JPH0199775A - 溶融接合における下地処理方法 - Google Patents

溶融接合における下地処理方法

Info

Publication number
JPH0199775A
JPH0199775A JP25521987A JP25521987A JPH0199775A JP H0199775 A JPH0199775 A JP H0199775A JP 25521987 A JP25521987 A JP 25521987A JP 25521987 A JP25521987 A JP 25521987A JP H0199775 A JPH0199775 A JP H0199775A
Authority
JP
Japan
Prior art keywords
steel
alloy
treatment
base material
blasting
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP25521987A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0367470B2 (enExample
Inventor
Toshihiro Arai
新居 稔弘
Yutaka Yuchi
有地 裕
Chitose Shiotani
塩谷 千歳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Sumikin Kozai Kogyo KK
Original Assignee
Sumitomo Metal Industries Ltd
Sumikin Kozai Kogyo KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sumitomo Metal Industries Ltd, Sumikin Kozai Kogyo KK filed Critical Sumitomo Metal Industries Ltd
Priority to JP25521987A priority Critical patent/JPH0199775A/ja
Publication of JPH0199775A publication Critical patent/JPH0199775A/ja
Publication of JPH0367470B2 publication Critical patent/JPH0367470B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Pressure Welding/Diffusion-Bonding (AREA)
  • Ceramic Products (AREA)
  • Coating By Spraying Or Casting (AREA)
  • Application Of Or Painting With Fluid Materials (AREA)
JP25521987A 1987-10-09 1987-10-09 溶融接合における下地処理方法 Granted JPH0199775A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP25521987A JPH0199775A (ja) 1987-10-09 1987-10-09 溶融接合における下地処理方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP25521987A JPH0199775A (ja) 1987-10-09 1987-10-09 溶融接合における下地処理方法

Publications (2)

Publication Number Publication Date
JPH0199775A true JPH0199775A (ja) 1989-04-18
JPH0367470B2 JPH0367470B2 (enExample) 1991-10-23

Family

ID=17275679

Family Applications (1)

Application Number Title Priority Date Filing Date
JP25521987A Granted JPH0199775A (ja) 1987-10-09 1987-10-09 溶融接合における下地処理方法

Country Status (1)

Country Link
JP (1) JPH0199775A (enExample)

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH03268867A (ja) * 1990-03-15 1991-11-29 Furukawa Alum Co Ltd ろう付け用アルミニウム又はアルミニウム合金板
US6635993B1 (en) 1998-08-26 2003-10-21 Ngk Insulators, Ltd. Joined bodies, high-pressure discharge lamps and a method for manufacturing the same
US6642654B2 (en) 2000-07-03 2003-11-04 Ngk Insulators, Ltd. Joined body and a high pressure discharge lamp
US6703136B1 (en) 2000-07-03 2004-03-09 Ngk Insulators, Ltd. Joined body and high-pressure discharge lamp
US6812642B1 (en) 2000-07-03 2004-11-02 Ngk Insulators, Ltd. Joined body and a high-pressure discharge lamp

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5195941A (en) * 1975-02-21 1976-08-23 Handatsukeseino suguretayojuaenmetsukikohan oyobi seizoho
JPS5223531A (en) * 1975-08-18 1977-02-22 Nissan Motor Abrasionnresistant sliding member and its production method

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS5195941A (en) * 1975-02-21 1976-08-23 Handatsukeseino suguretayojuaenmetsukikohan oyobi seizoho
JPS5223531A (en) * 1975-08-18 1977-02-22 Nissan Motor Abrasionnresistant sliding member and its production method

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH03268867A (ja) * 1990-03-15 1991-11-29 Furukawa Alum Co Ltd ろう付け用アルミニウム又はアルミニウム合金板
US6635993B1 (en) 1998-08-26 2003-10-21 Ngk Insulators, Ltd. Joined bodies, high-pressure discharge lamps and a method for manufacturing the same
US6844677B2 (en) 1998-08-26 2005-01-18 Ngk Insulators, Ltd. Joined bodies, high-pressure discharge lamps and a method for manufacturing the same
US6642654B2 (en) 2000-07-03 2003-11-04 Ngk Insulators, Ltd. Joined body and a high pressure discharge lamp
US6703136B1 (en) 2000-07-03 2004-03-09 Ngk Insulators, Ltd. Joined body and high-pressure discharge lamp
US6812642B1 (en) 2000-07-03 2004-11-02 Ngk Insulators, Ltd. Joined body and a high-pressure discharge lamp
US6850009B2 (en) 2000-07-03 2005-02-01 Ngk Insulators, Ltd. Joined body and high pressure discharge lamp

Also Published As

Publication number Publication date
JPH0367470B2 (enExample) 1991-10-23

Similar Documents

Publication Publication Date Title
US6344237B1 (en) Method of depositing flux or flux and metal onto a metal brazing substrate
US4173685A (en) Coating material and method of applying same for producing wear and corrosion resistant coated articles
US4621761A (en) Process for forming unusually strong joints between metals and ceramics by brazing at temperatures that do no exceed 750 degree C.
CN1161489C (zh) 金属附着层以及金属附着层的沉积方法
EP1916318B1 (en) Braze pre-placement using cold spray deposition
US6913184B2 (en) Alloy composition and method for low temperature fluxless brazing
US4763828A (en) Method for bonding ceramics and metals
US4725509A (en) Titanium-copper-nickel braze filler metal and method of brazing
JP5268937B2 (ja) タンタル被覆鋼構造体を接合する方法
US5723187A (en) Method of bonding thermally sprayed coating to non-roughened aluminum surfaces
US9108276B2 (en) Hardface coating systems and methods for metal alloys and other materials for wear and corrosion resistant applications
US7451906B2 (en) Products for use in low temperature fluxless brazing
CN101643899A (zh) 一种异种金属焊接中间层的制备方法
JP2008519157A (ja) 耐摩耗被覆を施したアルミニウム製品とその被覆を製品に施すための方法
CZ290659B6 (cs) Způsob vytváření přilnavého povlaku z hliníkové pájky na podkladovém materiálu a způsob vzájemného spojování součástí
US9982332B2 (en) Hardface coating systems and methods for metal alloys and other materials for wear and corrosion resistant applications
CN109355652A (zh) 激光熔覆用镍基合金粉末及其制备方法
JP7261167B2 (ja) 溶射された中間層を用いた溶接できない金属の抵抗溶接
CN106975861A (zh) 一种含有包覆层的碳化钨颗粒的硬面材料及其制备方法
CN113088960B (zh) 一种钛合金软包装耐磨涂层及其制备方法
JPS58188585A (ja) Al材と異種金属材の接合方法
JPH0367470B2 (enExample)
WO2014105239A1 (en) Hardface coating systems and methods for metal alloys and other materials for wear and corrosion resistant applications
JPS5983756A (ja) 銅基金属基材への銅基溶射皮膜の被着法
JP2000117427A (ja) スパッタリング用ターゲット板の接合方法