JP2013199318A - Bottom coated container and method for manufacturing the same - Google Patents

Bottom coated container and method for manufacturing the same Download PDF

Info

Publication number
JP2013199318A
JP2013199318A JP2012070424A JP2012070424A JP2013199318A JP 2013199318 A JP2013199318 A JP 2013199318A JP 2012070424 A JP2012070424 A JP 2012070424A JP 2012070424 A JP2012070424 A JP 2012070424A JP 2013199318 A JP2013199318 A JP 2013199318A
Authority
JP
Japan
Prior art keywords
container
label
shrink label
tack
shrink
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2012070424A
Other languages
Japanese (ja)
Inventor
Hiroyuki Fujita
弘幸 藤田
Tetsuya Shibata
哲也 柴田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Otsuka Pharmaceutical Co Ltd
Fuji Seal International Inc
Original Assignee
Otsuka Pharmaceutical Co Ltd
Fuji Seal International Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Otsuka Pharmaceutical Co Ltd, Fuji Seal International Inc filed Critical Otsuka Pharmaceutical Co Ltd
Priority to JP2012070424A priority Critical patent/JP2013199318A/en
Publication of JP2013199318A publication Critical patent/JP2013199318A/en
Pending legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To prevent damage to a tack label in a bottom coated container in which the tack label is stuck to the lower end of a shrink label, going around the bottom of the container, from below.SOLUTION: A bottom coated container has the following configuration. The lower part of a cylindrical shrink label 2 is configured to go around from the body 10 to the bottom 11 of a container 1. A tack label 3 is stuck to the shrink label 2 in order to close a lower end opening 20 of the shrink label 2. A recess 12 recessed above a part 13 to be placed is formed at the bottom 11 of the container 1. The lower end 2a of the shrink label 2 is located in a space 14 of the recess at the bottom 11 of the container 1, and also, forms an annular sticking support surface while being separated downward from a wall surface 12a of the recess. The tack label 3 is stuck onto the sticking support surface from below and stored in the space 14 of the recess.

Description

本発明は、容器の底部が被覆された底被覆容器、及び、その製造方法に関する。   The present invention relates to a bottom-coated container in which the bottom of the container is coated, and a method for manufacturing the same.

従来、下記特許文献1、2のように、容器の胴部を覆う筒状のシュリンクラベルの下部が容器の底部まで回り込んで該底部の周縁部を覆うと共に、その下側即ち表面側からタックラベルを貼着してシュリンクラベルの下端開口部を閉塞した底被覆容器が提案されている。   Conventionally, as in Patent Documents 1 and 2 below, the lower part of the cylindrical shrink label that covers the body of the container wraps around to the bottom of the container to cover the peripheral edge of the bottom, and is tacked from the lower side, that is, from the surface side. A bottom coating container has been proposed in which a label is attached to close a lower end opening of a shrink label.

かかる底被覆容器にあっては、シュリンクラベルで覆われる容器の底部の周縁部は、容器を載置する際の載置部であって最も下方に突出した部位である。そして、その載置部を覆うシュリンクラベルの下端部にタックラベルの周縁部が貼着されている。従って、タックラベルの周縁部は容器の載置部の下側に位置しており、必然的に、タックラベルは容器の底部の載置部よりも下側に突出して位置することになる。   In such a bottom-coated container, the peripheral edge portion of the bottom part of the container covered with the shrink label is a mounting part when the container is mounted and is a part that protrudes downward most. And the peripheral part of a tack label is stuck by the lower end part of the shrink label which covers the mounting part. Accordingly, the peripheral portion of the tack label is positioned below the placement portion of the container, and the tack label is necessarily positioned so as to protrude below the placement portion of the bottom portion of the container.

しかしながら、タックラベルが最も下側に位置して突出状態にあると、例えば製造ライン上を搬送する際や製造後の流通過程において、タックラベルの周縁部が他の物にひっかかって剥がれたり損傷したりする可能性がある。   However, if the tack label is in the lowest position and is in the protruding state, for example, when transported on the production line or in the distribution process after production, the peripheral edge of the tack label may be caught by other objects and peeled off or damaged. There is a possibility.

特開2006−82854号公報JP 2006-82854 A 特開2006−117269号公報JP 2006-117269 A

それゆえに本発明は上記従来の問題点に鑑みてなされ、容器の底部に回り込んだシュリンクラベルの下端部に下側からタックラベルが貼着された底被覆容器において、タックラベルの損傷を防止することができる底被覆容器とその製造方法を提供することを課題とする。   Therefore, the present invention has been made in view of the above-described conventional problems, and prevents damage to the tack label in a bottom-coated container in which a tack label is attached from the lower side to the lower end portion of the shrink label that wraps around the bottom of the container. It is an object of the present invention to provide a bottom coated container and a method for manufacturing the same.

本発明は、上記課題を解決すべくなされたものであって、本発明に係る底被覆容器は、筒状のシュリンクベルの下部が容器の胴部から底部に回り込んでいて該シュリンクラベルの下端開口部を閉塞すべくタックラベルがシュリンクラベルに貼着されている底被覆容器であって、容器の底部には載置部よりも上方に凹んだ凹部が形成され、シュリンクラベルの下端部は容器の底部の凹部空間内に位置すると共に該凹部壁面から下方に離間した状態で環状の貼り付け支持面を形成し、該貼り付け支持面にタックラベルが下側から貼着されて凹部空間内に収容されていることを特徴とする。   The present invention has been made to solve the above-mentioned problems, and the bottom-coated container according to the present invention is such that the lower part of the cylindrical shrink bell goes around from the body part of the container to the bottom part, and the lower end of the shrink label. A bottom-coated container in which a tack label is attached to a shrink label so as to close the opening, and a concave portion is formed in the bottom of the container so as to be recessed above the mounting portion, and the lower end of the shrink label is a container. An annular sticking support surface is formed in a state of being located in the recessed space at the bottom of the lower portion and spaced downward from the wall surface of the recessed portion, and a tack label is attached to the sticking supporting surface from below to enter the recessed space. It is housed.

