JP2010284868A - Groove member for forming ruled line - Google Patents

Groove member for forming ruled line Download PDF

Info

Publication number
JP2010284868A
JP2010284868A JP2009140032A JP2009140032A JP2010284868A JP 2010284868 A JP2010284868 A JP 2010284868A JP 2009140032 A JP2009140032 A JP 2009140032A JP 2009140032 A JP2009140032 A JP 2009140032A JP 2010284868 A JP2010284868 A JP 2010284868A
Authority
JP
Japan
Prior art keywords
ruled line
ruled
groove
cardboard
corrugated cardboard
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP2009140032A
Other languages
Japanese (ja)
Inventor
Takayuki Takeuchi
孝之 竹内
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Die Steel Co Ltd
Original Assignee
Nippon Die Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Die Steel Co Ltd filed Critical Nippon Die Steel Co Ltd
Priority to JP2009140032A priority Critical patent/JP2010284868A/en
Publication of JP2010284868A publication Critical patent/JP2010284868A/en
Pending legal-status Critical Current

Abstract

<P>PROBLEM TO BE SOLVED: To provide an improved groove member for forming a ruled line capable of putting the ruled line where a corrugated cardboard can be exactly folded at a prescribed position. <P>SOLUTION: In the groove member for forming ruled line in which a recessed groove 2 is formed oppositely to a ruled line pressing member 23, the corrugated cardboard 51 pressed by the ruled line pressing member 23 is received by the recessed groove 2 in accordance with approach of the ruled line pressing member 23 and thereby, the ruled line 52 is put on the corrugated cardboard 51, at least one side face of the recessed groove 2 is made to be an inclined side face 2a which is inclined outward from the bottom part to an opening part. When the corrugated cardboard 51 is pushed into the recessed groove 2 by the ruled line pressing member 23, since the corrugated cardboard 51 is pushed into the bottom part of the recessed groove 2 while being slid along the inclined face 2a of the recessed groove 2, the ruled line 52 can be put deeply and clearly without causing cracking of the corrugated cardboard 51 and the corrugated cardboard 51 can be folded without being affected by step parts 53. <P>COPYRIGHT: (C)2011,JPO&INPIT

Description

この発明は、段ボールに、押罫部材による押圧に伴い、折曲用の罫線を入れる罫線形成用溝部材に関するものである。   The present invention relates to a ruled line forming groove member for placing a bent ruled line on a corrugated board when pressed by a ruled member.

段ボールを打ち抜いて罫線を入れ、罫線に沿って折り曲げて箱を形成する場合、段ボールが罫線に沿って正確に折れ曲がらず、不良が発生するおそれがある。特に、段ボールのライナに挟まれた波状の中芯の段頂が延びる方向である段目の方向の罫線に沿って段ボールを折り曲げる場合に、段目と折曲位置との位置関係や角度が一定せず、折曲位置が所定の位置からずれる可能性が高くなる。   When a corrugated cardboard is punched to form a ruled line and bent along the ruled line to form a box, the cardboard is not bent accurately along the ruled line, which may cause a defect. In particular, when corrugated cardboard is folded along a ruled line in the direction of the corrugation, which is the direction in which the corrugated core step between the corrugated cardboard liners extends, the positional relationship and angle between the corrugation and the folding position are constant. Without this, there is a high possibility that the folding position will deviate from the predetermined position.

その対策として、図9に示すように、上盤11及び下盤12を備えたダイカッタ等の加工機において、上盤11にチェース13を介して長い切刃22及び押罫部材23を備えた型体21を装着し、下盤12にデッドプレート14を介して長い凹溝32を有する溝部材としての金属製の面板31を装着して、これにより段ボール51の打抜及び罫入れ加工が行なわれている。   As a countermeasure, as shown in FIG. 9, in a processing machine such as a die cutter provided with an upper board 11 and a lower board 12, a mold provided with a long cutting edge 22 and a ruled member 23 on the upper board 11 via a chase 13. The body 21 is mounted, and a metal face plate 31 as a groove member having a long concave groove 32 is mounted on the lower board 12 via the dead plate 14, whereby the corrugated cardboard 51 is punched and creased. ing.

