JP4719076B2 - ビニル重合体製造方法 - Google Patents
ビニル重合体製造方法 Download PDFInfo
- Publication number
- JP4719076B2 JP4719076B2 JP2006130904A JP2006130904A JP4719076B2 JP 4719076 B2 JP4719076 B2 JP 4719076B2 JP 2006130904 A JP2006130904 A JP 2006130904A JP 2006130904 A JP2006130904 A JP 2006130904A JP 4719076 B2 JP4719076 B2 JP 4719076B2
- Authority
- JP
- Japan
- Prior art keywords
- polymerization
- initiator
- vinyl
- mma
- e3fap
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
- 0 OS(C(*1CC1)(F)F)(O)=O Chemical compound OS(C(*1CC1)(F)F)(O)=O 0.000 description 1
Images
Landscapes
- Polymerization Catalysts (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2006130904A JP4719076B2 (ja) | 2006-05-10 | 2006-05-10 | ビニル重合体製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2006130904A JP4719076B2 (ja) | 2006-05-10 | 2006-05-10 | ビニル重合体製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2007302752A JP2007302752A (ja) | 2007-11-22 |
| JP2007302752A5 JP2007302752A5 (enExample) | 2009-06-25 |
| JP4719076B2 true JP4719076B2 (ja) | 2011-07-06 |
Family
ID=38836960
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2006130904A Expired - Fee Related JP4719076B2 (ja) | 2006-05-10 | 2006-05-10 | ビニル重合体製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP4719076B2 (enExample) |
Family Cites Families (5)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE69302117T2 (de) * | 1992-02-19 | 1996-08-29 | Bp Chem Int Ltd | Butenpolymere |
| US20020128532A1 (en) * | 2000-05-31 | 2002-09-12 | Chevron Chemical Company Llc | High viscosity polyalphaolefins prepared with ionic liquid catalyst |
| ZA200108461B (en) * | 2000-10-27 | 2002-06-06 | Celanese Chem Europe Gmbh | Process of telomerizing conjugated dienes. |
| DE10303931B4 (de) * | 2002-02-04 | 2013-04-18 | Institut Français du Pétrole | Katalytische Zusammensetzung zur Dimerisierung, Co-Dimerisierung, Oligomerisierung und Polymerisation der Olefine |
| JP4719080B2 (ja) * | 2005-05-20 | 2011-07-06 | 修一 菅野 | ビニル重合体製造方法 |
-
2006
- 2006-05-10 JP JP2006130904A patent/JP4719076B2/ja not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| JP2007302752A (ja) | 2007-11-22 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Strehmel et al. | Free radical polymerization of n-butyl methacrylate in ionic liquids | |
| Sarbu et al. | ATRP of methyl methacrylate in the presence of ionic liquids with ferrous and cuprous anions | |
| EP2069408A2 (en) | Living radical polymerization of activated and nonactivated monomers containing electron-withdrawing side groups | |
| RU2012114458A (ru) | Система и способ катионной полимеризации | |
| CN104194756B (zh) | 一种新型水合物动力学抑制剂及其制备方法及应用 | |
| WO2021049455A1 (ja) | 含フッ素化合物の製造方法及び共重合体の製造方法 | |
| WO2015122404A1 (ja) | リビングラジカル重合触媒及びそれを用いた重合体の製造方法 | |
| JP2026043011A (ja) | テルル含有化合物、重合体、及び重合体の製造方法 | |
| Nguyen et al. | TREN versus Me6‐TREN as ligands in SET‐LRP of methyl acrylate | |
| CN111051362A (zh) | 制备丁烯低聚物的方法 | |
| EP3617190A1 (en) | Organic tellurium compound, method for producing same, living radical polymerization initiator, method for producing vinyl polymer, and vinyl polymer | |
| JP2007302752A (ja) | ビニル重合体、その製造方法およびビニル重合体の重合開始剤 | |
| US20030130454A1 (en) | Process for producing amphipathic polymers | |
| JPS59161413A (ja) | フルオロアクリル酸系共重合体 | |
| JP2021523267A (ja) | 制御された構造を有するビニル芳香族ポリマーの合成のための重合方法 | |
| TW201920303A (zh) | 藉由自由基聚合的含有氧乙烯鏈的乙烯醚聚合物的製造方法 | |
| JP4719080B2 (ja) | ビニル重合体製造方法 | |
| CN102503844B (zh) | 一种具有双子表面活性的原子转移自由基聚合引发剂及其合成方法 | |
| Liu et al. | A facile, simple, and inexpensive ionic liquid, 1-alkyl-3-methylimidazole chloride, as ligand for the iron (III)-mediated reverse atom transfer radical polymerization of methyl methacrylate | |
| JP2005330446A (ja) | ビニル重合体、リビングラジカル重合体およびそれらの製造方法 | |
| CN103641938B (zh) | 一种可用于烯类单体聚合反应的引发剂 | |
| KR101453888B1 (ko) | 이온성 액체 내의 고비점 유기화합물을 제거하는 이온성 액체의 정제방법 | |
| Su | Ionic chain polymerization | |
| KR20110049353A (ko) | 고산화상태의 금속이온 화합물을 이용한 원자이동라디칼 중합법을 이용한 비닐단량체의 중합방법 | |
| JP2020019745A (ja) | シクロカーボネート基含有(メタ)アクリレートモノマー |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20090510 |
|
| A621 | Written request for application examination |
Free format text: JAPANESE INTERMEDIATE CODE: A621 Effective date: 20090510 |
|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20100706 |
|
| A711 | Notification of change in applicant |
Free format text: JAPANESE INTERMEDIATE CODE: A711 Effective date: 20100707 |
|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A821 Effective date: 20100708 |
|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A821 Effective date: 20100707 |
|
| A977 | Report on retrieval |
Free format text: JAPANESE INTERMEDIATE CODE: A971007 Effective date: 20101213 |
|
| A131 | Notification of reasons for refusal |
Free format text: JAPANESE INTERMEDIATE CODE: A131 Effective date: 20101221 |
|
| A521 | Request for written amendment filed |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20110221 |
|
| TRDD | Decision of grant or rejection written | ||
| A01 | Written decision to grant a patent or to grant a registration (utility model) |
Free format text: JAPANESE INTERMEDIATE CODE: A01 Effective date: 20110329 |
|
| A01 | Written decision to grant a patent or to grant a registration (utility model) |
Free format text: JAPANESE INTERMEDIATE CODE: A01 |
|
| A61 | First payment of annual fees (during grant procedure) |
Free format text: JAPANESE INTERMEDIATE CODE: A61 Effective date: 20110401 |
|
| R150 | Certificate of patent or registration of utility model |
Ref document number: 4719076 Country of ref document: JP Free format text: JAPANESE INTERMEDIATE CODE: R150 Free format text: JAPANESE INTERMEDIATE CODE: R150 |
|
| FPAY | Renewal fee payment (event date is renewal date of database) |
Free format text: PAYMENT UNTIL: 20140408 Year of fee payment: 3 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| LAPS | Cancellation because of no payment of annual fees |