該構成の底被覆容器にあっては、シュリンクラベルの下端部が容器の底部の凹部空間内に位置して環状の貼り付け支持面を形成しているので、シュリンクラベルの下端部が容器の底部の載置部から容器の中心に向けて略水平に延びている場合に比して、タックラベルを凹部空間内に容易に収容することができる。また、シュリンクラベルの下端部から形成される環状の貼り付け支持面が凹部壁面から下方に離間しているので、凹部壁面に密着するまでシュリンクラベルの下端部を上方に押し上げる必要がなく、押し上げによるシュリンクラベルの下端部への負荷や影響が小さくてシュリンクラベルの下端部の破れ等の損傷を防止することができる。更に、環状の貼り付け支持面が凹部壁面から下方に離間しているので、容器の底部がペタロイド形状のように凹凸の激しい形状であっても、タックラベルを貼着するための貼り付け支持面には凹凸がなく、タックラベルを体裁良く均一に貼着することができる。そして、タックラベルが凹部空間内に収容されているので、タックラベルが底被覆容器の載置面より下方に突出せず、輸送中等にタックラベルの周縁部が他の物に引っかかって剥がれたりするということが防止される。   In the bottom-coated container having such a configuration, the lower end portion of the shrink label is positioned in the recess space of the bottom portion of the container to form an annular sticking support surface, so that the lower end portion of the shrink label is the bottom portion of the container The tack label can be easily accommodated in the recessed space as compared with the case where the container extends substantially horizontally from the placing portion toward the center of the container. Moreover, since the annular sticking support surface formed from the lower end portion of the shrink label is spaced downward from the concave wall surface, it is not necessary to push the lower end portion of the shrink label upward until it is in close contact with the concave wall surface. The load and influence on the lower end portion of the shrink label are small, and damage such as tearing of the lower end portion of the shrink label can be prevented. Furthermore, since the annular sticking support surface is spaced downward from the wall surface of the recess, the sticking support surface for sticking the tack label even when the bottom of the container has a rugged shape such as a petaloid shape. There is no unevenness, and the tack label can be applied uniformly in a good appearance. And since the tack label is accommodated in the recessed space, the tack label does not protrude downward from the mounting surface of the bottom coating container, and the peripheral edge of the tack label may be caught by other objects and peeled off during transportation. This is prevented.

特に、タックラベルが底被覆容器の載置面よりも上方に離間して位置していることが好ましい。底被覆容器の載置面は底被覆容器が接触する面であり、該載置面とタックラベルとが面一であってもよいが、載置面よりもタックラベルが所定距離上方に離間して位置していることにより、搬送中等においてタックラベルが擦れて傷ついたりすることもなく、タックラベルの損傷をより一層防止できる。   In particular, it is preferable that the tack label is located apart from the mounting surface of the bottom coating container. The mounting surface of the bottom coating container is a surface that contacts the bottom coating container, and the mounting surface and the tack label may be flush with each other, but the tack label is spaced a predetermined distance above the mounting surface. Therefore, the tack label is not rubbed and damaged during transportation, and the tack label can be further prevented from being damaged.

また、シュリンクラベルとタックラベルが遮光性を有していることが好ましく、容器をいわゆる遮光容器として構成することができる。そして、タックラベルが貼着されてシュリンクラベルの下端開口部が閉塞されていることにより、シュリンクラベルのみの構成に比して、容器の底部の良好な外観体裁が得られると同時に、容器の底部における遮光性が確実なものとなる。   Moreover, it is preferable that a shrink label and a tack label have light-shielding property, and a container can be comprised as what is called a light-shielding container. And since the tack label is stuck and the lower end opening of the shrink label is closed, a good appearance appearance of the bottom of the container can be obtained at the same time as the structure of only the shrink label, and the bottom of the container As a result, the light shielding property at is ensured.

また、本発明に係る底被覆容器の製造方法は、筒状のシュリンクラベルを熱収縮させて該シュリンクラベルの下部を容器の胴部から容器の底部に回り込ませる収縮工程と、容器の底部に回り込んだシュリンクラベルの下端部を容器の底部の凹部空間内に押し込む押し込み工程と、タックラベルをシュリンクラベルの下端部に押し付けて貼着する貼着工程と、を備えることを特徴とする。   In addition, the method for manufacturing a bottom-coated container according to the present invention includes a shrinking process in which a cylindrical shrink label is thermally shrunk so that a lower part of the shrink label is wrapped around the bottom of the container from the body of the container. A pressing step of pushing the lower end portion of the shrink label into the recessed space at the bottom of the container; and an attaching step of attaching the tack label to the lower end portion of the shrink label.

該底被覆容器の製造方法にあっては、容器の底部に回り込んだシュリンクラベルの下端部を容器の底部の凹部空間内に押し込む押し込み工程により、シュリンクラベルの下端部が容器の底部の凹部空間内に位置して環状の貼り付け支持面が形成される。   In the manufacturing method of the bottom coated container, the lower end of the shrink label is pushed into the recessed space at the bottom of the container by the pushing process of pushing the lower end of the shrink label around the bottom of the container into the recessed space at the bottom of the container. An annular sticking support surface is formed inside.

また、押し込み工程の後に貼着工程を行うようにしてもよいが、押し込み工程と貼着工程を同時に行うことが好ましい。これにより、一工程でタックラベルを凹部空間内に位置させると同時にシュリンクラベルの下端部によって形成された貼り付け支持面にタックラベルを貼着することができる。   Moreover, although an adhesion process may be performed after an indentation process, it is preferable to perform an indentation process and an adhesion process simultaneously. Thereby, a tack label can be affixed on the affixing support surface formed by the lower end part of a shrink label at the same time it positions a tack label in recessed part space by one process.

以上のように、本発明に係る底被覆容器にあっては、シュリンクラベルの下端部が凹部空間内において凹部壁面から離間した環状の貼り付け支持面を形成してその貼り付け支持面にタックラベルが貼着されて凹部空間内に収容されているので、輸送中等におけるタックラベルの周縁部の損傷を防止することができる。また、シュリンクラベルの下端部が凹部壁面から離間した貼り付け支持面を形成しているので、容器の底部に凹部が形成されていても、タックラベルをシュリンクラベルの下端部に貼着することができる。特に、容器の底部がペタロイド形状のように凹凸の激しい形状であっても環状の貼り付け支持面が凹部壁面から離間しているので、容器の底部の凹凸形状の影響を受けることなくタックラベルをシュリンクラベルの下端部に貼着することができる。   As described above, in the bottom coating container according to the present invention, the lower end portion of the shrink label forms an annular sticking support surface separated from the wall surface of the recess in the recess space, and the tack label is formed on the sticking support surface. Is stuck and accommodated in the recessed space, so that damage to the peripheral portion of the tack label during transportation or the like can be prevented. In addition, since the lower end portion of the shrink label forms an affixing support surface separated from the concave wall surface, the tack label can be adhered to the lower end portion of the shrink label even if the concave portion is formed on the bottom of the container. it can. In particular, even if the bottom of the container has a rugged shape such as a petaloid shape, the annular sticking support surface is separated from the concave wall surface, so the tack label is not affected by the rugged shape of the bottom of the container. It can be attached to the lower end of the shrink label.