この場合、上盤11と下盤12の接近に伴い、型体21と面板31との間に挟み込んだ段ボール51を切刃22で打ち抜く際、図10に示すように、押罫部材23を段ボール51に押し付けて、段ボール51を凹溝32に押し込むことにより、段ボール51が下方へ湾曲した長い罫線52を段目53の方向に沿って形成する(下記特許文献1参照)。ここで、凹溝32は、両側面が垂直となっているものが想定されている。   In this case, when the corrugated cardboard 51 sandwiched between the mold body 21 and the face plate 31 is punched with the cutting blade 22 as the upper board 11 and the lower board 12 approach, as shown in FIG. The cardboard 51 is pressed into the concave groove 32 and pressed to form a long ruled line 52 in which the cardboard 51 is curved downward (see Patent Document 1 below). Here, the concave groove 32 is assumed to have vertical sides.

また、図11及び図12に示すように、型体21に、折曲用の罫線を入れる長い押罫部材23に加えて、これに交差する短い押罫部材24を保持具25で保持して固定し、デッドプレート14に長い凹溝34を有するプラスチック製の溝部材33を各罫線ごとに貼り付けて、罫入れ加工を行なうことも提案されている。   Further, as shown in FIGS. 11 and 12, in addition to a long ruled member 23 for putting a ruled line for bending in the mold body 21, a short ruled member 24 intersecting this is held by a holder 25. It has also been proposed to perform a crease process by fixing and attaching a plastic groove member 33 having a long concave groove 34 to the dead plate 14 for each ruled line.

この場合、押罫部材23を段ボール51に押し付け、段ボール51を凹溝34に押し込んで、段ボール51に下方へ湾曲した長い罫線52を形成すると共に、押罫部材24により、罫線52に交差する短い罫線52cを形成する。これにより、折曲時の応力が罫線52に集中して、段ボール51が長い罫線52に沿って折れ曲がり易くなる(下記特許文献2参照)。   In this case, the ruler member 23 is pressed against the corrugated cardboard 51 and the cardboard 51 is pushed into the concave groove 34 to form a long ruled line 52 curved downward in the cardboard 51, and a short line intersecting the ruled line 52 by the ruler member 24. A ruled line 52c is formed. Thereby, the stress at the time of bending concentrates on the ruled line 52, and the corrugated board 51 becomes easy to bend along the long ruled line 52 (refer patent document 2 below).

特開2003−145492号公報JP 2003-145492 A 特開平9−70905号公報JP-A-9-70905

しかしながら、上記のように凹溝32の両側面が垂直な溝部材としての面板31を用いて罫線52を入れると、凹溝32の開口端の角部で段ボールが破れる罫割れ現象が生じることがあり、罫線52の深さを抑制する必要があることから、所期の効果を得られない場合がある。   However, if the ruled line 52 is inserted using the face plate 31 as a groove member in which both side surfaces of the concave groove 32 are vertical as described above, a ruled cracking phenomenon in which the cardboard is broken at the corner of the opening end of the concave groove 32 may occur. In addition, since it is necessary to suppress the depth of the ruled line 52, the desired effect may not be obtained.

また、溝部材33を用いる場合、溝部材33の劣化に伴う交換が頻繁に必要となる等の手間を要し、打抜作業中に溝部材33がデッドプレート14から外れて、製品に混入するおそれがあるほか、押罫部材24で入れられた罫線52cによって段ボール51の見栄えが悪くなるという問題もある。   Further, when the groove member 33 is used, it takes time and effort to frequently replace the groove member 33 due to the deterioration of the groove member 33, and the groove member 33 is detached from the dead plate 14 during the punching operation and mixed into the product. Besides, there is a problem that the appearance of the cardboard 51 is deteriorated by the ruled line 52c inserted by the ruled member 24.

そこで、この発明は、罫線形成用溝部材の改良により、段ボールを所定の位置で正確に折り曲げられる罫線を入れることを課題とする。   SUMMARY OF THE INVENTION Accordingly, an object of the present invention is to provide a ruled line for accurately folding a cardboard at a predetermined position by improving the ruled line forming groove member.

