JP2012221833A - 鉛蓄電池 - Google Patents
鉛蓄電池 Download PDFInfo
- Publication number
- JP2012221833A JP2012221833A JP2011088258A JP2011088258A JP2012221833A JP 2012221833 A JP2012221833 A JP 2012221833A JP 2011088258 A JP2011088258 A JP 2011088258A JP 2011088258 A JP2011088258 A JP 2011088258A JP 2012221833 A JP2012221833 A JP 2012221833A
- Authority
- JP
- Japan
- Prior art keywords
- negative electrode
- carbon black
- mass
- surface layer
- lead
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
鉛蓄電池の負極活物質は、主成分が海綿状の鉛で、かつ平均粒子径が50nm以下で10nm以上のカーボンブラックを1.5mass%以上10mass%以下含有する表層と、主成分が海綿状の鉛で、カーボンブラック含有量が1.0mass%以下の内部層とで構成する。
【効果】
鉛蓄電池の放電容量を僅かしか低下しないようにしながら、高率PSOCサイクル寿命を効果的に向上させる。
【選択図】 図3
Description
0.07mass%のカルシウムと1.5mass%の錫と不可避不純物とを含み残余が鉛の鉛−カルシウム−錫系合金を、ロータリーエキスパンド法により加工した正極格子を使用した。正極活物質として、ボールミル法の鉛粉99.9mass%に0.1mass%のアクリル繊維を加え、この混合物100mass%に、水13mass%と20℃で比重が1.40の希硫酸10mass%とを混合し、正極活物質材料として、正極格子骨部に充填した。
・ 平均粒子径が20nmで、BET法で窒素ガスを吸着させた際の比表面積(以下同様)が 200m2/gのカーボンブラックA、
・ 平均粒子径が30nmで、比表面積70m2/gのカーボンブラックB、
・ 平均粒子径が50nmで、比表面積30m2/gのカーボンブラックC、
・ 平均粒子径が60nmで、比表面積30m2/gのカーボンブラックD、
の4種類である。なお内部層10にはカーボンブラックBを用いた。
各鉛蓄電池に対し、0.2C0.12A放電容量を測定した。さらに各鉛蓄電池に対し、1C0.6A×6分間の移行放電を行い、サイクル充放電として周囲温度25℃で、1C0.6A×18分間の放電と1C0.6A×18分間の充電とを行い、18分間の放電中に端子電圧が1.0V以下に低下するとサイクル充放電を打ち切り、打ち切りまでのサイクル数を高率PSOCサイクル数とした。この試験は、PSOC下での高率放電により負極活物質に硫酸鉛を蓄積させた際の耐久性を評価するものである。試料数は各3で、結果は平均値で示す。
4 負極格子骨部
6 負極活物質
8,9 表層
10 内部層
Claims (3)
- 負極格子骨部に負極活物質を支持させた負極板と、正極格子骨部に正極活物質を支持させた正極板と、負極板と正極板とを浸す電解液とを備える鉛蓄電池であって、
前記負極活物質は、主成分が海綿状の鉛で、かつ平均粒子径が50nm以下で10nm以上のカーボンブラックを1.5mass%以上10mass%以下含有する表層と、主成分が海綿状の鉛で、カーボンブラック含有量が1.0mass%以下で、かつ前記表層の内側の内部層とから成ることを特徴とする、鉛蓄電池。 - 負極板の左右両面に前記表層が設けられている場合は、左右の表層の合計厚さと前記負極板の厚さとの比が、負極板の片面にのみ前記表層が設けられている場合は、片面の表層の厚さと前記負極板の厚さとの比が、各々1/4以上2/5以下であることを特徴とする、請求項1の鉛蓄電池。
- 負極板の左右両面に前記表層が設けられていることを特徴とする、請求項1または2の鉛蓄電池。