JPH0211981B2 - - Google Patents
Info
- Publication number
- JPH0211981B2 JPH0211981B2 JP56215119A JP21511981A JPH0211981B2 JP H0211981 B2 JPH0211981 B2 JP H0211981B2 JP 56215119 A JP56215119 A JP 56215119A JP 21511981 A JP21511981 A JP 21511981A JP H0211981 B2 JPH0211981 B2 JP H0211981B2
- Authority
- JP
- Japan
- Prior art keywords
- cathode plate
- plate
- cathode
- acid
- immersed
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/26—Processes of manufacture
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56215119A JPS58117641A (ja) | 1981-12-29 | 1981-12-29 | 密閉形ニツケルカドミウム蓄電池用陰極板の製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP56215119A JPS58117641A (ja) | 1981-12-29 | 1981-12-29 | 密閉形ニツケルカドミウム蓄電池用陰極板の製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS58117641A JPS58117641A (ja) | 1983-07-13 |
| JPH0211981B2 true JPH0211981B2 (enrdf_load_stackoverflow) | 1990-03-16 |
Family
ID=16667051
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP56215119A Granted JPS58117641A (ja) | 1981-12-29 | 1981-12-29 | 密閉形ニツケルカドミウム蓄電池用陰極板の製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS58117641A (enrdf_load_stackoverflow) |
-
1981
- 1981-12-29 JP JP56215119A patent/JPS58117641A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS58117641A (ja) | 1983-07-13 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN110911662A (zh) | 一种具有保护层的锂负极及其制备方法和应用 | |
| US4055709A (en) | Rejuvenation of nickel-cadmium battery cells | |
| JP3412451B2 (ja) | アルカリ蓄電池正極用ニッケル焼結基板とその製造法およびアルカリ蓄電池 | |
| JPH0211981B2 (enrdf_load_stackoverflow) | ||
| US4139423A (en) | Sintered negative plate | |
| US4032697A (en) | Methods of producing electrodes for alkaline batteries | |
| JPH031783B2 (enrdf_load_stackoverflow) | ||
| US4713126A (en) | Process for manufacturing negative cadmium electrodes for sealed alkaline battery cells | |
| JPH0732008B2 (ja) | 電池用セパレ−タの製造法 | |
| JPH0218547B2 (enrdf_load_stackoverflow) | ||
| US2952726A (en) | Storage batteries | |
| JPS58194254A (ja) | 電池用セパレ−タの製造法 | |
| JPS5949670B2 (ja) | アルカリ電池のための電極の製法 | |
| JP2639916B2 (ja) | アルカリ蓄電池用焼結式ニツケル電極の製造方法 | |
| JPS5838459A (ja) | 密閉形アルカリ蓄電池用極板の製造法 | |
| Shi et al. | Effect of perfluoroalkylsulfonate on the discharge behaviour of PbO2 electrodes in sulfuric acid solution | |
| US4166010A (en) | Sintered negative plate | |
| JPH0410176B2 (enrdf_load_stackoverflow) | ||
| JP2541355B2 (ja) | 鉛蓄電池用極板の製造方法 | |
| JPS58186164A (ja) | アルカリ蓄電池用負極の製造法 | |
| JPS61142668A (ja) | 鉛蓄電池の製造方法 | |
| JPS58129762A (ja) | 密閉形ニツケルカドミウム蓄電池陰極板の製造法 | |
| JPH0475257A (ja) | アルカリ蓄電池用水酸化ニッケル電極の製造方法 | |
| DE3131664A1 (de) | Verfahren zur verringerung des kriechstrom-verlusts" | |
| JPS63160161A (ja) | アルカリ蓄電池用陽極板の製造法 |