
- flange
- pipe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Description
第1図は本考案の一実施例である直埋型絶縁継
手の説明図、第2図は第1図の要部の拡大説明図
である。 図において、1と2は管本体、3は第1溶接部
、4は第2溶接部、5はマスチツク、6はシユリ
ンクチユーブ、7は開先、8は継手用のリング、
9は環状溝、11と21はフランジ、12と22
はライニングである。なお、図中同一符号は同一
または相当部分を示す。
手の説明図、第2図は第1図の要部の拡大説明図
である。 図において、1と2は管本体、3は第1溶接部
、4は第2溶接部、5はマスチツク、6はシユリ
ンクチユーブ、7は開先、8は継手用のリング、
9は環状溝、11と21はフランジ、12と22
はライニングである。なお、図中同一符号は同一
または相当部分を示す。
Claims (1)
- 【実用新案登録請求の範囲】 内面ライニング管の溶接による現地接合におい
て、管に取り付けられたフランジの外周部で円周
溶接を行い、その際発生する溶接熱を利用してフ
ランジ面の内面ライニング材を軟化・溶融し、か
つ溶接収縮により接合させ、継手部の内面ライニ
ングを一体化する溶接継手において、 前記円周溶接用開先のルート面の内側における
フランジの接合面に管軸とほぼ同軸な環状溝を設
けたことを特徴とする管突合せ溶接継手。