また、本発明に係る底被覆容器の製造方法にあっては、容器の底部に回り込んだシュリンクラベルの下端部を容器の底部の凹部空間内に押し込む押し込み工程を備えているので、タックラベルが凹部空間内に位置する底被覆容器を容易に製造することができる。   Further, in the method for manufacturing a bottom-coated container according to the present invention, the tack label is provided with a pushing process of pushing the lower end portion of the shrink label that wraps around the bottom portion of the container into the recessed space of the bottom portion of the container. A bottom coating container located in the recessed space can be easily manufactured.

本発明の一実施形態における底被覆容器の要部を示す断面図。Sectional drawing which shows the principal part of the bottom coating container in one Embodiment of this invention. 同底被覆容器の要部拡大断面図。The principal part expanded sectional view of the bottom covered container. 同底被覆容器に使用されているシュリンクラベルを示す一部破断線を含む正面図。The front view including the partially broken line which shows the shrink label currently used for the same bottom covering container. 同シュリンクラベルの要部断面図。Sectional drawing of the principal part of the shrink label. 同シュリンクラベルの製造途中の状態を示す要部断面図。Sectional drawing which shows the principal part which shows the state in the middle of manufacture of the shrink label. 同底被覆容器の製造途中の状態を示す要部断面図。The principal part sectional drawing which shows the state in the middle of manufacture of the bottom covered container. 同底被覆容器の製造途中の状態であって、図6の次の工程を示す要部断面図。FIG. 7 is a cross-sectional view of the main part showing the next step of FIG. 同底被覆容器の製造途中の状態であって、図7の次の工程を示す要部断面図。FIG. 8 is a cross-sectional view of a principal part showing the next step of FIG. 本発明の他の実施形態における底被覆容器の製造方法を示す断面図。Sectional drawing which shows the manufacturing method of the bottom coating container in other embodiment of this invention.

以下、本発明の一実施形態に係る底被覆容器とその製造方法について図1〜図8を参酌しつつ説明する。図1に示す底被覆容器は、容器1の胴部10から底部11にかけて筒状のシュリンクラベル2が装着され、容器1の底部11に位置するシュリンクラベル2の下端開口部20を閉塞すべくタックラベル3がシュリンクラベル2に貼着されたものである。具体的には、容器1の底部11には載置部13よりも上方に凹んだ凹部12が形成されていて、シュリンクラベル2の下端部2aは容器1の底部11の凹部空間14内に位置すると共に凹部壁面12aから下方に離間した状態で略フラットな環状の貼り付け支持面を形成しており、該貼り付け支持面にタックラベル3が下側から貼着されて凹部空間14内に収容された状態となっている。即ち、図1に底被覆容器の載置面Pを二点鎖線で示しているが、この載置面Pよりもタックラベル3が上方に所定距離離間した状態となっている。以下、詳細に説明する。   Hereinafter, a bottom coating container and a manufacturing method thereof according to an embodiment of the present invention will be described with reference to FIGS. The bottom covering container shown in FIG. 1 has a cylindrical shrink label 2 attached from the body 10 to the bottom 11 of the container 1, and tacks to close the lower end opening 20 of the shrink label 2 located at the bottom 11 of the container 1. The label 3 is affixed to the shrink label 2. Specifically, the bottom portion 11 of the container 1 is formed with a recess 12 that is recessed above the placement portion 13, and the lower end portion 2 a of the shrink label 2 is positioned in the recess space 14 of the bottom portion 11 of the container 1. In addition, a substantially flat annular support surface is formed in a state of being spaced downward from the recess wall surface 12a, and the tack label 3 is attached to the adhesive support surface from below and accommodated in the recess space 14 It has become a state. That is, in FIG. 1, the placement surface P of the bottom covering container is indicated by a two-dot chain line, but the tack label 3 is separated from the placement surface P by a predetermined distance. Details will be described below.

容器1は、胴部10の上側に図示しない肩部と口部とを有している。肩部は口部から胴部10に向かって徐々に横断面積が大きくなるように下広がりに形成されている。容器1の底部11は、その周縁部に最も低い載置部13が形成され該載置部13の中心側に上側に向けて凹んだ凹部12を有する形状であって、例えば、ペタロイド形状に形成されている。従って、底部11の中央部即ち載置部13の中心側には凹部空間14が形成される。容器1は、ガラス瓶やペットボトルであって、光が透過可能であり、例えば、無色透明なものが採用される。尚、胴部10の断面形状は、円形の他、矩形等であってもよい。また、口部には図示しない蓋(キャップ)が装着される。   The container 1 has a shoulder portion and a mouth portion (not shown) on the upper side of the trunk portion 10. The shoulder portion is formed to spread downward so that the cross-sectional area gradually increases from the mouth portion toward the trunk portion 10. The bottom portion 11 of the container 1 has a shape in which the lowest placement portion 13 is formed at the peripheral portion thereof and has a concave portion 12 that is recessed upward on the center side of the placement portion 13. For example, the bottom portion 11 is formed in a petaloid shape. Has been. Accordingly, a recessed space 14 is formed at the center of the bottom 11, that is, at the center of the mounting portion 13. The container 1 is a glass bottle or a PET bottle and can transmit light. For example, a colorless and transparent one is adopted. In addition, the cross-sectional shape of the trunk | drum 10 may be a rectangle other than a circle. A lid (cap) (not shown) is attached to the mouth.

シュリンクラベル2は、図3に示すように、容器1へ装着される前の状態において既に筒状に形成されているものである。シュリンクラベル2は、各種の熱収縮性フィルムからなる基材フィルム21に印刷等が施されたものであって、該基材フィルム21の主延伸方向が周方向となるように主延伸方向の両端部同士が重ね合わせられて筒状に形成されており、従って、重ね合わせ部22は軸線方向に沿って形成されている。   As shown in FIG. 3, the shrink label 2 is already formed in a cylindrical shape before being attached to the container 1. The shrink label 2 is obtained by printing or the like on a base film 21 made of various heat-shrinkable films, and both ends in the main stretching direction so that the main stretching direction of the base film 21 is a circumferential direction. The portions are overlapped to form a cylinder, and thus the overlap portion 22 is formed along the axial direction.