上記のような課題を解決するため、この発明では、押罫部材に対向して凹溝を形成し、押罫部材との接近に伴い、押罫部材に押圧された段ボールを凹溝で受けて、段ボールに罫線を入れる罫線形成用溝部材において、前記凹溝の少なくとも一方の側面を、底部から開口部へかけて外側へ傾斜した傾斜側面としたのである。   In order to solve the above-described problems, in the present invention, a concave groove is formed facing the ruled member, and the cardboard pressed by the ruled member is received by the concave groove with the approach to the ruled member. In the groove member for forming a ruled line for putting a ruled line in the cardboard, at least one side surface of the concave groove is an inclined side surface inclined outward from the bottom part to the opening part.

この発明に係る罫線形成用溝部材を使用すると、段ボールを押罫部材で凹溝に押し込む際、段ボールが凹溝の傾斜側面に沿って滑りながら凹溝の底部に押し込まれるので、段ボールの割れを生じることなく、深く鮮明に罫線を入れることができ、その罫線に沿って、段ボールを所定の位置で正確に折り曲げることができる。   When the ruled line forming groove member according to the present invention is used, when the cardboard is pushed into the concave groove by the ruled member, the cardboard is pushed into the bottom of the concave groove while sliding along the inclined side surface of the concave groove. A ruled line can be drawn deeply and clearly without being generated, and the cardboard can be accurately bent at a predetermined position along the ruled line.

また、凹溝の両方の側面を傾斜側面とすると、罫線を両側対称な形状にでき、段ボールを罫線の幅方向中心線に沿って正確に折り曲げることができる。   Further, if both side surfaces of the concave groove are inclined side surfaces, the ruled line can be made symmetrical on both sides, and the cardboard can be accurately folded along the center line in the width direction of the ruled line.

また、凹溝の一方の側面のみを傾斜側面とし、他方の側面を垂直側面にしておくと、段ボールを押罫部材で凹溝に押し込む際、垂直側面を基準にして、段ボールが傾斜側面に沿って滑りながら凹溝に押し込まれ、段ボールの割れを生じることなく、深く鮮明に罫線を入れることができ、段ボールを折り曲げる際には、垂直側面で形成された罫線の一側に沿って、所定の位置で正確に折り曲げることができる。   In addition, if only one side surface of the groove is an inclined side surface and the other side surface is a vertical side surface, when the cardboard is pushed into the groove with a ruled member, the cardboard will follow the inclined side surface with respect to the vertical side surface. It can be slipped and pushed into the concave groove, and the ruled line can be deeply and clearly inserted without cracking the cardboard. Can be bent accurately at the position.

この発明の第1実施形態に係る罫線形成用溝部材としての面板と押罫部材とを加工機へ装着した状態を示す断面図Sectional drawing which shows the state which mounted | wore the processing machine with the face plate and ruled member as a ruled line formation groove | channel member concerning 1st Embodiment of this invention. 同上の面板のデッドプレートへの取付状態を示す断面図Sectional drawing which shows the attachment state to the dead plate of a face plate same as the above 同上の面板と押罫部材の間に段ボールを供給した状態を示す断面図Sectional drawing which shows the state which supplied the corrugated board between the face plate same as the above, and a ruled member 同上の面板と押罫部材による罫入れ状態を示す断面図Sectional drawing which shows the ruled state by a face plate and a ruled member same as the above この発明の第2実施形態に係る罫線形成用溝部材としての面板と押罫部材とを加工機へ装着した状態を示す断面図Sectional drawing which shows the state which mounted | wore the processing machine with the face plate and ruled member as a ruled line formation groove | channel member concerning 2nd Embodiment of this invention. 同上の面板のデッドプレートへの取付状態を示す断面図Sectional drawing which shows the attachment state to the dead plate of a face plate same as the above 同上の面板と押罫部材の間に段ボールを供給した状態を示す断面図Sectional drawing which shows the state which supplied the corrugated board between the face plate same as the above, and a ruled member 同上の面板と押罫部材による罫入れ状態を示す断面図Sectional drawing which shows the ruled state by a face plate and a ruled member same as the above 従来の罫線形成用溝部材としての面板と押罫部材とを加工機へ装着した状態を示す断面図Sectional drawing which shows the state which mounted | wore the processing machine with the face plate and the crease member as the conventional groove member for ruled line formation 同上の面板と押罫部材による罫入れ状態を示す断面図Sectional drawing which shows the ruled state by a face plate and a ruled member same as the above 従来の他の罫線形成用溝部材と押罫部材とを加工機へ装着した状態を示す断面図Sectional drawing which shows the state which mounted | wore the other conventional ruled line formation groove member and the crease member to the processing machine 同上の溝部材と押罫部材による罫入れ状態を示す断面図Sectional drawing which shows the ruled state by a groove member and a ruled member same as the above

