JP2005238331A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2005238331A5 JP2005238331A5 JP2005010020A JP2005010020A JP2005238331A5 JP 2005238331 A5 JP2005238331 A5 JP 2005238331A5 JP 2005010020 A JP2005010020 A JP 2005010020A JP 2005010020 A JP2005010020 A JP 2005010020A JP 2005238331 A5 JP2005238331 A5 JP 2005238331A5
- Authority
- JP
- Japan
- Prior art keywords
- aluminum
- ceramic particles
- aluminum alloy
- mold
- electroless nickel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2005010020A JP2005238331A (ja) | 2004-01-26 | 2005-01-18 | 複合材およびその製造方法 |
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2004016694 | 2004-01-26 | ||
| JP2005010020A JP2005238331A (ja) | 2004-01-26 | 2005-01-18 | 複合材およびその製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JP2005238331A JP2005238331A (ja) | 2005-09-08 |
| JP2005238331A5 true JP2005238331A5 (enExample) | 2006-12-21 |
Family
ID=35020608
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2005010020A Pending JP2005238331A (ja) | 2004-01-26 | 2005-01-18 | 複合材およびその製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JP2005238331A (enExample) |
Families Citing this family (9)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR101721818B1 (ko) * | 2008-07-17 | 2017-03-30 | 덴카 주식회사 | 알루미늄-다이아몬드계 복합체 및 그 제조 방법 |
| FR2984251B1 (fr) * | 2011-12-19 | 2014-01-10 | Saint Gobain | Vitrage eclairant pour vehicule |
| CN107611040B (zh) * | 2017-09-18 | 2019-06-14 | 上海开朋科技有限公司 | 铝金刚石复合材料表面覆盖铜箔同时镶嵌陶瓷材料的工艺 |
| CN107649663B (zh) * | 2017-09-18 | 2019-06-14 | 江苏凯讯新材料有限公司 | 一种在铝金刚石复合材料表面覆盖钼箔的工艺方法 |
| CN107470588B (zh) * | 2017-09-18 | 2019-05-10 | 上海开朋科技有限公司 | 在铝金刚石复合材料表面覆盖铜箔的方法 |
| CN107552768B (zh) * | 2017-09-18 | 2019-06-14 | 江苏凯讯新材料有限公司 | 一种在铝金刚石复合材料表面覆盖钼箔的工艺方法 |
| CN107695321B (zh) * | 2017-09-18 | 2019-06-07 | 江南大学 | 一种在铝碳化硅复合材料表面覆盖铝箔的工艺 |
| CN114603315B (zh) * | 2022-02-28 | 2023-03-24 | 江南大学 | 一种金属基陶瓷复合材料基板拱形表面的车削成形方法 |
| CN114582730B (zh) * | 2022-02-28 | 2022-11-04 | 江南大学 | 一种制备高性能铝基复合材料散热基板的方法 |
-
2005
- 2005-01-18 JP JP2005010020A patent/JP2005238331A/ja active Pending
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US10773456B2 (en) | Process for strengthening porous 3D printed objects | |
| JP5599769B2 (ja) | 複数の金属層を含むカバーを製造する方法及び装置 | |
| WO2005077114A3 (en) | Product forming molds and methods to manufacture same | |
| MY168688A (en) | Hardfaced wearpart using brazing and associated method and assembly for manufacturing | |
| CN102802860A (zh) | 具有装饰表面的铸造金属部件以及制造其的方法 | |
| WO2010022325A3 (en) | Method of making an earth-boring metal matrix rotary drill bit | |
| JP2007528810A5 (enExample) | ||
| JP2015226935A5 (enExample) | ||
| RU2018120687A (ru) | Высокопроводящий графано-металлический композит и методы его производства | |
| WO2010022322A3 (en) | Earth-boring metal matrix rotary drill bit | |
| JP2016500582A5 (enExample) | ||
| KR20200017470A (ko) | 세라믹 휴대폰 백커버 및 그 성형공정 | |
| CN105256168A (zh) | 一种铜基-石墨自润滑复合材料及其制备方法 | |
| JP2006228475A5 (enExample) | ||
| JP2012148553A5 (enExample) | ||
| CN104853577B (zh) | 超薄电磁屏蔽膜生产工艺 | |
| JP2010513706A5 (enExample) | ||
| WO2012065323A1 (zh) | 一种非晶金属与塑料的复合材料、复合壳件及其制备方法 | |
| CN101619801A (zh) | 实芯蜂窝板 | |
| JP2010202928A (ja) | 金属造形物の製造方法及び積層造形用の金属樹脂複合体粉末 | |
| JP2006219752A5 (enExample) | ||
| EP3429817A1 (en) | Method for manufacturing composite part of polymer and metal | |
| JP2012509836A5 (enExample) | ||
| JP2011156808A (ja) | 機能性樹脂成形体の製造方法 | |
| JP2006331714A5 (enExample) |