JP3258739B2 - 接着性に優れた表面処理鋼板の製造方法 - Google Patents
接着性に優れた表面処理鋼板の製造方法Info
- Publication number
- JP3258739B2 JP3258739B2 JP01215293A JP1215293A JP3258739B2 JP 3258739 B2 JP3258739 B2 JP 3258739B2 JP 01215293 A JP01215293 A JP 01215293A JP 1215293 A JP1215293 A JP 1215293A JP 3258739 B2 JP3258739 B2 JP 3258739B2
- Authority
- JP
- Japan
- Prior art keywords
- steel sheet
- treated steel
- adhesion
- water
- chromate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Links
Landscapes
- Application Of Or Painting With Fluid Materials (AREA)
- Laminated Bodies (AREA)
- Electroplating Methods And Accessories (AREA)
- Chemical Treatment Of Metals (AREA)
- Other Surface Treatments For Metallic Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP01215293A JP3258739B2 (ja) | 1993-01-28 | 1993-01-28 | 接着性に優れた表面処理鋼板の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP01215293A JP3258739B2 (ja) | 1993-01-28 | 1993-01-28 | 接着性に優れた表面処理鋼板の製造方法 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JPH06220657A JPH06220657A (ja) | 1994-08-09 |
| JPH06220657A5 JPH06220657A5 (enExample) | 2000-11-21 |
| JP3258739B2 true JP3258739B2 (ja) | 2002-02-18 |
Family
ID=11797505
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP01215293A Expired - Fee Related JP3258739B2 (ja) | 1993-01-28 | 1993-01-28 | 接着性に優れた表面処理鋼板の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP3258739B2 (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR20020045215A (ko) * | 2000-12-08 | 2002-06-19 | 이구택 | 도금 밀착성이 우수한 고장력 용융아연 도금강판의 제조방법 |
| KR100966862B1 (ko) * | 2007-12-14 | 2010-06-29 | 포스코강판 주식회사 | 메탈 인쇄회로기판용 방열 도장 강판 및 그 제조 방법 |
-
1993
- 1993-01-28 JP JP01215293A patent/JP3258739B2/ja not_active Expired - Fee Related
Also Published As
| Publication number | Publication date |
|---|---|
| JPH06220657A (ja) | 1994-08-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| TW507512B (en) | Method for manufacturing printed wiring board comprising electrodeposited copper foil with carrier and resistor circuit; and printed wiring board comprising resistor circuit | |
| US5071520A (en) | Method of treating metal foil to improve peel strength | |
| JPS5856758B2 (ja) | ドウハクヒヨウメンシヨリホウホウ | |
| JP2010000679A (ja) | アルミニウム材及びその製造方法 | |
| CN102714915B (zh) | 电子电路及其形成方法以及电子电路形成用覆铜层压板 | |
| JP2620151B2 (ja) | 印刷回路用銅箔 | |
| CN102265712A (zh) | 电子电路的形成方法 | |
| US5300158A (en) | Protective coating having adhesion improving characteristics | |
| JPH0512878B2 (enExample) | ||
| US7037597B2 (en) | Copper foil for printed-wiring board | |
| CN115334767B (zh) | 一种无胶覆铜板用压延铜箔表面处理方法、无胶挠性覆铜板用铜箔及其应用 | |
| JP2517503B2 (ja) | 印刷回路用銅箔の表面処理方法 | |
| CN102548202A (zh) | 经粗化处理的铜箔及其制造方法 | |
| EP0839440B1 (en) | Copper foil for the manufacture of printed circuits and method of producing same | |
| US5057193A (en) | Anti-tarnish treatment of metal foil | |
| JPH06220657A (ja) | 接着性に優れた表面処理鋼板の製造方法 | |
| JP3300160B2 (ja) | 銅箔の処理方法 | |
| JP2875186B2 (ja) | 印刷回路用銅箔の処理方法 | |
| JP3113445B2 (ja) | 印刷回路用銅箔及びその製造方法 | |
| JP3900116B2 (ja) | 電子回路基板用の表面処理銅箔及びその製造方法 | |
| JPH05167243A (ja) | 印刷回路用銅箔の表面処理方法 | |
| JPS6214040B2 (enExample) | ||
| JP2684164B2 (ja) | 印刷回路用銅箔の表面処理方法 | |
| JPH05275817A (ja) | 銅箔の製造方法 | |
| JPH07109558A (ja) | 水ぬれ性の良い銅箔の製造方法 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| LAPS | Cancellation because of no payment of annual fees |