以下、この発明の第1実施形態を図1乃至図4に基づいて説明する。   A first embodiment of the present invention will be described below with reference to FIGS.

図1に示す溝部材としての面板1は、ステンレス等の金属製とされ、上盤11及び下盤12を備えた平型ダイカッタである加工機の下盤12に、デッドプレート14を介して装着される。この加工機では、上盤11に対して下盤12が昇降し、若しくは下盤12に対して上盤11が昇降し、又は上盤11と下盤12の双方が昇降することにより、上盤11と下盤12とが相対的に接近離反する。   A face plate 1 as a groove member shown in FIG. 1 is made of a metal such as stainless steel, and is attached to a lower plate 12 of a processing machine, which is a flat die cutter provided with an upper plate 11 and a lower plate 12, via a dead plate 14. Is done. In this processing machine, the lower board 12 moves up and down with respect to the upper board 11, or the upper board 11 moves up and down with respect to the lower board 12, or both the upper board 11 and the lower board 12 move up and down. 11 and the lower board 12 approach and separate relatively.

上盤11には、チェース13を介して、それぞれ線状に長さを有する切刃22及び押罫部材23を備えた型体21が装着される。   A mold body 21 having cutting edges 22 and ruled members 23 each having a linear length is mounted on the upper board 11 via the chase 13.

面板1には、図2及び図3に示すように、押罫部材23の下部先端に対向する上面を切り込んで長い凹溝2が形成され、凹溝2の両側面は、下方の底部から上方の開口部へかけて外側へ傾斜した傾斜側面2aとされている。凹溝2の上端の開口部側の幅は、押罫部材23の幅より大きくなっている。   As shown in FIGS. 2 and 3, the face plate 1 is formed with long concave grooves 2 by cutting the upper surface facing the lower end of the ruled member 23, and both side surfaces of the concave grooves 2 are upward from the bottom at the bottom. It is set as the inclination side surface 2a which inclined outside toward the opening part. The width of the upper end side of the groove 2 on the opening side is larger than the width of the ruled member 23.

このような面板1を、図1に示す加工機に装着する際には、凹溝2と押罫部材23の幅方向の中心線が一致するように、型体21及び面板1を位置決めする。   When such a face plate 1 is mounted on the processing machine shown in FIG. 1, the mold body 21 and the face plate 1 are positioned so that the center line in the width direction of the groove 2 and the ruled line member 23 coincides.

いま、箱形成用のブランクを製造するため、段ボール51を打ち抜くと共に罫線を入れるには、上盤11に対して下盤12が下降し、面板1と型体21とが離反した状態で、図3に示すように、面板1と押罫部材23の間に、面板1の上面に沿って平坦な状態で段ボール51を供給する。ここでは、押罫部材23として、先端が平坦になった角罫を使用した場合を例示する。   Now, in order to produce a blank for forming a box, in order to punch out the cardboard 51 and put a ruled line, the lower plate 12 is lowered with respect to the upper plate 11, and the face plate 1 and the mold body 21 are separated from each other. As shown in FIG. 3, the corrugated cardboard 51 is supplied between the face plate 1 and the ruled member 23 in a flat state along the upper surface of the face plate 1. Here, a case where a square rule with a flat tip is used as the ruled member 23 is illustrated.

