granulation
compression molding
good
speed
wet granulation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2005180305A
Other languages
English (en)
Other versions
JP2007001875A (ja
JP4947613B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority to JP2005180305A priority Critical patent/JP4947613B2/ja
Priority claimed from JP2005180305A external-priority patent/JP4947613B2/ja
Publication of JP2007001875A publication Critical patent/JP2007001875A/ja
Publication of JP2007001875A5 publication Critical patent/JP2007001875A5/ja
Application granted granted Critical
Publication of JP4947613B2 publication Critical patent/JP4947613B2/ja
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Description

本発明で用いる湿式造粒法は、高速攪拌造粒、押し出し造粒、流動層造粒などの公知の湿式造粒法を用いて、均一な粒度分布と、圧縮成形して得られる錠剤が高い硬度と良好な崩壊時間を兼ね備えた圧縮成形特性とを有する造粒組成物を得ることができる。シアが大きく攪拌効率が良い点で、高速攪拌造粒を用いることが好ましい。
JP2005180305A 2005-06-21 2005-06-21 造粒組成物の製造方法 Active JP4947613B2 (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP2005180305A JP4947613B2 (ja) 2005-06-21 2005-06-21 造粒組成物の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP2005180305A JP4947613B2 (ja) 2005-06-21 2005-06-21 造粒組成物の製造方法

Publications (3)

Publication Number Publication Date
JP2007001875A JP2007001875A (ja) 2007-01-11
JP2007001875A5 true JP2007001875A5 (ja) 2008-07-31
JP4947613B2 JP4947613B2 (ja) 2012-06-06

Family

ID=37687802

Family Applications (1)

Application Number Title Priority Date Filing Date
JP2005180305A Active JP4947613B2 (ja) 2005-06-21 2005-06-21 造粒組成物の製造方法

Country Status (1)

Country Link
JP (1) JP4947613B2 (ja)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2007001999A (ja) * 2005-06-21 2007-01-11 Asahi Kasei Chemicals Corp 造粒組成物の製造方法
CN101981059B (zh) 2008-03-31 2014-08-20 旭化成化学株式会社 具有出色的崩解性能的经加工的淀粉粉末及其制造方法
JP2015218322A (ja) * 2014-05-21 2015-12-07 旭化成ケミカルズ株式会社 微小澱粉粒子及びその製造方法

Family Cites Families (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2005005484A1 (ja) * 2003-07-11 2005-01-20 Asahi Kasei Chemicals Corporation 機能性澱粉粉末

Similar Documents

Publication Publication Date Title
JP2005508424A5 (ja)
WO2006100281A3 (en) Solubilized ibuprofen
WO2009043844A3 (en) Orodispersible tablets
DK1917339T3 (da) Film med rengøringsmidler
JP2009519992A5 (ja)
NZ595902A (en) Method for the production of commercial nanoparticle and microparticle powders
RS51342B (en) Mucosal bioadhesive carrier for slow release of active substances
ATE515198T1 (de) Zusammensetzung für die enterale verabreichung von mikroorganismen
PL2020864T3 (pl) Sprasowana guma do żucia i sposób jej wytwarzania
JP2007001875A5 (ja)
EA201001537A1 (ru) Гранулированная агрохимическая композиция и способы её получения
JP2007001999A5 (ja)
EP1657275A4 (en) SILICA CHARGING GRANULAR RUBBER AND PROCESS FOR PRODUCING THE SAME
CN102321225A (zh) 一种高吸水复合材料的制备方法
CN1428410A (zh) 一种洗衣用片状洗涤剂及其制造方法
JP2014062064A5 (ja)
TW200738286A (en) Solubilized ibuprofen
JP2010531847A5 (ja)
JP2004536016A5 (ja)
ES2658566T3 (es) Método de compactación de composiciones basadas en heptahidrato de sulfato ferroso y producto obtenido a partir de ellas
JP2001518529A5 (ja)
WO2009149136A3 (en) Production of sustained release starch product
JP6902897B2 (ja) グルタチオン含有組成物の製造方法
CN103976964A (zh) 依托红霉素片及其制备方法
KR100909088B1 (ko) 나노크기의 결합재를 함유한 친환경 마그네슘보드