JP2009298893A5 JP2008153729A JP2008153729A JP2009298893A5 JP 2009298893 A5 JP2009298893 A5 JP 2009298893A5 JP 2008153729 A JP2008153729 A JP 2008153729A JP 2008153729 A JP2008153729 A JP 2008153729A JP 2009298893 A5 JP2009298893 A5 JP 2009298893A5
Authority
JP
Japan
Prior art keywords
content
reaction product
aqueous liquid
maleic anhydride
weight
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2008153729A
Other languages
English (en)
Japanese (ja)
Other versions
JP2009298893A (ja
JP5514408B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2008153729A priority Critical patent/JP5514408B2/ja
Priority claimed from JP2008153729A external-priority patent/JP5514408B2/ja
Publication of JP2009298893A publication Critical patent/JP2009298893A/ja
Publication of JP2009298893A5 publication Critical patent/JP2009298893A5/ja
Application granted granted Critical
Publication of JP5514408B2 publication Critical patent/JP5514408B2/ja
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

JP2008153729A 2008-06-12 2008-06-12 水性液用ゲル化剤、水性液ゲル及び水性液ゲルの製造方法 Expired - Fee Related JP5514408B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2008153729A JP5514408B2 (ja) 2008-06-12 2008-06-12 水性液用ゲル化剤、水性液ゲル及び水性液ゲルの製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2008153729A JP5514408B2 (ja) 2008-06-12 2008-06-12 水性液用ゲル化剤、水性液ゲル及び水性液ゲルの製造方法

Publications (3)

Publication Number Publication Date
JP2009298893A JP2009298893A (ja) 2009-12-24
JP2009298893A5 true JP2009298893A5 (enrdf_load_stackoverflow) 2011-05-26
JP5514408B2 JP5514408B2 (ja) 2014-06-04

Family

ID=41546121

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2008153729A Expired - Fee Related JP5514408B2 (ja) 2008-06-12 2008-06-12 水性液用ゲル化剤、水性液ゲル及び水性液ゲルの製造方法

Country Status (1)

Country Link
JP (1) JP5514408B2 (enrdf_load_stackoverflow)

Family Cites Families (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP3321123B2 (ja) * 1998-10-20 2002-09-03 三洋化成工業株式会社 水性液用ゲル化剤およびその物品
JP2003253246A (ja) * 2001-12-27 2003-09-10 Sanyo Chem Ind Ltd 水系ゲル成形体及びそれを使用した物品
JP2004000581A (ja) * 2002-04-26 2004-01-08 Sanyo Chem Ind Ltd 芳香材及び芳香剤
JP2006008896A (ja) * 2004-06-28 2006-01-12 Sanyo Chem Ind Ltd 装飾用膨潤性成形体及びそれを使用した物品
JP3904010B2 (ja) * 2004-08-24 2007-04-11 昭三 遠藤 形状保持性ゼラチン水性ゲルおよび製造方法
JP5148317B2 (ja) * 2008-02-26 2013-02-20 三洋化成工業株式会社 水性液用ゲル化剤、水性液ゲル及び水性液ゲルの製造方法

Similar Documents

Publication Publication Date Title
Karoyo et al. A review on the design and hydration properties of natural polymer-based hydrogels
CN102093513B (zh) 马铃薯淀粉接枝丙烯酸制备吸水树脂的方法
CN103881398B (zh) 一种聚三亚甲基碳酸酯与聚对二氧环己酮改进聚乙烯醇膜耐水性的方法
CN110437764B (zh) 一种树脂改性淀粉粘合剂及其制备方法
CN105315507B (zh) 一种制备改性石墨烯‑壳聚糖复合薄膜的方法
JP2006225669A5 (enrdf_load_stackoverflow)
JP2006225668A5 (enrdf_load_stackoverflow)
CN106009001A (zh) 壳聚糖气凝胶的制备方法
CN101362804B (zh) 高取代度乙酰淀粉及其制备方法
CN105218996B (zh) 一种改性石墨烯‑聚乙烯醇复合薄膜的制备方法
CN106893004A (zh) 一种壳聚糖‑酚酸轭合物的制备方法
CN104559832A (zh) Cmc淀粉胶
CN101215389B (zh) 一种壳聚糖水凝胶及其制备方法
CN103923274A (zh) 一种环境友好的木质素高吸水树脂及其制备方法
CN107619645A (zh) 一种基于全酶法制备多巴胺增强淀粉基粘合剂的方法
CN104559831A (zh) 涂布用改性淀粉胶粘剂
CN104946162A (zh) 一种炭基缓释复混肥造粒用淀粉胶黏剂的制备方法
Baruah et al. Guar gum-based hydrogel and hydrogel nanocomposites for biomedical applications
JP2009298893A5 (enrdf_load_stackoverflow)
CN102977334A (zh) 一种分子印迹聚合物及制备方法和应用
El Farkhani et al. A review of the chemical modification and applications of starch
JP2006501324A5 (enrdf_load_stackoverflow)
Wu et al. Study of the degradation mechanisms of oxidized cellulose-derivative hemostatic agent by using model compound
CN104761693A (zh) 一种含半乳糖温敏共聚物的自组装方法
CN103627366B (zh) 一种明胶基胶粘剂的制备方法