次に、図1及び図3に示す状態から、上盤11に対して下盤12を上昇させると、段ボール51が面板1と型体21とで挟まれて、切刃22で段ボール51が打ち抜かれ、箱のブランクの輪郭が形成される。この状態において、押罫部材23の下端部は、平坦な状態であった段ボール51の上面より下方に位置することとなる。   Next, when the lower board 12 is raised with respect to the upper board 11 from the state shown in FIGS. 1 and 3, the cardboard 51 is sandwiched between the face plate 1 and the mold body 21, and the cardboard 51 is hit by the cutting edge 22. It is pulled out and a blank outline of the box is formed. In this state, the lower end portion of the ruled line member 23 is positioned below the upper surface of the corrugated cardboard 51 that has been flat.

このとき、図4に示すように、剛性を有する段ボール51は、押罫部材23の押圧に伴い、凹溝2の両側の傾斜側面2aに沿って滑りながら、凹溝2の底部に接するまで凹溝2に押し込まれるので、長い罫線52を深く入れても、段ボール51のライナが過度に引っ張られて、段ボール51に割れを生じることがない。   At this time, as shown in FIG. 4, the corrugated cardboard 51 having rigidity is recessed until it contacts the bottom of the groove 2 while sliding along the inclined side surfaces 2 a on both sides of the groove 2 as the ruled member 23 is pressed. Since it is pushed into the groove 2, even if a long ruled line 52 is inserted deeply, the liner of the cardboard 51 is not excessively pulled and the cardboard 51 is not cracked.

これにより、罫線52は、幅方向の中心線に対して両側に対称形状の傾斜部52aが形成されたものとなって、折曲力の作用を罫線52の中心線辺りに集中させることができ、段ボール51の段目53の影響を受けることなく、段ボール51を罫線52の幅方向中心線に沿って正確に折り曲げることができ、精度の高い箱を製造することができる。   As a result, the ruled line 52 has symmetrical inclined portions 52 a formed on both sides with respect to the center line in the width direction, and the action of the bending force can be concentrated around the center line of the ruled line 52. The cardboard 51 can be accurately bent along the center line in the width direction of the ruled line 52 without being affected by the step 53 of the cardboard 51, and a highly accurate box can be manufactured.

次に、この発明の第2実施形態を図5乃至図8に基づいて説明する。   Next, a second embodiment of the present invention will be described with reference to FIGS.

図5に示す溝部材としての面板1もまた、ステンレス等の金属製とされ、上盤11及び下盤12を備えた平型ダイカッタである加工機の下盤12に、デッドプレート14を介して装着される。この加工機では、上盤11に対して下盤12が昇降し、若しくは下盤12に対して上盤11が昇降し、又は上盤11と下盤12の双方が昇降することにより、上盤11と下盤12とが相対的に接近離反する。   The face plate 1 as the groove member shown in FIG. 5 is also made of metal such as stainless steel, and is attached to the lower plate 12 of the processing machine, which is a flat die cutter provided with the upper plate 11 and the lower plate 12, via the dead plate 14. Installed. In this processing machine, the lower board 12 moves up and down with respect to the upper board 11, or the upper board 11 moves up and down with respect to the lower board 12, or both the upper board 11 and the lower board 12 move up and down. 11 and the lower board 12 approach and separate relatively.

上盤11には、チェース13を介して、それぞれ線状に長さを有する切刃22及び押罫部材23を備えた型体21が装着される。   A mold body 21 having cutting edges 22 and ruled members 23 each having a linear length is mounted on the upper board 11 via the chase 13.

