JP2013025297A - Method of producing member for liquid crystal display panel, and member for liquid crystal display panel - Google Patents
Method of producing member for liquid crystal display panel, and member for liquid crystal display panel Download PDFInfo
- Publication number
- JP2013025297A JP2013025297A JP2011163219A JP2011163219A JP2013025297A JP 2013025297 A JP2013025297 A JP 2013025297A JP 2011163219 A JP2011163219 A JP 2011163219A JP 2011163219 A JP2011163219 A JP 2011163219A JP 2013025297 A JP2013025297 A JP 2013025297A
- Authority
- JP
- Japan
- Prior art keywords
- display panel
- liquid crystal
- crystal display
- outer frame
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
本発明は携帯電話、高度情報端末、カーナビゲーション、電子書籍タブレット等に用いられる液晶表示パネル用部材の作成方法及び液晶表示パネル用部材において、液晶表示パネルの中央部の表示部の外側の外枠を作成する方法及び部材に関するものである。 The present invention relates to a method for producing a liquid crystal display panel member used for a mobile phone, an advanced information terminal, a car navigation, an electronic book tablet, and the like, and a liquid crystal display panel member. The present invention relates to a method and a member for creating a device.
図1は携帯電話の表示部の一例を示したものである。図1(a)に示される携帯電話の表示パネル100は、表示部である内枠部1と、表示部の外側の外枠部2とで構成されている。また、図1(b)に示される携帯電話の表示パネル101の外枠部には例えば携帯電話会社を表すミラー文字3が施されている場合もある。 FIG. 1 shows an example of a display unit of a mobile phone. A display panel 100 of a mobile phone shown in FIG. 1A includes an inner frame portion 1 that is a display portion, and an outer frame portion 2 outside the display portion. Further, the outer frame portion of the display panel 101 of the mobile phone shown in FIG. 1B may be provided with a mirror character 3 representing a mobile phone company, for example.
表示パネルの基本的構成について図面により説明する。図2(a)は上記携帯電話の表示パネル100の断面の一部を模式的に示す図で、図2(b)は上記携帯電話の表示パネル101の断面の一部を模式的に示す図である。 A basic configuration of the display panel will be described with reference to the drawings. 2A is a diagram schematically showing a part of the cross section of the display panel 100 of the mobile phone, and FIG. 2B is a diagram schematically showing a part of the cross section of the display panel 101 of the mobile phone. It is.
図2(a)に示される表示パネル100は、表示パネル基材4の裏面にインキ層6と接着層7が、また表面にはハードコート層8が設けられており、最上面には保護フィルム9が貼られている。 The display panel 100 shown in FIG. 2A is provided with an ink layer 6 and an adhesive layer 7 on the back surface of the display panel substrate 4, and a hard coat layer 8 on the surface, and a protective film on the top surface. 9 is affixed.
図2(b)に示される表示パネル101は、表示パネル基材4の裏面にはミラー文字を施したミラー印刷層5と、インキ層6と、接着層7とが、また表面にはハードコート層8が設けられており、最上面には保護フィルム9が貼られている。 The display panel 101 shown in FIG. 2B has a mirror printing layer 5 with a mirror character on the back surface of the display panel substrate 4, an ink layer 6, and an adhesive layer 7, and a hard coat on the surface. The layer 8 is provided and the protective film 9 is stuck on the uppermost surface.
表示パネル基材4として、ガラスシート、PMMA(ポリメタクリル酸メチル樹脂)シート、PC(ポリカーボネート)シート等のいずれかが用いられる。 As the display panel substrate 4, any one of a glass sheet, a PMMA (polymethyl methacrylate resin) sheet, a PC (polycarbonate) sheet, and the like is used.
ミラー印刷層5、インキ層6は一般的にはシルクスクリーン印刷によって形成されている。このインキ層6は表示パネルの意匠性を持たせるために隠蔽性や美粧性を有した層となっている。 The mirror printing layer 5 and the ink layer 6 are generally formed by silk screen printing. The ink layer 6 is a layer having a concealing property and a cosmetic property in order to give the design properties of the display panel.
図2に示される従来用いられている表示パネルでは、ミラー印刷層5は5〜7μmで、インキ層6は隠蔽性を確保するためにスクリーン印刷を数回まで重ねて加飾印刷する場合が多く、数μm〜25μm程度にまで厚くなる。 In the conventionally used display panel shown in FIG. 2, the mirror printing layer 5 is 5 to 7 μm, and the ink layer 6 is often subjected to decorative printing by repeating screen printing several times to ensure concealment. The thickness is increased to about several μm to 25 μm.