シュリンクラベル2の表面には表印刷層23が形成されている。図3において表印刷層23が形成されている領域を多数のドットを付して示している。このように、表印刷層23は、軸線方向の一端部である下端部2aから他端部である上端部2bまで全領域に亘って形成されているのではなく、下端部2aに所定幅に亘って形成された下側印刷領域23aと、軸線方向の他端部である上端部2bを含めて表面の大部分の領域を占める上側印刷領域23bとから構成されており、下側印刷領域23aの隣、即ち下側印刷領域23aの上側には所定幅に亘って印刷されていない未印刷領域24が形成されている。尚、未印刷領域24は下側印刷領域23aよりも幅広に形成されている。該表印刷層23は、図4に示すように、文字や図柄等のデザイン層40と、該デザイン層40を保護するための透明なニス層41とから構成されている。表印刷層23は、基材フィルム21の表面に印刷により形成されたものであるが、基材フィルム21の表面にデザイン層40が形成され、続いてその上にオーバーコート層としてニス層41が形成される。ニス層41はデザイン層40を覆うようにそれよりも大きい面積で形成されているため、上側印刷領域23bの下端はニス層41から構成される。また、下側印刷領域23aにはデザイン層40が存在せずニス層41のみからなる。但し、後述するように製造工程のバラツキから下側印刷領域23aの下端にもデザイン層40が存在する場合もある。また、デザインの配置の関係上、デザイン層40の大きさや配置は種々変化する。   A front printed layer 23 is formed on the surface of the shrink label 2. In FIG. 3, a region where the front print layer 23 is formed is shown with a number of dots. Thus, the front print layer 23 is not formed over the entire region from the lower end 2a, which is one end in the axial direction, to the upper end 2b, which is the other end, but has a predetermined width at the lower end 2a. A lower printing area 23a that occupies most of the surface area including the upper end 2b, which is the other end in the axial direction, and the lower printing area 23a. An unprinted area 24 that is not printed over a predetermined width is formed next to the upper print area 23a. The unprinted area 24 is formed wider than the lower print area 23a. As shown in FIG. 4, the front print layer 23 includes a design layer 40 such as characters and designs, and a transparent varnish layer 41 for protecting the design layer 40. The front print layer 23 is formed by printing on the surface of the base film 21, but the design layer 40 is formed on the surface of the base film 21, and then the varnish layer 41 is formed thereon as an overcoat layer. It is formed. Since the varnish layer 41 is formed with a larger area so as to cover the design layer 40, the lower end of the upper printing region 23 b is constituted by the varnish layer 41. Further, the design layer 40 does not exist in the lower printing area 23a, and only the varnish layer 41 is formed. However, as will be described later, the design layer 40 may also exist at the lower end of the lower printing area 23a due to variations in the manufacturing process. In addition, the size and arrangement of the design layer 40 are variously changed due to the arrangement of the design.

また、シュリンクラベル2は遮光性を有しており、そのためシュリンクラベル2の裏面には遮光層25が形成されている。図3において遮光層25が形成されている領域にはクロスハッチングを施して示している。遮光層25は図3及び図4のように、上端部2bと下端部2aを除く全領域に形成されている。即ち、シュリンクラベル2の裏面の上端部2bと下端部2aにはそれぞれ遮光層25が形成されていない未遮光領域26が存在している。下側の未遮光領域26は、下側印刷領域23aよりも幅広であり、従って、遮光層25は下側印刷領域23aよりも上側に位置している。   Further, the shrink label 2 has a light shielding property, and therefore, a light shielding layer 25 is formed on the back surface of the shrink label 2. In FIG. 3, the region where the light shielding layer 25 is formed is shown with cross-hatching. As shown in FIGS. 3 and 4, the light shielding layer 25 is formed in the entire region except the upper end 2b and the lower end 2a. That is, the non-light-shielding area | region 26 in which the light shielding layer 25 is not formed exists in the upper end part 2b and the lower end part 2a of the back surface of the shrink label 2, respectively. The lower unshielded area 26 is wider than the lower print area 23a. Therefore, the light shielding layer 25 is located above the lower print area 23a.

ここで、基材フィルム21には、ポリエステル系のフィルムやポリスチレン系のフィルム、ポリオレフィン系のフィルム等、各種の熱収縮性フィルムが使用でき、単層のものの他、多層のものであってよい。紫外線透過を抑制する観点から乳白PETフィルムを使用することも好ましい。表印刷層23は例えばグラビア印刷によって形成され、デザイン層40には、好ましくはアクリル系のインキが使用されるが、ウレタン系のもの等、各種のグラビアインキが使用できる。また、インキには顔料が含まれていても含まれていなくてもよく、また、UV硬化型のインキでもよい。同様にニス層41もUV硬化型のニスであってよい。遮光層25も例えばグラビア印刷によって形成される。遮光層25は一層構造よりも多層構造が好ましく、例えば、カーボンブラック等の黒色顔料が配合された黒色インキからなる一層あるいは二層以上の黒色層と、二酸化チタン等の白色顔料が配合された白色インキからなる一層あるいは二層以上の白色層とから構成される。   Here, as the base film 21, various heat-shrinkable films such as a polyester film, a polystyrene film, and a polyolefin film can be used, and a single film or a multilayer film may be used. It is also preferable to use a milk white PET film from the viewpoint of suppressing ultraviolet light transmission. The surface printing layer 23 is formed by, for example, gravure printing, and acrylic ink is preferably used for the design layer 40, but various gravure inks such as urethane-based ones can be used. The ink may or may not contain a pigment, and may be a UV curable ink. Similarly, the varnish layer 41 may be a UV curable varnish. The light shielding layer 25 is also formed by, for example, gravure printing. The light-shielding layer 25 preferably has a multilayer structure rather than a single-layer structure. For example, one or two or more black layers composed of a black ink blended with a black pigment such as carbon black and a white blend composed of a white pigment such as titanium dioxide. It is composed of a single layer of ink or two or more white layers.