面板1には、図6及び図7に示すように、押罫部材23の下部先端に対向する上面を切り込んで長い凹溝2が形成され、凹溝2の一方の側面は、下方の底部から上方の開口部へかけて外側へ傾斜した傾斜側面2aとされ、他方の側面は、面板1の上面から下方へほぼ垂直な垂直側面2bとされている。凹溝2の上端の開口部側の幅は、押罫部材23の幅より大きくなっている。   As shown in FIGS. 6 and 7, the face plate 1 is formed with a long groove 2 by cutting the upper surface facing the lower end of the ruled member 23, and one side surface of the groove 2 extends from the bottom at the bottom. An inclined side surface 2 a that is inclined outward toward the upper opening is formed, and the other side surface is a vertical side surface 2 b that is substantially vertical downward from the upper surface of the face plate 1. The width of the upper end side of the groove 2 on the opening side is larger than the width of the ruled member 23.

このような面板1を、図5に示す加工機に装着する際には、押罫部材23の幅方向の中心線が凹溝2の中間部に位置するように、型体21及び面板1を位置決めする。   When such a face plate 1 is mounted on the processing machine shown in FIG. 5, the mold body 21 and the face plate 1 are placed so that the center line in the width direction of the ruled member 23 is located in the middle portion of the groove 2. Position.

いま、箱形成用のブランクを製造するため、段ボール51を打ち抜くと共に罫線を入れるには、上盤11に対して下盤12が下降し、面板1と型体21とが離反した状態で、図7に示すように、面板1と押罫部材23の間に、面板1の上面に沿って平坦な状態で段ボール51を供給する。ここでは、押罫部材23として、先端が平坦になった角罫を使用した場合を例示する。   Now, in order to produce a blank for forming a box, in order to punch out the cardboard 51 and put a ruled line, the lower plate 12 is lowered with respect to the upper plate 11, and the face plate 1 and the mold body 21 are separated from each other. 7, the cardboard 51 is supplied between the face plate 1 and the ruled member 23 in a flat state along the upper surface of the face plate 1. Here, a case where a square rule with a flat tip is used as the ruled member 23 is illustrated.

次に、図5及び図7に示す状態から、上盤11に対して下盤12を上昇させると、段ボール51が面板1と型体21とで挟まれて、切刃22で段ボール51が打ち抜かれ、箱のブランクの輪郭が形成される。この状態において、押罫部材23の下端部は、平坦な状態であった段ボール51の上面より下方に位置することとなる。   Next, when the lower board 12 is raised with respect to the upper board 11 from the state shown in FIGS. 5 and 7, the cardboard 51 is sandwiched between the face plate 1 and the mold body 21, and the cardboard 51 is hit by the cutting edge 22. It is pulled out and a blank outline of the box is formed. In this state, the lower end portion of the ruled line member 23 is positioned below the upper surface of the corrugated cardboard 51 that has been flat.

このとき、図8に示すように、剛性を有する段ボール51は、押罫部材23の押圧に伴い、凹溝2の垂直側面2bを基準にし、傾斜側面2aに沿って滑りながら、凹溝2の底部に接するまで凹溝2に押し込まれるので、長い罫線52を深く入れても、段ボール51のライナが過度に引っ張られて、段ボール51に割れを生じることがない。   At this time, as shown in FIG. 8, the corrugated cardboard 51 having rigidity slides along the inclined side surface 2a with reference to the vertical side surface 2b of the concave groove 2 as the ruled member 23 is pressed, Since it is pushed into the groove 2 until it touches the bottom, even if a long ruled line 52 is inserted deeply, the liner of the cardboard 51 is not pulled excessively and the cardboard 51 is not cracked.

これにより、罫線52は、その一側に凹溝2の垂直側面2bに対応して垂直部52bが形成され、その他側に凹溝2の傾斜側面2aに対応して傾斜部52aが形成されたものとなり、段ボール51は、傾斜部52aよりも強く折り曲げられた垂直部52bの下方辺りで折れ曲がり易いものとなる。   As a result, the ruled line 52 has a vertical portion 52b corresponding to the vertical side surface 2b of the groove 2 on one side and an inclined portion 52a corresponding to the inclined side surface 2a of the groove 2 on the other side. Thus, the corrugated cardboard 51 is easily bent around the lower part of the vertical part 52b that is bent more strongly than the inclined part 52a.