そのため、表示部である内枠部1(以下、表示部)と、表示部の外側の外枠部2と段差は、図2(a)で示すミラー印刷層5のない表示パネルの場合は数μm〜25μmとなり、図2(b)で示すミラー印刷層5を有する表示パネルの場合は10〜30μm程度にまでなり、図3に示すように接着層7(層厚:数μm程度)を塗布しても、段差は埋めきれず(図3(a))、更にその下部にタッチパネル電極層10やRGB表示層11を設ける場合や(図3(b))や、タッチパネル機能のない表示パネルの場合にはRGB表示層11を設けるが(図3(c))、この場合に段差が原因となって表示部に気泡を抱き込んでしまい、不良品が発生してしまう問題がある。 Therefore, the inner frame portion 1 (hereinafter referred to as the display portion) which is the display portion and the outer frame portion 2 outside the display portion and the steps are several in the case of the display panel without the mirror print layer 5 shown in FIG. In the case of a display panel having the mirror printing layer 5 shown in FIG. 2B, the thickness is about 10 to 30 μm, and an adhesive layer 7 (layer thickness: about several μm) is applied as shown in FIG. However, the step cannot be filled (FIG. 3 (a)), and the touch panel electrode layer 10 and the RGB display layer 11 are provided in the lower part (FIG. 3 (b)), or the display panel having no touch panel function. In this case, the RGB display layer 11 is provided (FIG. 3 (c)). In this case, there is a problem that air bubbles are embraced in the display portion due to a step and a defective product is generated.
そこで本発明では、表示部の外側の外枠部2を表示部1と段差のない方法で形成した液晶表示パネル用部材の作成方法及び液晶表示パネル用部材を提供することを目的とする。 Accordingly, an object of the present invention is to provide a method for producing a liquid crystal display panel member and a liquid crystal display panel member in which the outer frame portion 2 outside the display portion is formed by a method having no step difference from the display portion 1.
そこで本発明の請求項1に係る発明は、液晶表示パネルに用いられる部材の作成方法において、
表示パネルの中央部の表示部の外側に設ける外枠部を作成する方法であって、
表示パネル基材の裏面に、表示部形状のマスクを介して、隠蔽性を有する蒸着層を単層または複数層形成し、
蒸着層の表示部側をレーザー加工してザラツキのない内端を有する外枠部を作成することを特徴とする液晶表示パネル用部材の作成方法である。
Accordingly, an invention according to claim 1 of the present invention is a method for producing a member used in a liquid crystal display panel,
A method of creating an outer frame portion provided outside the display portion at the center of the display panel,
On the back surface of the display panel base material, a vapor deposition layer having a concealing property is formed through a mask having a display portion shape, and a single layer or a plurality of layers are formed.
A method for producing a member for a liquid crystal display panel, characterized in that an outer frame portion having an inner end free from roughness is created by laser processing the display portion side of a vapor deposition layer.
本発明の請求項2に係る発明は、液晶表示パネルに用いられる部材の作成方法において、
表示パネルの中央部の表示部の外側に設ける外枠部を作成する方法であって、
表示パネル基材の裏面に、隠蔽性を有する蒸着層を単層または複数層形成し、
前記単層または複数の蒸着層上にフォトレジストを塗布した後、フォトマスクを介してフォトレジストを露光、現像して外枠を作成することを特徴とする液晶表示パネル用部材の作成方法である。
The invention according to claim 2 of the present invention is a method for producing a member used in a liquid crystal display panel,
A method of creating an outer frame portion provided outside the display portion at the center of the display panel,
A vapor deposition layer having a concealing property is formed on the back surface of the display panel substrate as a single layer or a plurality of layers,
A method for producing a member for a liquid crystal display panel, comprising: applying a photoresist on the single layer or the plurality of vapor deposition layers; and exposing and developing the photoresist through a photomask to create an outer frame. .
本発明の請求項3に係る発明は、前記複数の蒸着層の内の1層を、インクジェット層に変えたことを特徴とする請求項1または2に記載の液晶表示パネル用部材の作成方法である。 The invention according to claim 3 of the present invention is the method for producing a liquid crystal display panel member according to claim 1 or 2, wherein one of the plurality of vapor deposition layers is changed to an ink jet layer. is there.