かかる筒状のシュリンクラベル2は、短手方向を主延伸方向とする長尺フィルムの両側部同士を貼り合わせて長尺筒状ラベルを形成し、それをロール状に巻回したものを順次繰り出しながら所定長さ毎に切断することにより形成される。長尺筒状ラベル50の要部断面を図5に示しているが、図中の一点鎖線で示している位置が設計上の切断位置51である。該設計上の切断位置51に対して実際の切断位置はフィルム送り方向53の前後に位置ずれする可能性があるが、そのバラツキの範囲が符号52で示している範囲である。設計上の切断位置51の図中右側はシュリンクラベル2の下端部2aであり、図中左側は次のシュリンクラベル2の上端部2bである。仮に実際の切断位置が図中向かって右側にずれたとしても、シュリンクラベル2の下端部2aの表面には表印刷層23(下側印刷領域23a)が存在し、その裏面には遮光層25のない未遮光領域26が形成されることになる。実際の切断位置が逆に図中向かって左側にずれたとしても、シュリンクラベル2の下端部2aの表面には表印刷層23(下側印刷領域23a)が存在し、この場合、下側印刷領域23aにもデザイン層40が形成されることになり、また、その裏面には遮光層25のない未遮光領域26が形成される。このように長尺筒状ラベル50における表印刷層23を分断すると共に未遮光領域26を分断する位置を設計上の切断位置51とすることにより、実際の切断位置がフィルム送り方向53の前後にばらついたとしても、シュリンクラベル2の下端部2aの表面には表印刷層23(下側印刷領域23a)が形成され且つ裏面には未遮光領域26が形成されることになる。長尺筒状ラベル50における未遮光領域26を分断する位置を切断位置51とするので、図4のように、シュリンクラベル2の上端部2bの裏面にも未遮光領域26が形成される。   The cylindrical shrink label 2 is formed by laminating both sides of a long film whose main direction is the short direction to form a long cylindrical label, which is rolled out in a roll. However, it is formed by cutting every predetermined length. Although a cross section of the main part of the long cylindrical label 50 is shown in FIG. 5, the position indicated by the alternate long and short dash line in the figure is the designed cutting position 51. The actual cutting position may be displaced before and after the film cutting direction 53 with respect to the designed cutting position 51, but the range of variation is the range indicated by reference numeral 52. The right side of the design cutting position 51 in the figure is the lower end 2a of the shrink label 2, and the left side in the figure is the upper end 2b of the next shrink label 2. Even if the actual cutting position is shifted to the right side in the drawing, the front printing layer 23 (lower printing region 23a) exists on the surface of the lower end 2a of the shrink label 2, and the light shielding layer 25 is provided on the back surface thereof. An unshielded area 26 having no light is formed. Even if the actual cutting position is shifted to the left side in the figure, the front printing layer 23 (lower printing area 23a) exists on the surface of the lower end 2a of the shrink label 2, and in this case, the lower printing is performed. The design layer 40 is also formed in the region 23a, and an unshielded region 26 without the light shielding layer 25 is formed on the back surface thereof. Thus, by setting the position where the front printed layer 23 in the long cylindrical label 50 is divided and the unshielded area 26 is divided as the designed cutting position 51, the actual cutting position is before and after the film feed direction 53. Even if there is a variation, the front print layer 23 (lower print area 23a) is formed on the surface of the lower end 2a of the shrink label 2, and the unshielded area 26 is formed on the back surface. Since the position where the unshielded area 26 in the long cylindrical label 50 is divided is the cutting position 51, the unshielded area 26 is also formed on the back surface of the upper end portion 2b of the shrink label 2 as shown in FIG.

このようにして形成された筒状のシュリンクラベル2が容器1に装着されているのであるが、図2に拡大図を示しているように、シュリンクラベル2の下部は容器1の胴部10から底部11に回り込んでいる。シュリンクラベル2の裏面の遮光層25は胴部10から底部11にまで達しており、また、シュリンクラベル2の表面の未印刷領域24は容器1の底部11の下側に位置している。そして、容器1の底部11の下側には、シュリンクラベル2の下端部2aから形成された環状の貼り付け支持面が凹部空間14内に収容されるように位置している。該環状の貼り付け支持面は略フラットであって、しかも、凹部壁面12aから下方に離間した状態にある。該環状の貼り付け支持面にタックラベル3の周縁部が貼着されて、シュリンクラベル2の下端開口部20がタックラベル3によって閉塞されている。従って、容器1の底部11はシュリンクラベル2とタックラベル3によって完全に覆われた状態にある。   The cylindrical shrink label 2 formed in this way is attached to the container 1, but as shown in an enlarged view in FIG. 2, the lower part of the shrink label 2 extends from the body 10 of the container 1. It wraps around the bottom 11. The light shielding layer 25 on the back surface of the shrink label 2 extends from the body portion 10 to the bottom portion 11, and the unprinted area 24 on the surface of the shrink label 2 is located below the bottom portion 11 of the container 1. And the annular sticking | supporting support surface formed from the lower end part 2a of the shrink label 2 is located in the recessed part space 14 below the bottom part 11 of the container 1. As shown in FIG. The annular sticking support surface is substantially flat and is spaced downward from the recess wall surface 12a. The peripheral edge of the tack label 3 is stuck to the annular sticking support surface, and the lower end opening 20 of the shrink label 2 is closed by the tack label 3. Therefore, the bottom 11 of the container 1 is completely covered with the shrink label 2 and the tack label 3.

該タックラベル3も遮光性を有している。具体的には、タックラベル3は、PETフィルム等からなる透明なラベル基材30の片面に金属蒸着層(図示省略)が形成され、該金属蒸着層の上に粘着剤層31が形成された層構造を有するものであって、金属蒸着層によって遮光性が確保されている。かかるタックラベル3の周縁部がシュリンクラベル2に貼着されているのであるが、容器1の底部11の下側にシュリンクラベル2の未印刷領域24が位置しているため、その未印刷領域24にタックラベル3の周縁部が貼着されている。また、シュリンクラベル2の裏面の遮光層25に対してタックラベル3がオーバーラップするように貼着されており、シュリンクラベル2の下端部2aの未遮光領域26の外側にはタックラベル3がそれを覆うように位置している。従って、シュリンクラベル2の遮光層25とタックラベル3の遮光層である金属蒸着層とによって容器1の底部11は全体に亘って遮光され、この底被覆容器は、底部11まで遮光性を持った遮光容器となる。   The tack label 3 also has a light shielding property. Specifically, in the tack label 3, a metal vapor deposition layer (not shown) is formed on one side of a transparent label substrate 30 made of a PET film or the like, and an adhesive layer 31 is formed on the metal vapor deposition layer. It has a layer structure, and the light shielding property is ensured by the metal vapor deposition layer. The peripheral portion of the tack label 3 is attached to the shrink label 2. Since the unprinted region 24 of the shrink label 2 is located below the bottom 11 of the container 1, the unprinted region 24. The peripheral part of the tack label 3 is stuck to. Further, the tack label 3 is attached so as to overlap the light shielding layer 25 on the back surface of the shrink label 2, and the tack label 3 is attached to the outside of the unshielded area 26 at the lower end 2 a of the shrink label 2. It is located so as to cover. Accordingly, the bottom portion 11 of the container 1 is shielded from light by the light shielding layer 25 of the shrink label 2 and the metal vapor deposition layer as the light shielding layer of the tack label 3, and this bottom coating container has light shielding properties up to the bottom portion 11. It becomes a shading container.

以上のような構成の底被覆容器は、上述した長尺筒状ラベル50から切断されて形成された筒状のシュリンクラベル2を図6に二点鎖線にて示しているように容器1に被せた後、シュリンクラベル2の下部を容器1の胴部10から底部11に回り込ませる収縮工程と、容器1の底部11に回り込んだシュリンクラベル2の下端部2aを容器1の底部11の凹部空間14内に押し込む押し込み工程と、タックラベル3をシュリンクラベル2の下端部2aに押し付けて貼着する貼着工程を経て製造される。   The bottom-coated container having the above-described structure covers the container 1 as shown by a two-dot chain line in FIG. 6 with the cylindrical shrink label 2 cut from the long cylindrical label 50 described above. After that, the shrinking process of lowering the lower part of the shrink label 2 from the body part 10 of the container 1 to the bottom part 11, and the lower end part 2 a of the shrink label 2 wrapping around the bottom part 11 of the container 1 as the recessed space of the bottom part 11 of the container 1. 14 is manufactured through a pressing process of pressing into 14 and a sticking process of pressing the tack label 3 against the lower end 2a of the shrink label 2 and sticking.