このため、罫線52を段ボール51の段目53に平行な方向に入れた場合であっても、段ボール51の段目53の影響を受けることなく、段ボール51を罫線52の垂直部52bに沿って正確に折り曲げることができ、精度の高い箱を製造することができる。   For this reason, even when the ruled line 52 is placed in a direction parallel to the step 53 of the cardboard 51, the cardboard 51 is not affected by the step 53 of the cardboard 51, and the cardboard 51 is moved along the vertical portion 52b of the ruled line 52. It can be bent accurately, and a highly accurate box can be manufactured.

また、上記各実施形態の罫線形成用溝部材を使用すると、複数本の罫線52に対応する凹溝2を一枚の面板1に直接形成することにより、加工機への装着の作業性を改善し、押罫部材23に対する凹溝2の位置精度も向上させることができ、デッドプレート14からの剥がれによる不良発生も防止できる。   Moreover, when the groove member for ruled line formation of each said embodiment is used, the workability of mounting | wearing with a processing machine is improved by directly forming the concave groove 2 corresponding to the several ruled line 52 in the surface plate 1 of 1 sheet. In addition, the positional accuracy of the groove 2 with respect to the ruled member 23 can be improved, and the occurrence of defects due to peeling from the dead plate 14 can also be prevented.

さらに、硬度の高い金属板を面板1の材料として、耐久性を向上させることにより、交換の手間も省くことができる。   Furthermore, by using a metal plate having a high hardness as the material of the face plate 1 and improving the durability, it is possible to save labor for replacement.

なお、上記各実施形態では、加工機が平型ダイカッタである場合の溝部材としての面板について例示したが、ロータリーダイカッタに使用される湾曲した溝部材としての面板においても、凹溝2の両側面又は一側面を傾斜させることにより、同様の罫入れ加工をすることができる。   In each of the above embodiments, the face plate as a groove member when the processing machine is a flat die cutter is illustrated, but both sides of the concave groove 2 are also used in the face plate as a curved groove member used for a rotary die cutter. By inclining the surface or one side surface, it is possible to perform the same ruled processing.

1 面板
2 凹溝
2a 傾斜側面
2b 垂直側面
11 上盤
12 下盤
13 チェース
14 デッドプレート
21 型体
22 切刃
23 押罫部材
51 段ボール
52 罫線
52a 傾斜部
52b 垂直部
53 段目
DESCRIPTION OF SYMBOLS 1 Face plate 2 Groove | groove 2a Inclined side surface 2b Vertical side surface 11 Upper board 12 Lower board 13 Chase 14 Dead plate 21 Mold body 22 Cutting edge 23 Ruled member 51 Corrugated cardboard 52 Ruled line 52a Inclined part 52b Vertical part 53 Stage

Claims (3)

押罫部材に対向して凹溝を形成し、押罫部材との接近に伴い、押罫部材に押圧された段ボールを凹溝で受けて、段ボールに罫線を入れる罫線形成用溝部材において、前記凹溝の少なくとも一方の側面を、底部から開口部へかけて外側へ傾斜した傾斜側面としたことを特徴とする罫線形成用溝部材。   A groove for forming a ruled line that forms a concave groove facing the ruled member, receives the corrugated cardboard pressed by the ruled member with the concave groove as it approaches the ruled member, and puts a ruled line on the cardboard. A ruled line forming groove member characterized in that at least one side surface of the concave groove is an inclined side surface inclined outward from the bottom to the opening. 前記凹溝の両方の側面を、底部から開口部へかけて外側へ傾斜した傾斜側面としたことを特徴とする請求項1に記載の罫線形成用溝部材。   2. The ruled line forming groove member according to claim 1, wherein both side surfaces of the concave groove are inclined side surfaces that are inclined outward from a bottom portion to an opening portion. 前記凹溝の一方の側面のみを傾斜側面とし、他方の側面を垂直側面としたことを特徴とする請求項1に記載の罫線形成用溝部材。   2. The ruled line forming groove member according to claim 1, wherein only one side surface of the concave groove is an inclined side surface and the other side surface is a vertical side surface.
JP2009140032A 2009-06-11 2009-06-11 Groove member for forming ruled line Pending JP2010284868A (en)