JP2015032572A5 - - Google Patents

Download PDF

Info

Publication number
JP2015032572A5
JP2015032572A5 JP2013164010A JP2013164010A JP2015032572A5 JP 2015032572 A5 JP2015032572 A5 JP 2015032572A5 JP 2013164010 A JP2013164010 A JP 2013164010A JP 2013164010 A JP2013164010 A JP 2013164010A JP 2015032572 A5 JP2015032572 A5 JP 2015032572A5
Authority
JP
Japan
Prior art keywords
battery
electrode plate
analysis method
internal impedance
transfer resistance
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2013164010A
Other languages
English (en)
Japanese (ja)
Other versions
JP2015032572A (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2013164010A priority Critical patent/JP2015032572A/ja
Priority claimed from JP2013164010A external-priority patent/JP2015032572A/ja
Publication of JP2015032572A publication Critical patent/JP2015032572A/ja
Publication of JP2015032572A5 publication Critical patent/JP2015032572A5/ja
Pending legal-status Critical Current

Links

Images

JP2013164010A 2013-08-07 2013-08-07 電池の劣化分析方法 Pending JP2015032572A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2013164010A JP2015032572A (ja) 2013-08-07 2013-08-07 電池の劣化分析方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2013164010A JP2015032572A (ja) 2013-08-07 2013-08-07 電池の劣化分析方法

Publications (2)

Publication Number Publication Date
JP2015032572A JP2015032572A (ja) 2015-02-16
JP2015032572A5 true JP2015032572A5 (enExample) 2016-09-29

Family

ID=52517710

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2013164010A Pending JP2015032572A (ja) 2013-08-07 2013-08-07 電池の劣化分析方法

Country Status (1)

Country Link
JP (1) JP2015032572A (enExample)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109342954A (zh) * 2018-10-25 2019-02-15 东莞塔菲尔新能源科技有限公司 一种电池测试分析结构及其制造方法和电池测试分析方法
CN112687884A (zh) * 2020-12-14 2021-04-20 风帆有限责任公司 一种原位测试电池极片阻抗的锂电池及其制作方法
KR102657496B1 (ko) * 2020-12-28 2024-04-12 주식회사 엘지에너지솔루션 배터리 관리 장치 및 방법

Family Cites Families (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2003317810A (ja) * 2002-04-18 2003-11-07 Toyota Motor Corp 電池の特性評価方法
JP2012079582A (ja) * 2010-10-04 2012-04-19 Nec Corp 二次電池、二次電池の正極または負極の抵抗測定方法、および、二次電池の正極または負極の劣化程度診断方法
JP2012212513A (ja) * 2011-03-30 2012-11-01 Toyota Motor Corp リチウム二次電池の状態検出方法
JP5850492B2 (ja) * 2011-10-13 2016-02-03 学校法人早稲田大学 電池システムおよび電池の評価方法

Similar Documents

Publication Publication Date Title
JP6187069B2 (ja) リチウム電池
JP5850492B2 (ja) 電池システムおよび電池の評価方法
CN101490895B (zh) 蓄电装置
JP4228177B2 (ja) 二次電池、および、それを用いたバッテリー
CN109560245B (zh) 对称电池及其制备方法
CN102636142B (zh) 一种测试锂离子电池阳极片膨胀的方法
JP2013118122A5 (enExample)
CN103413975A (zh) 镍钴锰酸锂圆柱型高倍率电池及其制备方法
CN103904381B (zh) 电池内部温度测量装置
CN203941992U (zh) 一种锂离子电池的内部温度测试结构
CN104979591B (zh) 电化学储能电芯和蓄电池及获取其电极电位的方法
CN207233865U (zh) 电极极片及锂离子电池
CN103500859B (zh) 一种锂离子电池用三电极电池装置
JP2017527950A (ja) 冷却性能が改善された電池セル
CN104037458A (zh) 一种锂离子储能器件的制造方法
PL3748760T3 (pl) Elektroda z błoną izolacyjną, sposób jej wytwarzania oraz zawierająca ją litowa bateria akumulatorowa
CN102593545A (zh) 一种锂离子电池及其内部温度的测量方法
JP2015118024A (ja) 二次電池モジュールおよび二次電池監視装置
JP2015032572A5 (enExample)
CN107275669A (zh) 锂二次电池
CN104953087B (zh) 一种锂电池及其负极、电芯、负极电压监控方法
CN210120185U (zh) 一种软包三电极锂离子电池的极耳结构
JP2014075285A (ja) リチウム二次電池の電極電位測定装置およびこれを用いた電極電位の測定方法
CN107785625B (zh) 一种简易的软包四电极锂离子电池测试体系
CN104485481A (zh) 锂离子电芯体以及带该电芯体的锂离子电池