本発明の請求項4に係る発明は、液晶表示パネルに用いられる部材において、
表示パネルの中央部の表示部の外側に外枠を備えた液晶表示パネル用部材であって、
表示パネル基材の裏面に、表示部形状のマスクを介して隠蔽性を有する蒸着層を単層または複数層設け、
蒸着層の表示部側をレーザー加工してザラツキのない内端を有する外枠部を備えたことを特徴とする液晶表示パネル用部材である。
The invention according to claim 4 of the present invention is a member used for a liquid crystal display panel,
A liquid crystal display panel member having an outer frame outside the display portion at the center of the display panel,
On the back surface of the display panel substrate, a vapor deposition layer having concealability is provided via a mask having a display portion shape, and a single layer or a plurality of layers are provided,
A liquid crystal display panel member comprising an outer frame portion having an inner end free from roughness by laser processing of a display portion side of a vapor deposition layer.
本発明の請求項5に係る発明は、液晶表示パネルに用いられる部材において、
表示パネルの中央部の表示部の外側に外枠部を備えた液晶表示パネル用部材であって、
表示パネル基材の裏面に、隠蔽性を有する蒸着層を単層または複数層設け、
前記単層または複数の蒸着層上にフォトレジストを塗布した後、フォトマスクを介してフォトレジストを露光、現像して得られた外枠部を備えたことを特徴とする液晶表示パネル用部材である。
The invention according to claim 5 of the present invention is a member used for a liquid crystal display panel,
A liquid crystal display panel member having an outer frame portion outside the display portion at the center of the display panel,
On the back surface of the display panel substrate, a vapor deposition layer having a concealing property is provided as a single layer or multiple layers,
A liquid crystal display panel member comprising an outer frame portion obtained by applying a photoresist on the single layer or the plurality of vapor deposition layers, and then exposing and developing the photoresist through a photomask. is there.
本発明の請求項6に係る発明は、前記複数の蒸着層の内の1層を、インクジェット層に変えたことを特徴とする請求項4または5に記載の液晶表示パネル用部材である。 The invention according to claim 6 of the present invention is the liquid crystal display panel member according to claim 4 or 5, wherein one of the plurality of vapor deposition layers is changed to an ink jet layer.
本発明によれば、表示部と段差の少ない隠蔽性のある外枠部を作成することが出来、その結果、タッチパネル電極層あるいはRGB表示層を設ける場合に気泡の抱き込みを発生することがなくなる。更に表示部形状のマスクを介して作成した外枠部の内端をレーザー加工することによって、またフォトレジストを塗布した後、フォトマスクを介してフォト
レジストを露光、現像して外枠を作成することによって、ザラツキのない外枠を作成することが出来るため、美粧性に優れた外枠部を得ることが出来る。
According to the present invention, it is possible to create a concealing outer frame portion having a small step with respect to the display portion, and as a result, when the touch panel electrode layer or the RGB display layer is provided, the inclusion of bubbles does not occur. . Furthermore, by laser processing the inner edge of the outer frame portion created through the display-shaped mask, and after applying a photoresist, the photoresist is exposed and developed through the photomask to create an outer frame. Therefore, an outer frame free from roughness can be created, so that an outer frame portion having excellent cosmetic properties can be obtained.
以下、図面を参照して本発明に係る液晶表示パネル用部材の作成方法及び液晶表示パネル用部材を実施するための形態を説明する。 DESCRIPTION OF EMBODIMENTS Hereinafter, a method for producing a liquid crystal display panel member and a liquid crystal display panel member according to the present invention will be described with reference to the drawings.
図4は本発明による液晶表示パネル用部材110を作成する方法を説明するための図である。表示パネル用部材110は、ガラスシート、PMMAシート、PCシートのいずれかを用いたパネル基材14に蒸着層26−1、接着層17、ハードコート層18が設けられており、また最上面には保護フィルム19が貼られている。 FIG. 4 is a view for explaining a method of producing the liquid crystal display panel member 110 according to the present invention. In the display panel member 110, a vapor deposition layer 26-1, an adhesive layer 17, and a hard coat layer 18 are provided on a panel base material 14 using any one of a glass sheet, a PMMA sheet, and a PC sheet, and on the uppermost surface. The protective film 19 is affixed.
