JPH01307411A5 - - Google Patents

Info

Publication number
JPH01307411A5
JPH01307411A5 JP1-76385A JP7638589A JPH01307411A5 JP H01307411 A5 JPH01307411 A5 JP H01307411A5 JP 7638589 A JP7638589 A JP 7638589A JP H01307411 A5 JPH01307411 A5 JP H01307411A5
Authority
JP
Japan
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP1-76385A
Other languages
English (en)
Japanese (ja)
Other versions
JP2747318B2 (ja
JPH01307411A (ja
Filing date
Publication date
Priority claimed from DE3810166A external-priority patent/DE3810166A1/de
Application filed filed Critical
Publication of JPH01307411A publication Critical patent/JPH01307411A/ja
Publication of JPH01307411A5 publication Critical patent/JPH01307411A5/ja
Application granted granted Critical
Publication of JP2747318B2 publication Critical patent/JP2747318B2/ja
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Links

JP1076385A 1988-03-25 1989-03-27 エチレンアクリル酸共重合体含有水性濃厚物ならびにラッカーおよび有機塗料組成物の凝集方法 Expired - Lifetime JP2747318B2 (ja)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
DE3810166A DE3810166A1 (de) 1988-03-25 1988-03-25 Verwendung eines waessrigen konzentrates, enthaltend ein ethylen-acrylsaeure-copolymerisat, sowie verfahren zur koagulation von lacken und anderen organischen beschichtungsmitteln
DE3810166.1 1988-03-25

Publications (3)

Publication Number Publication Date
JPH01307411A JPH01307411A (ja) 1989-12-12
JPH01307411A5 true JPH01307411A5 (enExample) 1997-02-10
JP2747318B2 JP2747318B2 (ja) 1998-05-06

Family

ID=6350710

Family Applications (1)

Application Number Title Priority Date Filing Date
JP1076385A Expired - Lifetime JP2747318B2 (ja) 1988-03-25 1989-03-27 エチレンアクリル酸共重合体含有水性濃厚物ならびにラッカーおよび有機塗料組成物の凝集方法

Country Status (8)

Country Link
US (1) US4933091A (enExample)
EP (1) EP0335210B1 (enExample)
JP (1) JP2747318B2 (enExample)
BR (1) BR8901411A (enExample)
DE (2) DE3810166A1 (enExample)
ES (1) ES2032066T3 (enExample)
FI (1) FI94256C (enExample)
HU (1) HU206384B (enExample)

Families Citing this family (20)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE3931907A1 (de) * 1989-09-25 1991-04-04 Henkel Kgaa Waessriges lackoverspray-schutzcoating fuer spritzkabinen sowie verfahren zu dessen herstellung
CH680710A5 (enExample) * 1989-12-22 1992-10-30 Unicolor Ag
DE4025729A1 (de) * 1990-08-14 1992-02-20 Henkel Kgaa Verwendung von molybdaenverbindungen zur lack-koagulierung
RU2034788C1 (ru) * 1990-12-28 1995-05-10 Совместное советско-западногерманское предприятие "Аква Ремонт" Способ очистки воды от органических соединений
US5282970A (en) * 1991-04-09 1994-02-01 Unicolor Ag Method for environmentally benign paint spraying with an air-drying lacquer dissolved, emulgated or dispersed in water
CH680711A5 (enExample) * 1991-04-09 1992-10-30 Unicolor Ag
GB9113568D0 (en) * 1991-06-24 1991-08-14 Brent Chemicals Int Paint denaturant
GB9116004D0 (en) * 1991-07-24 1991-09-11 Brent Chemicals Int Method for removing coatings from metal substrates prone to corrosion or deterioration
FR2679915B1 (fr) * 1991-08-02 1994-09-09 Francais Prod Ind Cfpi Procede de denaturation des peintures hydrodiluables et des peintures solvantees et solution de denaturation mise en óoeuvre dans ce procede.
DE4216352A1 (de) * 1992-05-18 1993-11-25 Henkel Kgaa Verfahren zur Entklebung von Koagulation von Lacken
DE19617535A1 (de) * 1995-05-03 1996-11-07 Peter H Deil Verfahren zur Aufarbeitung von flüssigkeitshaltigen Lackschlämmen
RU2156741C1 (ru) * 1999-12-22 2000-09-27 Государственное предприятие Комплексный научно-исследовательский и конструкторско-технологический институт водоснабжения, канализации, гидротехнических сооружений и инженерной гидрогеологии Коагулянт для очистки воды от лакокрасочных материалов
DE102005012891A1 (de) 2005-03-17 2006-09-21 Dbk David + Baader Gmbh Faltheizelement und Verfahren zu dessen Herstellung
US20060246299A1 (en) * 2005-04-29 2006-11-02 Brady Michael D Methods for protecting glass
US20060246302A1 (en) * 2005-04-29 2006-11-02 Brady Michael D Methods for protecting glass
US8470911B2 (en) * 2006-04-06 2013-06-25 Styrolution GmbH Process for coagulation of aqueous polymer dispersions
BRPI0713654A2 (pt) * 2006-06-28 2012-10-23 Valspar Sourcing Inc método para vedar a borda de um substrato de madeira processado e sistema de vedação de borda para um substrato de madeira processado
US20100304126A1 (en) * 2006-06-28 2010-12-02 Valspar Sourcing, Inc. Method and system for coating wood substrates using organic coagulants
JP5468171B1 (ja) * 2013-08-02 2014-04-09 アイビーグリーン株式会社 吸液性固状物、吸液性固状物の製造方法、凝固剤、除菌性凝固剤、研磨助剤、消臭・芳香剤、及び防虫剤。
PL3805296T3 (pl) 2019-10-07 2025-04-28 Sk Innovation Co., Ltd. Wodna dyspersja kopolimeru etylen-kwas karboksylowy i sposób jej wytwarzania

