JP2010179353A - ガスシールドアーク溶接方法 - Google Patents
ガスシールドアーク溶接方法 Download PDFInfo
- Publication number
- JP2010179353A JP2010179353A JP2009027343A JP2009027343A JP2010179353A JP 2010179353 A JP2010179353 A JP 2010179353A JP 2009027343 A JP2009027343 A JP 2009027343A JP 2009027343 A JP2009027343 A JP 2009027343A JP 2010179353 A JP2010179353 A JP 2010179353A
- Authority
- JP
- Japan
- Prior art keywords
- gas
- welding
- arc welding
- zinc
- welding method
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Arc Welding In General (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2009027343A JP2010179353A (ja) | 2009-02-09 | 2009-02-09 | ガスシールドアーク溶接方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2009027343A JP2010179353A (ja) | 2009-02-09 | 2009-02-09 | ガスシールドアーク溶接方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2010179353A true JP2010179353A (ja) | 2010-08-19 |
| JP2010179353A5 JP2010179353A5 (enExample) | 2012-02-23 |
Family
ID=42761297
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2009027343A Pending JP2010179353A (ja) | 2009-02-09 | 2009-02-09 | ガスシールドアーク溶接方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2010179353A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2013035060A (ja) * | 2011-07-13 | 2013-02-21 | Nisshin Steel Co Ltd | Zn−Al−Mg系めっき鋼板アーク溶接構造部材の製造法 |
| US20150231726A1 (en) * | 2014-02-19 | 2015-08-20 | Nisshin Steel Co., Ltd. | METHOD FOR PRODUCING ARC-WELDED Zn-Al-Mg ALLOY COATED STEEL PLATE STRUCTURAL MEMBER |
Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02228050A (ja) * | 1989-02-28 | 1990-09-11 | Hitachi Ltd | 回路基板とその製法および該基板を用いた電子回路装置 |
| JPH11138265A (ja) * | 1997-10-31 | 1999-05-25 | Daihen Corp | 交流パルスマグ溶接方法及び装置 |
-
2009
- 2009-02-09 JP JP2009027343A patent/JP2010179353A/ja active Pending
Patent Citations (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH02228050A (ja) * | 1989-02-28 | 1990-09-11 | Hitachi Ltd | 回路基板とその製法および該基板を用いた電子回路装置 |
| JPH11138265A (ja) * | 1997-10-31 | 1999-05-25 | Daihen Corp | 交流パルスマグ溶接方法及び装置 |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2013035060A (ja) * | 2011-07-13 | 2013-02-21 | Nisshin Steel Co Ltd | Zn−Al−Mg系めっき鋼板アーク溶接構造部材の製造法 |
| US20150231726A1 (en) * | 2014-02-19 | 2015-08-20 | Nisshin Steel Co., Ltd. | METHOD FOR PRODUCING ARC-WELDED Zn-Al-Mg ALLOY COATED STEEL PLATE STRUCTURAL MEMBER |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US10155276B2 (en) | Method of welding surface-treated members using a welding wire | |
| CN101977721B (zh) | 等离子焊炬以及等离子焊接法 | |
| CN106163719B (zh) | 开启和使用组合填充焊丝送进和高强度能源以用于复合管内径的根部焊道焊接的焊接系统和方法 | |
| US10086461B2 (en) | Method and system to start and use combination filler wire feed and high intensity energy source for welding | |
| CN102814578B (zh) | 双电极焊接法 | |
| US20130092667A1 (en) | Method and System to Start and Use Combination Filler Wire Feed and High Intensity Energy Source for Welding | |
| WO2014054261A1 (ja) | アーク溶接制御方法 | |
| JP5884209B1 (ja) | 立向き狭開先ガスシールドアーク溶接方法 | |
| US20150129560A1 (en) | Plasma-mig welding method and welding torch | |
| CN104093517A (zh) | 直流电极负极旋转电弧焊接方法和系统 | |
| JP2009107017A (ja) | 溶接部の品質を制御する方法 | |
| KR20200054331A (ko) | 용접 와이어 전극,용접 방법 및 용접 시스템 | |
| JPWO2014073184A1 (ja) | アーク溶接装置およびアーク溶接制御方法 | |
| KR20130103495A (ko) | 복합 용접 방법 및 복합 용접용 용접 토치 | |
| JP2009208137A (ja) | プラズマミグ溶接方法 | |
| CN108367376B (zh) | 立式窄坡口气体保护弧焊方法 | |
| US20190299314A1 (en) | Method of cleaning a workpiece after a thermal joining process with cathodic cleaning; cleaning device and processing gas | |
| JP5302558B2 (ja) | プラズマ溶接法およびこれに用いられるアウターガス | |
| JP2010179353A (ja) | ガスシールドアーク溶接方法 | |
| JP2009078274A (ja) | 2電極アーク溶接方法 | |
| JP2010234409A (ja) | 狭開先溶接トーチ及び該溶接トーチを備えたタンデムアーク溶接装置 | |
| JP2005103592A (ja) | アーク溶接装置 | |
| JP2006075847A (ja) | レーザとアークのハイブリッド溶接方法 | |
| JP2004195528A (ja) | マグネシウム又はマグネシウム合金のレーザ照射アーク溶接方法 | |
| JP4120468B2 (ja) | プラズマアーク溶接方法及びその装置 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| A521 | Written amendment |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20120106 |
|
| A621 | Written request for application examination |
Free format text: JAPANESE INTERMEDIATE CODE: A621 Effective date: 20120106 |
|
| A977 | Report on retrieval |
Free format text: JAPANESE INTERMEDIATE CODE: A971007 Effective date: 20130417 |
|
| A131 | Notification of reasons for refusal |
Free format text: JAPANESE INTERMEDIATE CODE: A131 Effective date: 20130423 |
|
| A521 | Written amendment |
Free format text: JAPANESE INTERMEDIATE CODE: A523 Effective date: 20130612 |
|
| A02 | Decision of refusal |
Effective date: 20131001 Free format text: JAPANESE INTERMEDIATE CODE: A02 |