(実施例1)
本発明に係る蒸着層26−1は、先ず、パネル基材14に表示部をマスキングして、隠蔽を考慮した黒蒸着(例えばクロム蒸着)によって第一の蒸着層26−1を加飾形成して外枠部を得る(図4(a))。隠蔽性が足りない場合は、第二蒸着層またはインクジェット層26−2を加飾形成する(図4(b))。この場合の第二蒸着層またはインクジェット層26−2は、第一の蒸着層と同等又は同等以下の極薄加飾層である。
Example 1
First, the vapor deposition layer 26-1 according to the present invention masks the display portion on the panel base 14 and decorates and forms the first vapor deposition layer 26-1 by black vapor deposition (for example, chromium vapor deposition) in consideration of concealment. To obtain an outer frame (FIG. 4A). When the concealability is insufficient, the second vapor-deposited layer or the inkjet layer 26-2 is decorated and formed (FIG. 4B). In this case, the second vapor-deposited layer or the inkjet layer 26-2 is an ultra-thin decorative layer that is equal to or less than or equal to the first vapor-deposited layer.
次に、マスキングを剥離し、その後、接着材OCA(光学接着剤)を塗布しUV硬化を行って接着層17を形成する(図4(c))。 Next, the masking is peeled off, and then an adhesive OCA (optical adhesive) is applied and UV curing is performed to form the adhesive layer 17 (FIG. 4C).
図5(a)は(図4(c))を上面から見た図で、この場合、マスキングされた表示部30の外枠部31の内端32は鋸歯状のザラツキが見られる(図5(b))。このザラツキは、意匠性を悪くするため、以下に述べるレーザーによる微細加工を施す。 FIG. 5A is a top view of FIG. 4C. In this case, the inner end 32 of the outer frame portion 31 of the masked display portion 30 has saw-toothed roughness (FIG. 5). (B)). In order to deteriorate the designability, this roughness is subjected to fine processing by laser as described below.
そこで、近紫外レーザー、遠紫外レーザー、超短パルスレーザーなどのレーザー光線を外枠部31の内端32に沿って照射し、黒蒸着を溶かして内端32をザラツキのない内端32aに仕上げる(図5(c))。 Therefore, a laser beam such as a near-ultraviolet laser, a far-ultraviolet laser, or an ultrashort pulse laser is irradiated along the inner end 32 of the outer frame portion 31 to melt the black deposition and finish the inner end 32 to an inner end 32a without roughness ( FIG. 5 (c)).
上記レーザー加工によれば、(図5(d))に示すザラツキの大きさ(山谷のピーク高さの範囲Pを指す)はサンプル数n=3で、蒸着直後が432μmであったのに対して、レーザー加工後は225μmと滑らかになり、レーザー加工による効果が認められ、美粧性に優れた外枠が得られた。 According to the above laser processing, the roughness (showing the peak height range P of the valley) shown in (FIG. 5 (d)) was n = 3 and 432 μm immediately after the deposition. After the laser processing, it became as smooth as 225 μm, the effect of laser processing was recognized, and an outer frame excellent in cosmetics was obtained.
また、上記第一の蒸着層26−1は、2420〜3330Å程度であり、第二の蒸着層またはインクジェット層26−2は第一の蒸着層と同等、又はより薄いため、UV硬化OCA接着剤(厚み:数μm)をその後全面塗布しても、パネル基材14の裏面の表示部と外枠部との厚み段差が生じることはない。 Moreover, since the said 1st vapor deposition layer 26-1 is about 2420-3330 mm, and the 2nd vapor deposition layer or the inkjet layer 26-2 is equivalent to a 1st vapor deposition layer, or thinner, UV hardening OCA adhesive agent Even if (thickness: several μm) is subsequently applied to the entire surface, a thickness step between the display portion and the outer frame portion on the back surface of the panel substrate 14 does not occur.