図6の二点鎖線のような容器1への被嵌状態において、シュリンクラベル2の図示しない上端部2bは容器1の胴部10を上側に越えて肩部あるいは口部近傍にまで達しており、シュリンクラベル2の下部は容器1の底部11よりも下方に所定長さ伸びている。そして、シュリンクトンネル等でシュリンクラベル2を収縮させて容器1にシュリンクラベル2を密着させるのであるが(収縮工程)、シュリンクラベル2が収縮することによって図6に実線で示しているようにシュリンクラベル2の下部は容器1の底部11の下側に回り込んだ状態となる。かかる収縮状態においてシュリンクラベル2の下部は、容器1の底部10の載置部13で中心側に向けて折れ曲がって載置部13から容器1の中心に向けて略水平に延びた状態となっている。   6, the upper end portion 2b (not shown) of the shrink label 2 extends over the body portion 10 of the container 1 and reaches the shoulder portion or the vicinity of the mouth portion. The lower portion of the shrink label 2 extends a predetermined length below the bottom 11 of the container 1. Then, the shrink label 2 is shrunk by a shrink tunnel or the like to bring the shrink label 2 into close contact with the container 1 (shrinking step). As the shrink label 2 shrinks, the shrink label as shown by a solid line in FIG. The lower part of 2 is in a state of wrapping around below the bottom 11 of the container 1. In such a contracted state, the lower portion of the shrink label 2 is bent toward the center side at the placement portion 13 of the bottom portion 10 of the container 1 and extends substantially horizontally from the placement portion 13 toward the center of the container 1. Yes.

尚、シュリンクラベル2の下端部2aの表面には収縮抑制用被覆層として表印刷層23の下側印刷領域23aが形成されているので、該下端部2aにおいては表面側の収縮が抑制される結果、シュリンクラベル2の下端部2aは表面側即ち下側には反り返ることがなく、図6に示すようにフラットな状態、あるいは、裏面側に若干反った状態となる。特に、シュリンクラベル2の下端部2aの裏面に遮光層25が形成されずに未遮光領域26が存在しているので、表面側への反り返りが確実に防止される。そして、収縮状態においてシュリンクラベル2の下端部2aに表面側への反り返りが生じていないために、次のタックラベル3の貼着工程がスムーズなものとなり、タックラベル3を容易にしかも確実に貼着することができる。   In addition, since the lower printing area 23a of the surface printing layer 23 is formed as a shrinkage-suppressing coating layer on the surface of the lower end 2a of the shrink label 2, the shrinkage on the surface side is suppressed at the lower end 2a. As a result, the lower end portion 2a of the shrink label 2 does not warp to the front side, that is, the lower side, and is in a flat state as shown in FIG. In particular, since the light shielding layer 25 is not formed on the back surface of the lower end portion 2a of the shrink label 2 and the non-light shielding region 26 exists, the warping to the front surface side is reliably prevented. In the contracted state, the lower end portion 2a of the shrink label 2 does not warp to the surface side, so the sticking process of the next tack label 3 becomes smooth, and the tack label 3 is easily and securely attached. Can be worn.

即ち、上記収縮工程の後、図7及び図8のようにタックラベル3を載せた押し込み治具70を使用して押し込み工程と貼着工程とを同時に行う。該押し込み治具70は、上面が凹んだ全体としてカップ状のものであり、その周壁部71の内周面71aはテーパ状に形成され、底部内面72の周縁部に容器1の底部11の載置部13が位置するように構成されている。周壁部71のテーパ状の内周面71aによって押し込み治具70に対する容器1の水平方向の位置決めがなされる。また、底部内面72の中央部には周縁部に対して一段高くなった突部73が形成され、該突部73の上面にタックラベル3が載置される。尚、突部73の上面に吸引孔を形成してタックラベル3を吸引保持するようにすることも好ましい。尚、突部73の上面は平坦面に形成されている。   That is, after the shrinking step, the pushing step and the sticking step are simultaneously performed using the pushing jig 70 on which the tack label 3 is placed as shown in FIGS. The pushing jig 70 is cup-shaped as a whole with a concave upper surface, and the inner peripheral surface 71a of the peripheral wall portion 71 is formed in a taper shape, and the bottom portion 11 of the container 1 is placed on the peripheral portion of the bottom inner surface 72. It is comprised so that the mounting part 13 may be located. The container 1 is positioned in the horizontal direction with respect to the pushing jig 70 by the tapered inner peripheral surface 71 a of the peripheral wall portion 71. Further, a protrusion 73 that is one step higher than the peripheral edge is formed at the center of the bottom inner surface 72, and the tack label 3 is placed on the upper surface of the protrusion 73. It is also preferable to form a suction hole on the upper surface of the protrusion 73 so as to suck and hold the tack label 3. In addition, the upper surface of the protrusion 73 is formed in a flat surface.

このような押し込み治具70を容器1の下側に配置して、押し込み治具70を容器1に向けて相対的に上昇接近させる。容器1の高さを固定して押し込み治具70を上昇させてもよいし、逆に押し込み治具70の高さを固定しておいて容器1を下降させてもよいし、あるいは、容器1を下降させつつ押し込み治具70を上昇させてもよい。何れにしても容器1の底部11に向けて押し込み治具70を接近させていき、突部73の上面に載置されたタックラベル3でシュリンクラベル2の下端部2aを凹部空間14内に押し込んでいく。その際、周囲の雰囲気温度をシュリンクラベル2が軟化する程度の温度に高く設定しておいて押し込み治具70でシュリンクラベル2の下端部2aを押し込む際にシュリンクラベル2が押し込み治具70で成形できるようにしておく。あるいは、周囲の雰囲気温度を上げておくのではなく、押し込み治具70の特にその突部73を加熱しておいて押し込み治具70でシュリンクラベル2の下端部2aを加熱しつつ押し上げて変形させるようにしてもよく、また、その両方を併用してもよい。   Such a pushing jig 70 is arranged on the lower side of the container 1, and the pushing jig 70 is relatively moved upward and close toward the container 1. The height of the container 1 may be fixed and the pushing jig 70 may be raised. Conversely, the height of the pushing jig 70 may be fixed and the container 1 may be lowered, or the container 1 The pushing jig 70 may be raised while lowering. In any case, the pushing jig 70 is approached toward the bottom 11 of the container 1, and the lower end 2 a of the shrink label 2 is pushed into the recessed space 14 with the tack label 3 placed on the upper surface of the protrusion 73. Go. At that time, the ambient temperature is set high enough to soften the shrink label 2, and when the lower end 2 a of the shrink label 2 is pushed by the pushing jig 70, the shrink label 2 is formed by the pushing jig 70. Keep it available. Alternatively, the ambient temperature is not raised, but the protrusion 73 of the pushing jig 70, in particular, its projection 73 is heated, and the lower end 2a of the shrink label 2 is pushed up and deformed by the pushing jig 70. You may make it, and you may use both together.

