JP2008001785A5 - - Google Patents

Download PDF

Info

Publication number
JP2008001785A5
JP2008001785A5 JP2006171980A JP2006171980A JP2008001785A5 JP 2008001785 A5 JP2008001785 A5 JP 2008001785A5 JP 2006171980 A JP2006171980 A JP 2006171980A JP 2006171980 A JP2006171980 A JP 2006171980A JP 2008001785 A5 JP2008001785 A5 JP 2008001785A5
Authority
JP
Japan
Prior art keywords
lacquer
based paint
paint according
manufacturing
linseed oil
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2006171980A
Other languages
Japanese (ja)
Other versions
JP2008001785A (en
JP5013582B2 (en
Filing date
Publication date
Application filed filed Critical
Priority to JP2006171980A priority Critical patent/JP5013582B2/en
Priority claimed from JP2006171980A external-priority patent/JP5013582B2/en
Publication of JP2008001785A publication Critical patent/JP2008001785A/en
Publication of JP2008001785A5 publication Critical patent/JP2008001785A5/ja
Application granted granted Critical
Publication of JP5013582B2 publication Critical patent/JP5013582B2/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Claims (11)

生漆又は精製漆に、重合アマニ油、重合アマニ油及びロジン、エチレングリコール、グリセリン並びに界面活性剤よりなる群から選ばれた添加剤を添加する添加工程、及び、
得られた混合物を媒体撹拌ミルにより微細化して、油中水滴型エマルションに含まれる水滴の粒径範囲を50〜150nmにする微細化工程を含む
漆系塗料の製造方法。
An addition step of adding an additive selected from the group consisting of polymerized linseed oil, polymerized linseed oil and rosin, ethylene glycol, glycerin and a surfactant to fresh lacquer or purified lacquer , and
A method for producing a lacquer-based paint, comprising a step of refining the obtained mixture with a medium stirring mill to make the particle size range of water droplets contained in the water-in-oil emulsion 50 to 150 nm .
生漆又は精製漆に、重合アマニ油、重合アマニ油及びロジン並びにエチレングリコールよりなる群から選ばれた添加剤を添加する添加工程である、請求項1に記載の漆系塗料の製造方法。  The manufacturing method of the lacquer-type coating material of Claim 1 which is an addition process which adds the additive chosen from the group which consists of polymeric linseed oil, polymeric linseed oil, rosin, and ethylene glycol to fresh lacquer or refined lacquer. 20〜40℃において微細化する微細化工程である請求項1又は2に記載の漆系塗料の製造方法。 A refining step of refining at 20 to 40 ° C., the manufacturing method of the lacquer-based paint according to claim 1 or 2. 生漆又は精製漆の油性成分に対し水分が5〜15重量%となるように含水率を調節する水分調節工程の後に、前記添加工程及び前記微細化工程を含む請求項1〜3いずれか1つに記載の漆系塗料の製造方法。 Any one of Claims 1-3 including the said addition process and the said refinement | miniaturization process after the water | moisture-content adjustment process which adjusts a moisture content so that a water | moisture content may be 5 to 15 weight% with respect to the oil-based component of raw lacquer or refined lacquer. The manufacturing method of the lacquer-type coating material as described in one . 媒体として比重が4.5以上で直径が0.3〜0.8mmのビーズを使用する請求項1〜いずれか1つに記載の漆系塗料の製造方法。 The method for producing a lacquer-based paint according to any one of claims 1 to 4 , wherein beads having a specific gravity of 4.5 or more and a diameter of 0.3 to 0.8 mm are used as a medium. 精製漆が無油透漆又は有油透漆である請求項1〜いずれか1つに記載の漆系塗料の製造方法。 Purification lacquer is Muabura Toruurushi or Yuabura Toruurushi method of lacquer-based paint according to any one claims 1-5. 請求項1〜いずれか1つに記載の製造方法により製造された漆系塗料。 The lacquer-type coating material manufactured by the manufacturing method as described in any one of Claims 1-6 . アルコキシシラン類、ウレタン樹脂及びエポキシ樹脂よりなる群から選ばれた添加剤を含む請求項に記載の漆系塗料。 Alkoxysilanes, containing a urethane resin and an additive selected from the group consisting of epoxy resin, lacquer-based paint according to claim 7. 請求項又はに記載の漆系塗料を有機溶剤により希釈して得られるインクジェット用漆インク。 Inkjet lacquer inks obtained by diluting with an organic solvent lacquer-based paint according to claim 7 or 8. 請求項に記載の漆インクを基材にインクジェット方法により吐出する印刷工程を含む漆系塗料の塗装方法。 The coating method of the lacquer-type paint including the printing process which discharges the lacquer ink of Claim 9 to a base material with an inkjet method. 基材上に吐出された漆インクから有機溶剤を揮発させる乾燥工程、及び、
漆インクの指触乾燥前に金属粉、金属箔、金属蒸着フィルム粉若しくは積層フィルム粉を蒔き付けるか又は金属箔を貼り付ける加飾工程を更に含む請求項10に記載の漆系塗料の塗装方法。
A drying step of volatilizing the organic solvent from the lacquer ink discharged on the substrate, and
The coating of the lacquer-based paint according to claim 10 , further comprising a decorating step in which a metal powder, a metal foil, a metal vapor-deposited film powder, or a laminated film powder is applied before the lacquer ink is dried by touching the metal foil. Method.
JP2006171980A 2006-06-21 2006-06-21 Lacquer-based paint, its production method and lacquer coating material Expired - Fee Related JP5013582B2 (en)