従来のスクリーン印刷によって得られた外枠部を備えた液晶表示用部材と上記方法によって得られた外枠部を備えた液晶表示用部材の0.5mmΦ以上の気泡の抱き込み不良の発生回数を比較した結果、サンプル数n=10に対して従来のスクリーン印刷によって得られた外枠部を備えた液晶表示用部材が5回であったのに対して、上記方法によって得られた外枠部を備えた液晶表示用部材の場合には2回であり、不良発生の頻度が少ないことが認められた。 The number of occurrences of defective inclusion of bubbles of 0.5 mmΦ or more in a liquid crystal display member having an outer frame part obtained by conventional screen printing and a liquid crystal display member having an outer frame part obtained by the above method As a result of comparison, the number of samples n = 10 was 5 times for the liquid crystal display member having the outer frame portion obtained by conventional screen printing, whereas the outer frame portion obtained by the above method was used. In the case of the liquid crystal display member provided with the number of times, it was confirmed that the frequency of defects was small.
(実施例2)
上記では、第一の蒸着層26−1、更に第二の蒸着層26−2をマスクを用いて形成したが、図6に示すように、ガラスシート、PMMAシート、PCシートのいずれかを用いたパネル基材14の裏面に蒸着層36を設けた(図6(a))後、蒸着層36の全面にフォトレジスト膜を37を塗布し(図6(b))、次に表示枠に相当するフォトマスク38を介して露光した後(図6(c))、現像(図6(d))、レジスト膜37を剥離(図6(e))することによって外枠を作成しても良い。この場合の外枠の内端はザラツキのないものが得られ、上記レーザー加工を必要としない。
(Example 2)
In the above, the first vapor deposition layer 26-1 and the second vapor deposition layer 26-2 were formed using a mask, but as shown in FIG. 6, any one of a glass sheet, a PMMA sheet, and a PC sheet was used. After the vapor deposition layer 36 was provided on the back surface of the panel substrate 14 (FIG. 6A), a photoresist film 37 was applied to the entire surface of the vapor deposition layer 36 (FIG. 6B), and then the display frame was formed. Even after exposure through the corresponding photomask 38 (FIG. 6C), development (FIG. 6D), and peeling off the resist film 37 (FIG. 6E), an outer frame can be formed. good. In this case, the inner edge of the outer frame is free from roughness, and the laser processing is not required.
尚、上記説明ではクロム蒸着によって黒色に加飾形成する外枠部を例示したが、これに限定されず、蒸着膜の設計を行い、蒸着の材料種類や膜厚や層数を決めることによって、有色でしかも美粧性、隠蔽性に優れた外枠部を加飾形成することが出来る。 In the above description, the outer frame portion that is decorated in black by chromium vapor deposition is exemplified, but the present invention is not limited to this, by designing the vapor deposition film, and by determining the material type, film thickness, and number of layers for vapor deposition, It is possible to decorate and form an outer frame portion that is colored and excellent in cosmetics and concealment.
また、蒸着による外枠部の形成であるので図7に示すような外枠部31に形成された例えばアイコン部40を有する静電容量のタッチパネルにおいて、容易にタッチレスポンスを得ることが出来る。 Further, since the outer frame portion is formed by vapor deposition, a touch response can be easily obtained in a capacitive touch panel having, for example, the icon portion 40 formed on the outer frame portion 31 as shown in FIG.
このようにして、段差のない隠蔽性、美粧性に優れた蒸着加飾パネルを得ることが出来る。 In this way, it is possible to obtain a vapor-deposited decorative panel excellent in concealability and cosmetics without steps.
以上のように本発明による液晶表示パネル用部材の作成方法によれば、隠蔽性、美粧性の高い液晶表示パネル用部材が得られる。また、パネル基材の裏面に形成される表示部と外枠部との段差は、従来に比べて格段に小さくなり、パネルに加工する際の歩留まり向上が可能となる。 As described above, according to the method for producing a member for a liquid crystal display panel according to the present invention, a member for a liquid crystal display panel having high concealability and cosmetics can be obtained. Further, the step between the display portion and the outer frame portion formed on the back surface of the panel base material is remarkably smaller than the conventional case, and the yield when processing into a panel can be improved.