タックラベル3を載置した押し込み治具70でシュリンクラベル2の下端部2aを上側に押し上げていくことで、シュリンクラベル2の下端部2aは凹部空間14内に位置することとなりその下端部2aから略フラットな環状の貼り付け支持面が形成され、それと同時に貼り付け支持面にタックラベル3の周縁部が貼着されることとなる。貼り付け支持面は凹部壁面12aから下側に離間している状態であるが、シュリンクラベル2の下端部2aが押し上げられる際に下側への反力を発生させるので、その下側への反力によってタックラベル3を貼り付け支持面に貼着することができる。また、シュリンクラベル2の下端部2aに表面側への反り返りが生じていないため、タックラベル3を容易に貼着することができ、接着力も確保される。更に、シュリンクラベル2の表面の下側印刷領域23aの隣に未印刷領域24が形成されていてその未印刷領域24にタックラベル3の周縁部を貼着できるので、表印刷層23にタックラベル3の周縁部を貼着する場合に比して大きな接着力が得られる。   By pushing up the lower end portion 2a of the shrink label 2 with the pushing jig 70 on which the tack label 3 is placed, the lower end portion 2a of the shrink label 2 is positioned in the recess space 14, and from the lower end portion 2a. A substantially flat annular sticking support surface is formed, and at the same time, the peripheral edge of the tack label 3 is stuck on the sticking support surface. The affixing support surface is in a state of being spaced downward from the concave wall surface 12a. However, when the lower end portion 2a of the shrink label 2 is pushed up, a downward reaction force is generated. The tack label 3 can be attached to the supporting surface by force. Moreover, since the lower end part 2a of the shrink label 2 is not warped to the surface side, the tack label 3 can be easily attached and an adhesive force is also ensured. Further, an unprinted area 24 is formed next to the lower print area 23 a on the surface of the shrink label 2, and the peripheral portion of the tack label 3 can be adhered to the unprinted area 24. Compared with the case where 3 peripheral parts are stuck, a big adhesive force is obtained.

以上のようにして製造された底被覆容器は、その後、搬送ベルトに載置されて製造ラインを搬送されたり、あるいは、流通過程において輸送されることになるが、タックラベル3が凹部空間14内に収容された状態にあって下方に突出していないので、搬送中等においてタックラベル3の周縁部が他の物にひっかかって剥がれたりするということがない。特に、載置面Pからタックラベル3が上方に離間しているので、タックラベル3の下面が擦れて汚れたり傷ついたりするということも防止できる。しかも、シュリンクラベル2の下端部2aは収縮量が大きい箇所であってシュリンクラベル2の他の部分よりも固い状態となっているので、輸送中にシュリンクラベル2の下端部2aがタックラベル3と共に垂れ下がってくるということもなく、タックラベル3は凹部空間14内に確実に保持される。   The bottom coating container manufactured as described above is then placed on a transport belt and transported on the manufacturing line or transported in the distribution process. Since it is housed in the container and does not protrude downward, the peripheral edge of the tack label 3 does not get caught by other objects during transportation or the like. In particular, since the tack label 3 is spaced upward from the placement surface P, it is possible to prevent the lower surface of the tack label 3 from being rubbed and dirty or damaged. Moreover, since the lower end 2a of the shrink label 2 is a portion where the amount of contraction is large and is in a harder state than the other portions of the shrink label 2, the lower end 2a of the shrink label 2 together with the tack label 3 during transportation. The tack label 3 is securely held in the recessed space 14 without being hung down.

尚、上記実施形態では、押し込み工程と貼着工程とを同時に行ったが、別々に行ってもよい。その場合には、押し込み治具70の突部73の突出量を図7で示したものよりも大きくしておく。そして、押し込み治具70でシュリンクラベル2の下端部2aを押し上げて環状の貼り付け支持面を形成するが、その後、周囲の雰囲気温度を低下させるなどすることによって貼り付け支持面を固化させ、該固化した貼り付け支持面にタックラベル3を貼着させる。   In addition, in the said embodiment, although the pushing process and the sticking process were performed simultaneously, you may perform separately. In that case, the protrusion amount of the protrusion 73 of the pushing jig 70 is set larger than that shown in FIG. Then, the lower end portion 2a of the shrink label 2 is pushed up by the pushing jig 70 to form an annular sticking support surface. Thereafter, the sticking support surface is solidified by lowering the ambient temperature, etc. The tack label 3 is stuck on the solidified sticking support surface.

また、図7では押し込み治具70の突部73の上面を平坦面としたが、図9のように上側凸の曲面を有する突部73としてもよい。この場合には、環状の貼り付け支持面は略フラットではなく突部73の湾曲形状に沿った形状となり、タックラベル3も上側凸に湾曲した状態で貼着されることになる。外観体裁上は平坦面を有する突部73でタックラベル3を貼着することが好ましいが、逆に上側凸の曲面を有する突部73でタックラベル3を貼着すると、より一層強固に貼着することができるというメリットがある。従って、用途に応じて使い分けるとよい。また、この場合も上述したのと同様に貼着工程を押し込み工程とは別に行ってもよい。   In FIG. 7, the upper surface of the protrusion 73 of the pushing jig 70 is a flat surface. However, as shown in FIG. 9, the protrusion 73 may have an upward convex curved surface. In this case, the annular sticking support surface is not substantially flat but has a shape along the curved shape of the protrusion 73, and the tack label 3 is also stuck in a state of being curved upward. In terms of appearance, it is preferable to stick the tack label 3 with the protrusion 73 having a flat surface, but conversely, if the tack label 3 is attached with the protrusion 73 having an upwardly convex curved surface, the tack label 3 is more firmly attached. There is a merit that you can. Therefore, it is good to use properly according to the application. Also in this case, the sticking process may be performed separately from the pushing process, as described above.

また、タックラベル3を載置面Pから上方に離間させていたが、タックラベル3が載置面Pと面一に貼着されていてもよい。   Further, although the tack label 3 is separated upward from the placement surface P, the tack label 3 may be adhered flush with the placement surface P.