Family Cites Families (15)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE1017957B (de) * 1954-12-14 1957-10-17 Henkel & Cie Gmbh Zusatzmittel fuer Spuelwaesser zum Niederschlagen von Lacknebeln
DE1517409A1 (de) * 1965-04-24 1969-09-11 Solvay Werke Gmbh Zusatzmittel zur Spuelfluessigkeiten zur Koagulierung von Lack- und Grundiermittelteilchen
US3515575A (en) * 1968-03-06 1970-06-02 Grace W R & Co Process of deactivating and collecting paints with a water curtain
US3723148A (en) * 1971-03-15 1973-03-27 Oxy Metal Finishing Corp Process for recovering coating materials
JPS5013277A (enExample) * 1973-06-09 1975-02-12
DE2347068C3 (de) * 1973-09-19 1982-01-28 Hoechst Ag, 6000 Frankfurt Lackentklebungs- und Sedimentationsmittel
US3861887A (en) * 1973-11-01 1975-01-21 Steven W Forney Process for controlling pollution and contamination in paint or lacquer spray booths
US3958227A (en) * 1974-09-24 1976-05-18 International Business Machines Corporation Control store system with flexible control word selection
US3990986A (en) * 1974-12-19 1976-11-09 Nalco Chemical Company Composition for the clarification and detackification of paint spray booth wastes
DE3412763A1 (de) * 1984-04-05 1985-10-17 Henkel Kgaa Mittel zur koagulierung von lacken, wachsen und beschichtungsmitteln
DE3416119A1 (de) * 1984-04-30 1985-10-31 Henkel KGaA, 4000 Düsseldorf Hydrophobierte polymerampholyte fuer die lackkoagulation
DE3512564A1 (de) * 1985-04-06 1986-10-16 Basf Ag, 6700 Ludwigshafen Waessrige wachsdispersionen als konservierungsmittel fuer metall- und lackoberflaechen, ihre verwendung und ein verfahren zum temporaeren konservieren von metall- und lackoberflaechen
US4699730A (en) * 1985-05-24 1987-10-13 Chemfil Corporation Magnesium sulfate and complex silicate mineral paint denaturant
EP0280440A1 (en) * 1987-02-11 1988-08-31 Betz Europe, Inc. Paint spray booth detackification method
US4764561A (en) * 1987-06-12 1988-08-16 Nalco Chemical Company Melamine-formaldehyde/styrene-acrylate paint detackification composition

Similar Documents

Publication Publication Date Title
JPH0218036A5 (enExample)
JPH01244845A5 (enExample)
JPH01217002A5 (enExample)
JPH01215935A5 (enExample)
JPH01217499A5 (enExample)
JPH01228940A5 (enExample)
JPH01248055A5 (enExample)
JPH02132008A5 (enExample)
JPH01223181A5 (enExample)
JPH01219171A5 (enExample)
JPH01247211A5 (enExample)
JPH01240136A5 (enExample)
JPH01230989A5 (enExample)
JPH01268632A5 (enExample)
JPH01242358A5 (enExample)
JPH01224635A5 (enExample)
JPH01245959A5 (enExample)
JPH01254673A5 (enExample)
JPH01240529A5 (enExample)
JPH01244988A5 (enExample)
JPH01219172A5 (enExample)
JPH01247469A5 (enExample)
JPH01242750A5 (enExample)
JPH01226886A5 (enExample)
JPH01299290A5 (enExample)