JP2006080059A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2006080059A5 JP2006080059A5 JP2005231726A JP2005231726A JP2006080059A5 JP 2006080059 A5 JP2006080059 A5 JP 2006080059A5 JP 2005231726 A JP2005231726 A JP 2005231726A JP 2005231726 A JP2005231726 A JP 2005231726A JP 2006080059 A5 JP2006080059 A5 JP 2006080059A5
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2005231726A JP4784197B2 (ja) | 2004-08-11 | 2005-08-10 | 固体電解質型燃料電池の燃料極材料用酸化ニッケル粉及び燃料極材料 |
Applications Claiming Priority (3)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2004233994 | 2004-08-11 | ||
JP2004233994 | 2004-08-11 | ||
JP2005231726A JP4784197B2 (ja) | 2004-08-11 | 2005-08-10 | 固体電解質型燃料電池の燃料極材料用酸化ニッケル粉及び燃料極材料 |
Publications (3)
Publication Number | Publication Date |
---|---|
JP2006080059A JP2006080059A (ja) | 2006-03-23 |
JP2006080059A5 true JP2006080059A5 (enrdf_load_stackoverflow) | 2008-03-06 |
JP4784197B2 JP4784197B2 (ja) | 2011-10-05 |
Family
ID=36159319
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP2005231726A Expired - Lifetime JP4784197B2 (ja) | 2004-08-11 | 2005-08-10 | 固体電解質型燃料電池の燃料極材料用酸化ニッケル粉及び燃料極材料 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JP4784197B2 (enrdf_load_stackoverflow) |
Families Citing this family (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US8288053B2 (en) | 2005-08-18 | 2012-10-16 | Sumitomo Metal Mining Co., Ltd. | Nickel oxide powder material for solid oxide fuel cell, production process thereof, raw material composition for use in the same, and anode material using the nickel oxide powder material |
JP5131098B2 (ja) * | 2008-09-04 | 2013-01-30 | 住友金属鉱山株式会社 | ニッケル微粉及びその製造方法 |
JP5136904B2 (ja) * | 2008-12-02 | 2013-02-06 | 住友金属鉱山株式会社 | ニッケル粉の製造方法 |
CN103199288B (zh) * | 2013-03-21 | 2015-06-17 | 中国科学院宁波材料技术与工程研究所 | 固体氧化物燃料电池的电极及其制备方法 |
JP2020186154A (ja) * | 2019-05-16 | 2020-11-19 | 住友金属鉱山株式会社 | 大粒径酸化ニッケル粉末及びその製造方法 |
Family Cites Families (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
NL9002168A (nl) * | 1990-10-05 | 1992-05-06 | Blandikus Catharikus Jaspers E | Holle elektrode voor een elektrochemische cel voorzien van ten minste een toe- en een afvoeropening voor gassen, alsmede elektrochemische cel die een dergelijke elektrode omvat. |
JP3151933B2 (ja) * | 1992-05-28 | 2001-04-03 | 株式会社村田製作所 | 固体電解質型燃料電池 |
JPH10134825A (ja) * | 1996-10-29 | 1998-05-22 | Mitsubishi Heavy Ind Ltd | 固体電解質型電気化学セル |
JP4051771B2 (ja) * | 1997-06-10 | 2008-02-27 | 堺化学工業株式会社 | 水酸化ニッケル粒子、その製造方法、これを原料とするリチウム・ニッケル複合酸化物粒子及びその製造方法 |
JP3724762B2 (ja) * | 1997-07-11 | 2005-12-07 | 日本電信電話株式会社 | 固体電解質型燃料電池の燃料電極の製造方法 |
JP2002068742A (ja) * | 2000-08-28 | 2002-03-08 | Dai Ichi Kogyo Seiyaku Co Ltd | 複合酸化物の製造方法及びそれにより製造した複合酸化物ゾルと固体電解質型燃料電池 |
WO2004049491A1 (en) * | 2002-10-25 | 2004-06-10 | Antonino Salvatore Arico | SOLID OXIDE FUEL CELL WITH CERMET Cu/Ni ALLOY ANODE |
-
2005
- 2005-08-10 JP JP2005231726A patent/JP4784197B2/ja not_active Expired - Lifetime