JP2011530008A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2011530008A5 JP2011530008A5 JP2011521444A JP2011521444A JP2011530008A5 JP 2011530008 A5 JP2011530008 A5 JP 2011530008A5 JP 2011521444 A JP2011521444 A JP 2011521444A JP 2011521444 A JP2011521444 A JP 2011521444A JP 2011530008 A5 JP2011530008 A5 JP 2011530008A5
- Authority
- JP
- Japan
- Prior art keywords
- sliding component
- operating surface
- alloy
- copper
- beryllium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
- 239000000956 alloy Substances 0.000 claims 6
- 229910045601 alloy Inorganic materials 0.000 claims 6
- 229910052790 beryllium Inorganic materials 0.000 claims 6
- 238000000034 method Methods 0.000 claims 6
- 239000010936 titanium Substances 0.000 claims 6
- 229910052719 titanium Inorganic materials 0.000 claims 6
- RYGMFSIKBFXOCR-UHFFFAOYSA-N Copper Chemical compound [Cu] RYGMFSIKBFXOCR-UHFFFAOYSA-N 0.000 claims 3
- RTAQQCXQSZGOHL-UHFFFAOYSA-N Titanium Chemical compound [Ti] RTAQQCXQSZGOHL-UHFFFAOYSA-N 0.000 claims 3
- 239000000654 additive Substances 0.000 claims 3
- ATBAMAFKBVZNFJ-UHFFFAOYSA-N beryllium atom Chemical compound [Be] ATBAMAFKBVZNFJ-UHFFFAOYSA-N 0.000 claims 3
- 239000011248 coating agent Substances 0.000 claims 3
- 238000000576 coating method Methods 0.000 claims 3
- 238000002485 combustion reaction Methods 0.000 claims 3
- 229910052802 copper Inorganic materials 0.000 claims 3
- 239000010949 copper Substances 0.000 claims 3
- 238000000151 deposition Methods 0.000 claims 2
- 230000008021 deposition Effects 0.000 claims 1
- 238000007749 high velocity oxygen fuel spraying Methods 0.000 claims 1
- 238000004519 manufacturing process Methods 0.000 claims 1
- 238000007750 plasma spraying Methods 0.000 claims 1
- 239000007921 spray Substances 0.000 claims 1
- 238000007751 thermal spraying Methods 0.000 claims 1
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| DE102008036657.9 | 2008-08-06 | ||
| DE102008036657.9A DE102008036657B4 (de) | 2008-08-06 | 2008-08-06 | Kolbenring mit adaptiver Beschichtung und Herstellungsverfahren davon |
| PCT/EP2009/002907 WO2010015289A1 (de) | 2008-08-06 | 2009-04-21 | Gleitelement mit adaptiver beschichtung und herstellungsverfahren davon |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2011530008A JP2011530008A (ja) | 2011-12-15 |
| JP2011530008A5 true JP2011530008A5 (cg-RX-API-DMAC7.html) | 2012-04-26 |
| JP5788793B2 JP5788793B2 (ja) | 2015-10-07 |
Family
ID=40823595
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2011521444A Expired - Fee Related JP5788793B2 (ja) | 2008-08-06 | 2009-04-21 | 適合性コーティングを備える滑り部品及びその製造方法 |
Country Status (4)
| Country | Link |
|---|---|
| JP (1) | JP5788793B2 (cg-RX-API-DMAC7.html) |
| DE (1) | DE102008036657B4 (cg-RX-API-DMAC7.html) |
| GB (1) | GB2474791B (cg-RX-API-DMAC7.html) |
| WO (1) | WO2010015289A1 (cg-RX-API-DMAC7.html) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US20130064490A1 (en) * | 2011-09-13 | 2013-03-14 | II Ronald G. Brock | Thermal spray coating of sliding bearing lining layer |
| DE102011114420A1 (de) * | 2011-09-26 | 2013-03-28 | Audi Ag | Verfahren zum Herstellen eines Zylinderrohrs einer Brennkraftmaschine sowie entsprechendes Zylinderrohr |
| WO2018128773A1 (en) * | 2017-01-06 | 2018-07-12 | Materion Corporation | Piston compression rings of copper-beryllium alloys |
Family Cites Families (18)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE676628C (de) * | 1931-08-01 | 1939-06-08 | Metallgesellschaft Akt Ges | Kupfer-Beryllium-Legierung |
| US2030921A (en) * | 1933-06-17 | 1936-02-18 | Heraeus Vacuumschmelze Ag | Copper-beryllium alloys |
| DE1254869B (de) * | 1957-02-20 | 1967-11-23 | Ver Deutsche Metallwerke Ag | Verwendung von warm aushaertbaren Kupfer-Titan-Legierungen als Werkstoff fuer Gegenstaende, die hohe Warmfestigkeit, Unempfindlichkeit gegenueber heissen Gasen, hohe Wechselfestigkeit, Dauerstandfestigkeit und geringe elastische Nachwirkung aufweisen Muessen |