更に、シュリンクラベル2とタックラベル3が遮光性を有する場合について説明したが、遮光性を有しないものであってもよい。   Furthermore, although the case where the shrink label 2 and the tack label 3 have light shielding properties has been described, they may not have light shielding properties.

また、表印刷層23がニス層41を有するものであったが、ニス層41がないものであってもよく、収縮抑制用被覆層としての下側印刷領域23aがニス層41ではなくデザイン層40即ちインキ層から構成されていても構わない。また、収縮抑制用被覆層を印刷によって形成するのではなく、インキ等の塗布により形成してもよい。   Moreover, although the surface printing layer 23 has the varnish layer 41, the varnish layer 41 may not be provided, and the lower printing region 23a as the shrinkage suppression coating layer is not the varnish layer 41 but the design layer. 40, that is, an ink layer. Further, the shrinkage-suppressing coating layer may be formed not by printing but by application of ink or the like.

更に、シュリンクラベル2の下端部2aの表面に収縮抑制用被覆層を形成することが好ましいが、それを省略しても構わない。   Furthermore, although it is preferable to form a shrinkage-suppressing coating layer on the surface of the lower end 2a of the shrink label 2, it may be omitted.

また、上述の説明では、長尺筒状ラベル50から形成した筒状のシュリンクラベル2を使用する場合について説明したが、シュリンクラベル2は、容器1への装着前に予め筒状とされているものには限られない。矩形即ち枚葉型であって容器1への装着に際して筒状とされる構成であってもよい。即ち、容器1に巻き付けつつ主延伸方向の両端部同士を重ね合わせて筒状とする構成や、容器1に被嵌する直前に一旦ドラムに巻き付けつつ主延伸方向の両端部同士を重ね合わせて筒状とし、その後に容器1に被嵌する構成であってもよい。   In the above description, the case where the cylindrical shrink label 2 formed from the long cylindrical label 50 is used has been described. However, the shrink label 2 is formed into a cylindrical shape before being attached to the container 1. It is not limited to things. A rectangular shape, that is, a single-wafer type, may be configured to be cylindrical when mounted on the container 1. That is, a structure in which both ends in the main stretching direction are overlapped with each other while being wound around the container 1 to form a cylinder, or both ends in the main stretching direction are overlapped with each other in the main stretching direction once before being fitted on the container 1 It may be configured to be in a shape and then fitted into the container 1.

1 容器
2 シュリンクラベル
2a 下端部
2b 上端部
3 タックラベル
10 胴部
11 底部
12 凹部
12a 凹部壁面
13 載置部
14 凹部空間
20 下端開口部
21 基材フィルム
22 重ね合わせ部
23 表印刷層
23a 下側印刷領域
23b 上側印刷領域
24 未印刷領域
25 遮光層
26 未遮光領域
30 ラベル基材
31 粘着剤層
40 デザイン層
41 ニス層
50 長尺筒状ラベル
51 設計上の切断位置
52 切断位置のバラツキ範囲
53 フィルム送り方向
70 押し込み治具
71 周壁部
71a 内周面
72 底部内面
73 突部
P 載置面
DESCRIPTION OF SYMBOLS 1 Container 2 Shrink label 2a Lower end part 2b Upper end part 3 Tack label 10 trunk | drum 11 Bottom part 12 Recessed part 12a Recessed wall surface 13 Mounting part 14 Recessed space 20 Lower end opening part 21 Base film 22 Overlapping part 23 Front printing layer 23a Lower side Print area 23b Upper print area 24 Unprinted area 25 Light-shielding layer 26 Non-light-shielded area 30 Label base material 31 Adhesive layer 40 Design layer 41 Varnish layer 50 Long cylindrical label 51 Designed cutting position 52 Cutting position variation range 53 Film feeding direction 70 Pushing jig 71 Peripheral wall 71a Inner peripheral surface 72 Bottom inner surface 73 Protrusion P Placement surface

Claims (5)

筒状のシュリンクベルの下部が容器の胴部から底部に回り込んでいて該シュリンクラベルの下端開口部を閉塞すべくタックラベルがシュリンクラベルに貼着されている底被覆容器であって、
容器の底部には載置部よりも上方に凹んだ凹部が形成され、シュリンクラベルの下端部は容器の底部の凹部空間内に位置すると共に該凹部壁面から下方に離間した状態で環状の貼り付け支持面を形成し、該貼り付け支持面にタックラベルが下側から貼着されて凹部空間内に収容されていることを特徴とする底被覆容器。
A bottom-coated container in which the lower part of the cylindrical shrink bell goes around from the body part of the container to the bottom and the tack label is attached to the shrink label so as to close the lower end opening of the shrink label,
The bottom of the container is formed with a recess recessed upward from the mounting portion, and the lower end of the shrink label is positioned in the recess space of the bottom of the container and is attached in an annular shape while being spaced downward from the wall of the recess A bottom coating container, wherein a support surface is formed, and a tack label is attached to the attachment support surface from below and is accommodated in a recessed space.
タックラベルが底被覆容器の載置面よりも上方に離間して位置している請求項1記載の底被覆容器。   The bottom covering container according to claim 1, wherein the tack label is positioned above and spaced from the mounting surface of the bottom covering container. シュリンクラベルとタックラベルが遮光性を有している請求項1又は2記載の底被覆容器。   The bottom coating container according to claim 1 or 2, wherein the shrink label and the tack label have light shielding properties. 請求項1乃至3の何れかに記載の底被覆容器の製造方法であって、
筒状のシュリンクラベルを熱収縮させて該シュリンクラベルの下部を容器の胴部から容器の底部に回り込ませる収縮工程と、容器の底部に回り込んだシュリンクラベルの下端部を容器の底部の凹部空間内に押し込む押し込み工程と、タックラベルをシュリンクラベルの下端部に押し付けて貼着する貼着工程とを備えることを特徴とする底被覆容器の製造方法。
A method for manufacturing a bottom-coated container according to any one of claims 1 to 3,
A shrinking process in which a cylindrical shrink label is thermally shrunk so that a lower part of the shrink label is drawn from the body part of the container to the bottom part of the container, and a lower end part of the shrink label that has turned around the bottom part of the container is a recessed space in the bottom part of the container. The manufacturing method of the bottom coating container characterized by including the pressing process pushed in, and the sticking process which presses and sticks a tack label to the lower end part of a shrink label.
押し込み工程と貼着工程を同時に行う請求項4記載の底被覆容器の製造方法。   The manufacturing method of the bottom coating container of Claim 4 which performs a pushing process and a sticking process simultaneously.
JP2012070424A 2012-03-26 2012-03-26 Bottom coated container and method for manufacturing the same Pending JP2013199318A (en)