1・・・内枠部(表示部)
2・・・外枠部
3・・・ミラー文字
4・・・表示パネル基材
5・・・ミラー印刷層
6・・・インキ層
7・・・接着層
8・・・ハードコート層
9・・・保護フィルム
10・・・タッチパネル電極層
11・・・RGB表示層
14・・・パネル基材
17・・・接着層
18・・・ハードコート層
19・・・保護フィルム
26−1・・・第一の蒸着層
26−2・・・第二蒸着層またはインクジェット層
30・・・マスキングされた表示部
31・・・マスキングされた表示部の外側の外枠部
32・・・外枠部31の内端
32a・・・ザラツキのない内端
37・・・レジスト膜
38・・・フォトマスク
40・・・アイコン部
100、101・・・携帯電話の表示パネル
110・・・本発明による液晶表示パネル用部材
P・・・山谷のピーク高さの範囲
1 ... Inner frame (display)
2 ... Outer frame part 3 ... Mirror character 4 ... Display panel base material 5 ... Mirror printing layer 6 ... Ink layer 7 ... Adhesive layer 8 ... Hard coat layer 9 ... Protective film 10 ... Touch panel electrode layer 11 ... RGB display layer 14 ... Panel substrate 17 ... Adhesive layer 18 ... Hard coat layer 19 ... Protective film 26-1 ... No. One vapor deposition layer 26-2 ... second vapor deposition layer or inkjet layer 30 ... masked display part 31 ... outer frame part 32 outside masked display part ... outer frame part 31 Inner end 32a ... Roughly inner end 37 ... Resist film 38 ... Photomask 40 ... Icon portion 100, 101 ... Mobile phone display panel 110 ... Liquid crystal display panel according to the present invention Member P ... Peak valley range
Claims (6)
表示パネルの中央部の表示部の外側に設ける外枠部を作成する方法であって、
表示パネル基材の裏面に、表示部形状のマスクを介して、隠蔽性を有する蒸着層を単層または複数層形成し、
蒸着層の表示部側をレーザー加工してザラツキのない内端を有する外枠部を作成することを特徴とする液晶表示パネル用部材の作成方法。 In a method for creating a member used in a liquid crystal display panel,
A method of creating an outer frame portion provided outside the display portion at the center of the display panel,
On the back surface of the display panel base material, a vapor deposition layer having a concealing property is formed through a mask having a display portion shape, and a single layer or a plurality of layers are formed.
A method for producing a member for a liquid crystal display panel, characterized in that an outer frame portion having an inner end without roughness is produced by laser processing the display portion side of a vapor deposition layer.
表示パネルの中央部の表示部の外側に設ける外枠部を作成する方法であって、
表示パネル基材の裏面に、隠蔽性を有する蒸着層を単層または複数層形成し、
前記単層または複数の蒸着層上にフォトレジストを塗布した後、フォトマスクを介してフォトレジストを露光、現像して外枠を作成することを特徴とする液晶表示パネル用部材の作成方法。 In a method for creating a member used in a liquid crystal display panel,
A method of creating an outer frame portion provided outside the display portion at the center of the display panel,
A vapor deposition layer having a concealing property is formed on the back surface of the display panel substrate as a single layer or a plurality of layers,
A method for producing a member for a liquid crystal display panel, comprising: applying a photoresist on the single layer or the plurality of deposited layers; and exposing and developing the photoresist through a photomask to create an outer frame.
表示パネルの中央部の表示部の外側に外枠を備えた液晶表示パネル用部材であって、
表示パネル基材の裏面に、表示部形状のマスクを介して隠蔽性を有する蒸着層を単層または複数層設け、
蒸着層の表示部側をレーザー加工してザラツキのない内端を有する外枠部を備えたことを特徴とする液晶表示パネル用部材。 In members used for liquid crystal display panels,
A liquid crystal display panel member having an outer frame outside the display portion at the center of the display panel,
On the back surface of the display panel substrate, a vapor deposition layer having concealability is provided via a mask having a display portion shape, and a single layer or a plurality of layers are provided,
A member for a liquid crystal display panel, comprising an outer frame portion having an inner end free from roughness by laser processing of the display portion side of the vapor deposition layer.
表示パネルの中央部の表示部の外側に外枠部を備えた液晶表示パネル用部材であって、
表示パネル基材の裏面に、隠蔽性を有する蒸着層を単層または複数層設け、
前記単層または複数の蒸着層上にフォトレジストを塗布した後、フォトマスクを介してフォトレジストを露光、現像して得られた外枠部を備えたことを特徴とする液晶表示パネル用部材。 In members used for liquid crystal display panels,
A liquid crystal display panel member having an outer frame portion outside the display portion at the center of the display panel,
On the back surface of the display panel substrate, a vapor deposition layer having a concealing property is provided as a single layer or multiple layers,
A member for a liquid crystal display panel, comprising an outer frame portion obtained by applying a photoresist on the single layer or the plurality of vapor deposition layers and then exposing and developing the photoresist through a photomask.