| US3773504A (en) * | 1970-12-28 | 1973-11-20 | I Niimi | Copper base alloy having wear resistance at high temperatures |
| JPS5768247A (en) * | 1980-10-13 | 1982-04-26 | Chuetsu Gokin Chuko Kk | Precipitation hardening type mold material for continuous casting |
| JPS5810986B2 (ja) * | 1980-07-07 | 1983-02-28 | トヨタ自動車株式会社 | 摺動部材 |
| JPS5832949A (ja) * | 1981-08-22 | 1983-02-26 | Nippon Piston Ring Co Ltd | ピストンリング |
| DE3329034A1 (de) * | 1983-08-11 | 1985-02-28 | M.A.N. Maschinenfabrik Augsburg-Nürnberg AG, 4200 Oberhausen | Fluessigkeitsgesperrte wellendichtung mit reduzierter gleitringtemperatur |
| US4606889A (en) * | 1985-11-07 | 1986-08-19 | Cabot Corporation | Copper-titanium-beryllium alloy |
| DK174241B1 (da) * | 1996-12-05 | 2002-10-14 | Man B & W Diesel As | Cylinderelement, såsom en cylinderforing, et stempel, et stempelskørt eller en stempelring, i en forbrændingsmotor af dieseltypen samt en stempelring til en sådan motor. |
| JPH1180921A (ja) * | 1997-07-09 | 1999-03-26 | Nippon Piston Ring Co Ltd | 摺動部材のなじみ性溶射被膜層 |
| JPH11241153A (ja) * | 1998-02-27 | 1999-09-07 | Nippon Piston Ring Co Ltd | 摺動部材のなじみ性溶射被膜層 |
| DE19908107C2 (de) * | 1999-02-25 | 2003-04-10 | Man B & W Diesel As Kopenhagen | Verfahren zur Erzeugung einer verschleißfesten Oberfläche bei aus Stahl bestehenden Bauteilen sowie Maschine mit wenigstens einem derartigen Bauteil |
| JP3366304B2 (ja) * | 1999-11-25 | 2003-01-14 | 誠石 勝見 | ダイカスト用プランジャチップ |
| JP4369757B2 (ja) * | 2002-01-18 | 2009-11-25 | 株式会社リケン | 溶射ピストンリング |
| JP4170195B2 (ja) * | 2003-10-29 | 2008-10-22 | 山陽特殊製鋼株式会社 | 摺動部材用Cu基合金 |
| DE102004043914A1 (de) * | 2004-09-10 | 2006-03-16 | Linde Ag | Gleitlagerbauteil mit einer aufgebrachten Schicht aus Lagermetall und Verfahren zum Aufbringen einer Schicht aus Lagermetall |
| JP4725229B2 (ja) * | 2005-07-28 | 2011-07-13 | トヨタ自動車株式会社 | 組合せ摺動部材、及びこれを用いた内燃機関及びすべり軸受機構 |
-
2008
- 2008-08-06 DE DE102008036657.9A patent/DE102008036657B4/de not_active Expired - Fee Related
-
2009
- 2009-04-21 GB GB1101319.0A patent/GB2474791B/en not_active Expired - Fee Related
- 2009-04-21 JP JP2011521444A patent/JP5788793B2/ja not_active Expired - Fee Related
- 2009-04-21 WO PCT/EP2009/002907 patent/WO2010015289A1/de not_active Ceased
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| WO2007134148A3 (en) | Thermal oxidation protective surface for steel pistons | |
| RU2008129858A (ru) | Топливный стержень с покрытием, препятствующим истиранию | |
| JP2014166949A5 (cg-RX-API-DMAC7.html) | ||
| WO2011075804A8 (pt) | Anel de pistão | |
| WO2013134606A3 (en) | Thermal spray applications using iron based alloy powder | |
| CN102115836B (zh) | 一种MCrAlY合金体系的高温防护涂层及制备方法 | |
| WO2011094755A4 (en) | Nickel based thermal spray powder and coating, and method for making the same | |
| WO2017080645A8 (en) | Turbine clearance control coatings and method | |
| CN104775087B (zh) | 一种金属复合陶瓷热障涂层的制备方法 | |
| JP2010522823A5 (cg-RX-API-DMAC7.html) | ||
| JP2008168346A5 (cg-RX-API-DMAC7.html) | ||
| JP2009203552A5 (cg-RX-API-DMAC7.html) | ||
| JP2011530008A5 (cg-RX-API-DMAC7.html) | ||
| JP2013174013A (ja) | 被覆物品及び物品を被覆する方法 | |
| CN103628014A (zh) | 一种钛合金的抗空蚀表面Ti-Al化涂层的制备方法 | |
| CN105441860A (zh) | 新型SiC晶须增强燃气轮机叶片复合涂层及其制备方法 | |
| CN101691647B (zh) | 一种具有高性能的热喷涂涂层 | |
| JP2016500756A5 (cg-RX-API-DMAC7.html) | ||
| US20180282853A1 (en) | Hybrid Thermal Barrier Coating and Process of Making Same | |
| CN104651835B (zh) | 一种燃气轮机叶片复合涂层 | |
| JP2022191217A (ja) | 表面を予め活性化しないシリンダボアのコーティング | |
| Jegadeeswaran et al. | Oxidation studies on as-received and HVOF sprayed Stellite-6 coating on turbine alloys at 800 C | |
| EP2964807B1 (en) | Turbine engine component comprising a lightweight and corrosion resistant abradable coating | |
| CN102388158A (zh) | 阻止热喷涂中金属氧化的方法 | |
| CN115896674A (zh) | 镍钴基低温超音速喷涂-激光伴随强化涂层的制备方法及涂层 |